A line for continuously annealing and pickling a stainless steel strip comprising: a drying/temperature adjusting zone, provided between a water cooling zone and a tank containing a neutral salt electrolytic solution, including hot air jetting means which controls the temperature and amount of hot air so as to dry the stainless steel strip after the stainless steel strip is cooled with water and uniformly heat the temperature of the material of the stainless steel strip.
A line for continuously annealing and pickling a stainless steel strip comprising:
Dependencies are inferred from the claim text.
Drawings are temporarily unavailable. Open the PDF at USPTO
No related US applications are recorded in the indexed filing history.
No references of this kind are recorded.
Term ended 19 Mar 2012 (estimated)
USPTO file history isn’t available for this patent, so only indexed dates are shown.
1. Field of the Invention
The present invention relates to a line for continuously annealing and pickling a stainless steel strip.
2. Description of the Related Arts
These and other objects and features of the present invention will become apparent from the following description taken in conjunction with the preferred embodiments thereof with reference to the accompanying drawings, in which:
FIG. 1 is a front view showing a principal portion of a line for continuously annealing and pickling a stainless steel strip according to the present invention;
FIG. 2 is a sectional view taken along a line II--II of FIG. 1;
Before the description of the present invention proceeds, it is to be noted that like parts are designated by like reference numerals throughout the accompanying drawings.
An embodiment of the present invention will be described below with reference to FIGS. 1, 2, and 3.
As apparent from FIG. 1, in the line for continuously annealing and pickling a stainless steel strip (S), a drying/temperature adjusting zone 10 is provided between the spray type water cooling zone 1 and the tank 6 containing a neutral salt electrolytic solution.