Foam concentrate
AssigneeChubb National Foam, Inc.
InventorsLouis R. DiMaio, Peter J. Chiesa, Jr.
Life of this patent
Estimating the term…
Abstract
An improved foamable protein hydrolysate based concentrate is provided containing multivalent cations and a water soluble polymer, which remains stable in storage for at least six months and which, when diluted with 10 to 50 parts of water and mixed with air to generate a foam, produces a foam which lasts essentially unchanged for at least three days.
Claims24
A foamable concentrate composition comprising 300 to 900 parts protein hydrolysate, 15 to 60 parts of a metal based salt;
- 5 to 50 parts of a polysaccharide polymer selected from the group consisting of xanthan gum, algin, scleroglucan, welan gum, gellan gum, gum arabic, gum tragacanth, carrageenan, rhamson gum, and polysaccharide PS-7, and a combination of said polymers;
- 1-30 parts of an imbibing agent;
- and 10 to 40 parts of a cosolvent in which the polymer is essentially insoluble;
- which concentrate remains stable in storage for at least six months and which when diluted with 10 to 50 parts of water produces a foam which lasts for at least three days.
A foamable concentrate composition which remains stable in storage for at least six months and which when diluted with 10 to 50 parts of water produces a foam which lasts for at least three days, comprising the following ingredients in the percentages indicated by weight:
- ______________________________________ protein hydrolysate 40-80 ammonium hydroxide 0-5 hexylene glycol 0-4 sodium lignosulfonate 0-10 ferrous chloride (29% sol) 6-18 N-methyl-2-pyrrolidone 1.5-3.5 xanthan gum 1.5-3.5 ammonium thiocyanate 1-3 ______________________________________
A method for making a foamable concentrate composition comprising 300 to 900 parts protein hydrolysate, 15 to 60 parts of a metal based salt and 5 to 50 parts of a polysaccharide polymer, which concentrate remains stable in storage for at least six months and which, when diluted with 10 to 50 parts of water and mixed with air to generate a foam, produces a foam which lasts essentially unchanged for at least three days, which method comprises the following steps:
- a) first mixing the metal based salt with the protein hydrolysate;
- and
- b) combining the mixture obtained in a) above with a suitable imbibing agent prior to adding the polymer.