Method of making permanent magnets
AssigneeIowa State University Research Foundation, Inc.
InventorsR. William McCallum, Kevin W. Dennis, Barbara K. Lograsso, Iver E. Anderson
Life of this patent
Estimating the term…
Abstract
A method for making an isotropic permanent magnet comprises atomizing a melt of a rare earth-transition metal alloy (e.g., an Nd--Fe--B alloy enriched in Nd and B) under conditions to produce protectively coated, rapidly solidified, generally spherical alloy particles wherein a majority of the particles are produced/size classified within a given size fraction (e.g., 5 to 40 microns diameter) exhibiting optimum as-atomized magnetic properties and subjecting the particles to concurrent elevated temperature and elevated isotropic pressure for a time effective to yield a densified, magnetically isotropic magnet compact having enhanced magnetic properties and mechanical properties.
Claims20
A method of making an isotropic magnet, comprising the steps of:
- a) inert gas atomizing a melt comprising a rare earth and a transition metal to form generally spherical, rapidly solidified rare earth-transition metal alloy particles,
- b) coating the atomized particles with an environmentally protective coating thereon by contact with a reactive gas downstream of the atomizing location, and
- c) subjecting the atomized and coated particles to concurrent elevated temperature and elevated isotropic pressure for a time to produce a densified, magnetically isotropic magnet compact.
The method of cliam 1 wherein the coating comprises an inner nitride layer and an outer graphite layer.
A method of making an isotropic permanent magnet, comprising the steps of:
- a) inert gas atomizing a melt comprising a rare earth-transition metal alloy to form generally spherical, rapidaly solidified alloy particles wherein a majority of the particles are produced having a particle size less than a larger particle size which larger size exhibits coercivity below about 5 kOe,
- b) coating the atomized particles with an environmentally protective coating thereon by contact with a reactive gas downstream of the atomizing location, and
- c) subjecting the atomized and coated particles to concurrent elevated temperature and elevated isotropic pressure for a time to produce a densified, magnetically isotropic magnet compact.
A method of making an isotropic permanent magnet, comprising the steps of:
- a) inert gas atomizing a melt comprising a rare earth-transition metal alloy to from generally spherical, rapidly solidified alloy powder in a range of particle sizes,
- b) coating the atomized powder with an environmentally protective coating thereon by contact with a reactive gas downstream of the atomizing location, and
- c) separating the atomized and coated powder into one or more particle size fractions, and
- d) subjecting the atomized and coated powder of a particular size fraction to concurrent elevated temperature and elevated isotropic pressure for a time to produce a densified, magnetically isotropic magnet compact.
A method of making an isotropic permanent magnet, comprising the steps of:
- a) inert gas atomizing a melt comprising a rare earth-iron-boron alloy to form generally spherical, rapidly solidified alloy powder in a range of particle sizes,
- b) coating the atomized powder with an environmentally protective coating thereon by contact with a reactive gas downstream of the atomizing location,
- c) separating the atomized and coated alloy powder into one or more particle size fractions, and
- d) subjecting the atomized and coated powder of a particular size fraction to concurrent elevated temperature and elevated isotropic pressure for a time to produce a densified, magnetically isotropic magnet compact.
A method of making an isotropic magnet, comprising the steps of:
- a) atomizing a melt comprising a rare earth and a transition metal to form generally spherical, rapidly solidified rare earth-transition metal alloy particles,
- b) coating the atomized particles with an environmentally protective coating thereon by contact with a reactive gas downstream of the atomizing location, and
- c) subjecting the atomized particles to concurrent elevated temperature and elevated isotropic pressure for a time effective to produce particle-to-particle bonding and improved magnetic properties as compared to as-atomized particle magnet properties so as to yield a densified, interparticle-bonded, magnetically isotropic magnet compact.
A method of making an isotropic permanent magnet, comprising the steps of:
- a) atomizing a melt comprising a rare earth-transition metal alloy to produce generally spherical, rapidly solidified alloy particles wherein a majority of the particles are produced having a particle size less than a larger particle size which large size exhibits coercivity below about 5 kOe,
- b) coating the atomized particles with an environmentally protective coating thereon by contact with a reactive gas downstream of the atomizing location, and
- c) subjecting the atomized particles to concurrent elevated temperature and elevated isotropic pressure for a time to produce particle-to-particle bonding and improved magnetic properties as compared to as-atomized particle magnetic properties so as to yield a densified, interparticle-bonded, magnetically isotropic magnet compact.
A method for making an isotropic permanent magnet, comprising the steps of:
- a) atomizing a melt of rare earth-transition metal alloy to produce generally spherical, rapidly solidified alloy powder in a range of particle sizes,
- b) coating the atomized particles with an environmentally protective coating thereon by contact with a reactive gas downstream of the atomizing location,
- c) separating the atomized alloy powder into one or more particle size fractions, and
- d) subjecting the atomized powder of a particular size fraction to concurrent elevated temperature and elevated isotropic pressure for a time effective to produce particle-to-particle binding and improved magnetic properties as compared to as-atomized particle magnetic properties so as to yield a densified, interparticle-bonded magnetically isotropic magnet compact.
A method of making an isotropic permanent magnet, comprising the steps of:
- a) atomizing a melt of a rare earth-iron-boron alloy to produce rapidly solidified, generally spherical alloy powder in a range of particle sizes,
- b) coating the atomized particles with an environmentally protective coating thereon by contact with a reactive gas downstream of the atomizing location,
- c) separating the atomized alloy powder into one or more particle size fractions, and
- d) subjecting the atomized powder of a particular size fraction to concurrent elevated temperature and elevated isotropic pressure for a time effective to produce particle-to-particle bonding and improved magnetic properties as compared to as-atomized particle magnetic properties so as to yield a densified, interparticle-bonded, magnetically isotropic magnet compact.
Dependencies are inferred from the claim text.