# US 5,122,204 A · Camshafts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,122,204 A
- Document ID: US5122204A
- Status: Granted
- Kind: A
- Application number: 07/679,185
- Filed: 1991-04-02
- Granted: 1992-06-16
- Earliest claimed: 1991-04-02
- Assignees: Lydmet Limited
- Inventors: Alexander K. McDonald
- Web page: https://patentgrep.com/patent/US5122204A

## CPC

- B22D 15/00: Casting using a mould or core of which a part significant to the process is of high thermal conductivity, e.g. chill casting; Moulds or accessories specially adapted therefor
- B22D 25/02: by its peculiarity of shape; of works of art {(cylinders, pistons B22D15/02)}
- Y10S 148/904: Crankshaft
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method of producing a chilled iron camshaft is described, wherein the iron has a white iron structure adjacent chill inserts in a casting mould and a grey iron structure in substantially all other regions remote from the chills. The method comprises the steps of assembling a sand casting mould having a camshaft shaped cavity and also having chill inserts adjacent the cavity regions where while iron is desired, preparing a molten metal charge of cast iron having a carbon equivalent lying in the range from 3.3 to 3.85 wt % and adding sufficient nucleant prior to pouring to fill the mould cavity to ensure that undercooling of residual liquid remaining after solidification of the white iron structure adjacent the chills remains above the iron-cementite eutectic temperature prior to solidfication into grey iron.

## Claims

### Claim 1

A method of producing a chilled iron camshaft, the iron having a white iron structure adjacent chill inserts in a casting mould and a grey iron structure in substantially all other regions remote from the chills, the method comprising the steps of assembling a sand casting mould having a camshaft shaped cavity and also having chill inserts adjacent the cavity regions where white iron is desired, preparing a molten metal charge of cast iron having a carbon equivalent lying in the range from 3.3 to 3.85 wt% and adding nucleant prior to pouring, and pouring the molten metal to fill the mould cavity to form the camshaft, wherein said range of carbon equivalent and said nucleant addition are sufficient to ensure that undercooling of residual liquid remaining after solidification of the white iron structure adjacent the chills remains above the iron-cementite eutectic temperature prior to solidification into grey iron.

### Claim 2 (depends on 1)

A method according to claim 1 wherein the carbon equivalent includes from 2.9 to 3.4 wt% of carbon.

### Claim 3 (depends on 2)

A method according to claim 2 wherein the carbon equivalent remainder is substantially silicon.

### Claim 4 (depends on 1)

A camshaft when made by the method claim 1.