Light-weight polyester film and process for its production
AssigneeUnitika Ltd.
InventorsKenji Yasue, Eiji Y. Yamamoto, Katsuyuki Toma, Minoru Kishida, Yoshiaki Kozuka
Life of this patent
Estimating the term…
Loading patent…
AssigneeUnitika Ltd.
InventorsKenji Yasue, Eiji Y. Yamamoto, Katsuyuki Toma, Minoru Kishida, Yoshiaki Kozuka
Estimating the term…
A light-weight polyester film which comprises (A) from 50 to 95% by weight of a crystalline polyester resin and (B) from 5 to 50% by weight of a maleimide copolymer, said maleimide copolymer being dispersed in the film in the form of particles having diameters of from 0.1 to 20 .mu.m and fine voids being present in the film, and which has an apparent specific gravity of from 0.3 to 1.1, wherein said maleimide copolymer comprises from 30 to 50 mol % of a maleimide monomer group, from 30 to 70 mol % of an aromatic vinyl monomer group, from 0 to 40 mol % of an unsaturated dicarboxylic anhydride monomer group and from 0 to 40 mol % of other copolymerizable monomer group, and said maleimide copolymer has a glass transition temperature higher by at least 10.degree. C. than the crystalline polyester resin.
A light-weight polyester film which comprises (A) from 50 to 95% by weight of a crystalline polyester resin and (B) from 5 to 50% by weight of a maleimide copolymer, said maleimide copolymer being dispersed in the film in the form of particles having diameters of from 0.1 to 20 .mu.m and fine voids being present in the film, and which has an apparent specific gravity of from 0.3 to 1.1, wherein said maleimide copolymer comprises from 30 to 50 mol % of a maleimide monomer group, from 30 to 70 mol % of an aromatic vinyl monomer group, from 0 to 40 mol % of an unsaturated dicarboxylic anhydride monomer group and from 0 to 50 mol % of other copolymerizable monomer group, and said maleimide copolymer has a glass transition temperature higher by at least 10.degree. C. than the crystalline polyester resin.
A process for producing a light-weight polyester film, which comprises melt-extruding a composition comprising (A) from 50 to 95% by weight of a crystalline polyester resin and (B) from 5 to 50% by weight of a maleimide copolymer to obtain an unstretched polyester film, and at least monoaxially stretching the polyester film at least 1.5 times within a temperature range of at least the glass transition temperature of the crystalline polyester resin and at most the crystallization temperature of the crystalline polyester resin.
Dependencies are inferred from the claim text.