# US 5,085,804 A · Refractory electrical device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,085,804 A
- Document ID: US5085804A
- Status: Granted
- Kind: A
- Application number: 07/659,648
- Filed: 1991-02-25
- Granted: 1992-02-04
- Earliest claimed: 1984-11-08
- Assignees: Norton Company
- Inventors: Malcolm E. Washburn
- Web page: https://patentgrep.com/patent/US5085804A

## CPC

- C04B 35/645: Pressure sintering
- C04B 35/565: based on silicon carbide
- C04B 35/58092: {based on refractory metal silicides}
- C04B 35/581: based on aluminium nitride
- C04B 35/583: based on boron nitride
- C04B 35/584: based on silicon nitride
- C04B 35/593: obtained by pressure sintering
- F23Q 7/22: Details
- H01C 7/042: {mainly consisting of inorganic non-metallic substances (H01C7/041 takes precedence)}
- H05B 3/148: {Silicon, e.g. silicon carbide, magnesium silicide, heating transistors or diodes}
- C04B 2235/75: Products with a concentration gradient
- H05B 2203/018: Heaters using heating elements comprising mosi2
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F23Q: IGNITION (devices or installations peculiar to internal-combustion engines F02P; of cigarettes or tobacco A24F; compositions therefor, chemical igniters C06C); EXTINGUISHING-DEVICES
- H01C: RESISTORS
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL

## Abstract

The present invention is an electrical device made up of a mixture of silicon carbide and molybdenum disilicide, and may include silicon nitride or aluminum nitride or boron nitride. An electrical device is also disclosed which is particularly suited for use as an igniter in liquid and gas fuel burning systems. The device is made up of a sintered, preferably hot-pressed, mixture of fine powders of aluminum nitride or silicon nitride, silicon carbide and molybdenum disilicide where, when all three are present, they are present in substantial quantities.

## Claims

### Claim 1

An igniter for fluid fuels comprised of a hot zone and cold ends consisting essentially of a sintered mixture of 5 to 50% by volume of molybdenum disilicide and 50 to 95% by volume of a mixture of silicon carbide and silicon nitride; 4% or less of open porosity, a room temperature flexural strength of at least 30,000 psi (207 MPa), a resistivity range of from 0.0001 to 90 ohm centimeters, a ratio of room temperature resistivity to that at 1200.degree. C. of from 0.2 to 19.8, a response time from room temperature to about 1200.degree. C. of less than 25 seconds, said igniter consuming from about 20 to about 50 watts per square centimeter of radiating surface at 1200.degree. C.

### Claim 2 (depends on 1)

The igniter of claim 1 wherein said igniter consists essentially of 30% to 70% by volume of a silicon nitride, 5% to 40% by volume of silicon carbide, 5% to 50% by volume of molybdenum disilicide, and 0 to 3% by weight of a sintering aid.

### Claim 3 (depends on 1)

The igniter of claim 1 wherein the composition varies from the hot zone to the cold ends such that said cold ends are made up of all molybdenum disilicide.

### Claim 4 (depends on 3)

The igniter of claim 3 wherein the composition changes gradually from hot zone to cold ends.

### Claim 5 (depends on 3)

The igniter of claim 3 wherein the composition varies abruptly from hot zone to cold ends.

### Claim 6 (depends on 3)

The igniter of claim 3 having cold ends and a hot zone with a resistivity differential therebetween which is the result of said cold ends being made up of 30% to 70% by volume of said nitride, 5% to 30% by volume of silicon carbide, and 30% to 50% by volume of molybdenum disilicide; and said hot zone is made up of 30% to 70% by volume of said nitride, 10% to 40% by volume of silicon carbide, and 5% to 20% by volume of molybdenum disilicide.

### Claim 7 (depends on 3)

The igniter of claim 3 wherein said igniter is formed from 40% to 70% by volume of silicon nitride powder having an average particle size of about 3 microns, 10% to 40% by weight of silicon carbide having an average particle size of about 3 microns, 5% to 30% by weight of molybdenum disilicide having a particle size of about 3 microns and 0.5% to 3.0% by weight of a source of magnesium oxide having an average particle size of about 3 microns, and wherein said igniter has a density of at least 2.62 Mg/M.sup.3.

### Claim 8 (depends on 1)

The igniter of claim 1 having cold ends and a hot zone wherein the resistance differential between the cold ends and the hot zone is a result of the cold ends having a volume 5 to 10 times greater than the volume of the hot zone.

### Claim 9 (depends on 1)

The igniter of claim 1 which is provided with a protective mixed oxide coating.

### Claim 10 (depends on 1)

The igniter of claim 1 which includes a protective coating thereon selected from the group consisting of silica, silicon oxynitride and silicon nitride.

### Claim 11 (depends on 1)

The igniter composition of claim 1 made up of two separate but intertwined structures including a first dense continuous phase made up of silicone nitride and a second dense continuous phase made up of a mixture of silicon carbide and molybdenum disilicide.