Abstract
An improved, extended lifetime collimator for cathode sputtering has a plurality of passages which taper longitudinally from a target side of the collimator to a wafer side of the collimator. This longitudinal tapering reduces the adverse effects on collimator useful life and wafer deposition rate which are generally caused by the accumulation of sputtered particles on exposed surfaces on the target side of the collimator. Compared to prior collimators, this collimator may be used to sputter coat a greater number of wafers before replacement or cleaning is necessary, thereby enhancing throughput capability.
Claims13
A sputter coating apparatus comprising:
- an evacuable chamber;
- a sputter target mounted in said chamber;
- a wafer mounted to said chamber opposite said target;
- and
- a collimator mounted between said target and said wafer, said collimator being spaced away from the wafer and said collimator having a plurality of passages which extend therethrough, each of said passages having a relatively large transverse cross sectional are entrance on a target side of the collimator and a relatively small transverse cross sectional area exit on a wafer side of the collimator, said passages tapering longitudinally from said relatively large transverse cross sectional area entrance to said relatively small transverse cross sectional area exit, the greatest transverse cross sectional area of each of the passages being smaller than the surface area of deposition on the wafer.
A sputter coating apparatus comprising:
- an evacuable chamber;
- a sputter target mounted in said chamber;
- a water mounted in said chamber opposite said target;
- and
- a collimator mounted between said target and said wafer, said collimator being spaced away from the wafer and said collimator having a plurality of open unit cells which permit the passage therethrough of sputtered particles from said target to said wafer, said unit cells being trapezoidal in longitudinal cross section and having a smallest effective transverse cross sectional open area at a wafer end of said collimator, the greatest transverse cross sectional open area of each of the unit cells being smaller than the surface area of deposition on the wafer.
A method of sputter coating a wafer comprising the steps of:
- placing a collimator between a target and a wafer in a sputter coating chamber so that the collimator is spaced from both the target and the wafer, the collimator having a plurality of passages therethrough defined by internal walls, said internal walls having a lesser thickness at a target side of the collimator than at a wafer side of the collimator so that each of said passages tapers inwardly in a longitudinal direction from said target to said wafer, the greatest transverse cross sectional area of each of the passages being less than the surface area of deposition on the wafer;
- and
- sputtering particles from said target to said water and intercepting some of said sputtered particles upon contact with said internal walls of said collimator and allowing some of said sputtered particles to pass through said tapered passages.
A wafer processing component for use during sputter coating of a wafer mounted opposite a target in a sputtering chamber comprising:
- a collimator having a plurality of passages which permit sputtered particles to pass therethrough from the target to the wafer, said passages tapering inwardly continuously in a longitudinal direction from a target side to a wafer side of the collimator, and the greatest transverse cross sectional area of each of the passages being less than the surface area of deposition on the wafer.
Dependencies are inferred from the claim text.