# US 5,202,384 A · Polyester reinforced rubber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,202,384 A
- Document ID: US5202384A
- Status: Granted
- Kind: A
- Application number: 07/609,858
- Filed: 1990-11-07
- Granted: 1993-04-13
- Earliest claimed: 1989-03-27
- Assignees: The Goodyear Tire & Rubber Company
- Inventors: James B. Pyle; Richard G. Bauer; Donald J. Burlett
- Web page: https://patentgrep.com/patent/US5202384A

## CPC

- C08G 81/027: {containing polyester or polycarbonate sequences}
- C08C 19/40: with epoxy radicals
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS

## Abstract

It is often desirable to increase the modulus of rubbers utilized in a wide variety of applications. This invention discloses a technique for modifying rubbers to improve their modulus without sacrificing other properties. By utilizing the process of this invention, rubber compositions having increased modulus are prepared by grafting polyester onto rubber. This can be accomplished by reacting a polydiene rubber with a thioacid or maleic anhydride and subsequently with the polyester. It is also possible to prepare such polyester modified rubber compositions by reacting an epoxidized rubber with the polyester.

## Claims

### Claim 1

A process for preparing a rubber composition having a high modulus which comprises reacting at least one dithio diacid having the structural formula HOOC--A-S-S-A--COOH, wherein A represents an alkylene group containing from 1 to about 10 carbon atoms with at least one polydiene rubber and at least one polyester elastomer having a melting point of less than about 240.degree. C.

### Claim 2 (depends on 1)

A process as specified in claim 1 which is carried out by reacting the dithio diacid with the polyester to form a modified polyester containing mercaptan groups; and subsequently reacting the modified polyester containing mercaptan groups with the polydiene rubber.

### Claim 3 (depends on 2)

A process as specified in claim 2 wherein the dithio diacid is reacted with the polyester at a temperature which is within the range of about 150.degree. C. to about 300.degree. C. and wherein the modified polyester containing mercaptan groups is reacted with the polydiene rubber at a temperature which is within the range of about 120.degree. C. to about 250.degree. C.

### Claim 4 (depends on 1)

A process as specified in claim 1 wherein said polydiene rubber is selected from the group consisting of polybutadiene, styrene-butadiene rubber, synthetic polyisoprene, natural rubber, isoprene-butadiene rubber, isoprene-buadiene-styrene rubber, nitrile rubber, and EPDM rubber.

### Claim 5 (depends on 3)

A process as specified in claim 3 wherein from about 0.5 parts per hundred parts of polydiene rubber to about 3 parts per hundred parts of polydiene rubber of the dithio diacid is utilized.

### Claim 6 (depends on 5)

A process as specified in claim 5 wherein said dithio diacid is dithio dipropionic acid.

### Claim 7 (depends on 1)

The rubber composition made by the process specified in claim 1.