Copper bearing alloy
AssigneeTaiho Kogyo Co., Ltd.
InventorsTakashi Tomikawa, Yoshio Kumada
Life of this patent
Estimating the term…
Abstract
Copper bearing alloy comprises more than 4% by weight and up to 35% by weight of Bi, 0.2 to less than 1.5% by weight of Pb and the rest of Cu. This considerably improves the erosion resistance while maintaining the excellent seizure resistance and fatigue strength.
Claims3
Copper bearing alloy consisting of more than 4% by weight and up to 35% by weight of Bi, 0.2 to less than 1.5% by weight of Pb and the rest of Cu.
Copper bearing alloy consisting of more than 4% by weight of up to 35% by weight of Bi, 0.2 to less than 1.5% by weight of Pb, at least one of from 0.1 to 5% by weight of Sn, from 0.1 to 1% by weight of Zn, from 0.1 to 1% by weight of Si, from 0.1 to 1% by weight of Sb, from 0.01 to 1% by weight of P, and from 0.1 to 5% by weight of Ni and the remainder Cu.
Copper bearing alloy consisting of more than 4% by weight and up to 35% by weight of Bi, 0.2 to less than 1.5% by weight of Pb, at least one of from 1 to 3% by weight of Sn, from 0.5 to 0.7% by weight of Zn, from 0.3 to 0.5% by weight of Si, from 0.3 to 0.5% by weight of Sb, from 0.05 to 0.5% by weight of P, and from 1 to 3% by weight of Ni and the remainder Cu.