US 5,149,687 AGranted
Method for making oriented bismuth and thallium superconductors comprising cold pressing at 700 MPa
AssigneeUnited Technologies Corporation
InventorFrancis S. Galasso
Life of this patent
Estimating the term…
Abstract
An oriented superconducting material may be made by cold pressing a nonoriented superconducting material selected from the group consisting of Bi.sub.1, Bi.sub.2, Tl.sub.1, Tl.sub.2, Pb substituted Bi.sub.1, Pb substituted Bi.sub.2, Pb substituted Tl.sub.1, and Pb substituted Tl.sub.2 superconductor materials at a pressure sufficient to form an oriented superconducting material.
Claims4
A method for making an oriented superconducting material, comprising:
- cold pressing a nonoriented superconducting material selected from the group consisting of Bi.sub.1, Bi.sub.2, Tl.sub.1, Tl.sub.2, Pb substituted Bi.sub.1, Pb substituted bi.sub.2, Pb substituted Tl.sub.1, and Pb substituted Tl.sub.2 superconductor materials at a pressure of at least about 700 MPa to form an oriented superconducting material that has a ratio of x-ray refection intensity from the (0010) plane to the reflection intensity from the (105) plane of 1.6 or greater.
Dependencies are inferred from the claim text.