Friction welding method with induction heat treating
AssigneeSociete Nationale d'Etude et de Construction de Motors d'Aviation "S.N.E.C.M.A."
InventorsJean-Pierre Ferte, Francois Pierquin
Life of this patent
Estimating the term…
Abstract
A method and an apparatus for friction welding two elements together are disclosed in which the areas of the two elements to be welded are heated by an induction heater. The induction heater may be used to heat the areas to be welded prior to contact between the elements, during such contact, and after the friction welding has been achieved in order to provide a heat treatment of the welded zone. The induction heater is generally annular in shape and may be dimensioned so as to be located around the elements at the welding zone, or to be placed between the surfaces of the elements to be welded together.
Claims2
In a method of friction welding two elements of precipitation-hardened nickel-based super alloy together having the steps of:
- orienting the elements such that surfaces to be friction welded face each other;
- holding one of the elements stationary;
- rotating the other of the elements;
- and bringing the elements into contact with each other such that the contacting surfaces are welded together, the improvement comprising the step of providing means to heat the elements in the areas adjacent to the surfaces to be welded, and the additional step of heating the elements in areas adjacent to the welded surfaces after the friction welding is completed to a temperature between 1,100.degree. and 1,500.degree. C. for between 15 and 60 minutes.
Dependencies are inferred from the claim text.