Many cleaners, are extremely hard on many plastic products causing environmental stress cracking. Small household articles made from a polymer alloy of a clear brittle styrenic acrylate, a rubbery block styrene-diene copolymer, and a ductile styrene-diene polymer when exposed to such cleaners have significantly less environmental stress cracking.
Claims31
A small household article having good environmental stress crack resistance to cleaners said article comprising:
- from 80 to 100% of a polymer alloy consisting essentially of:
- (i) from 30 to 82 weight % of a brittle polymer comprising:
- (a) from 80 to 40 weight percent of one or more C.sub.8-12 vinyl aromatic monomers which are unsubstituted or substituted by a C.sub.1-4 alkyl radical;
- (b) from 20 to 60 weight percent of one or more C.sub.1-6 alkyl esters of C.sub.3-6 ethylenically unsaturated carboxylic acids;
- and
- (c) from 0 to 5 weight percent of one or more C.sub.3-6 ethylenically unsaturated carboxylic acids;
- (ii) from 3 to 50 weight % of a rubbery polymer comprising:
- (a) from 40 to 45 weight percent of one or more C.sub.8-12 vinyl aromatic monomers;
- and
- (b) from 60 to 55 weight percent of one or more C.sub.4-6 conjugated diolefins;
- and
- (iii) from 15 to 67 weight percent of a ductile polymer comprising:
- (a) from 70 to 80 weight percent of one or more C.sub.8-12 vinyl aromatic monomers;
- and
- (b) from 30 to 20 weight percent of one or more C.sub.4-6 conjugated diolefins.