# US 5,075,360 A · High-speed starch-based corrugating adhesive containing a carrier phase comprised of starch, modified starch or dextrin and polyvinyl alcohol

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,075,360 A
- Document ID: US5075360A
- Status: Granted
- Kind: A
- Application number: 07/563,379
- Filed: 1990-08-06
- Granted: 1991-12-24
- Earliest claimed: 1990-08-06
- Assignees: CPC International Inc.
- Inventors: Larry E. Fitt; James J. Pienkowski; Jack R. Wallace
- Web page: https://patentgrep.com/patent/US5075360A

## CPC

- C09J 103/00: Adhesives based on starch, amylose or amylopectin or on their derivatives or degradation products
- C09J 103/10: Oxidised starch
- C08L 2666/02: Organic macromolecular compounds, natural resins, waxes or and bituminous materials
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A high speed corrugating adhesive having a carrier phase comprised of starch, modified starch or dextrin and polyvinyl alcohol in an aqueous emulsion wherein a cold water soluble, partially hydrolyzed, polyvinyl alcohol is used as a starting material. The polyvinyl alcohol is further hydrolyzed in situ to a degree of hydrolysis of more than about 95% by heating it in the presence of water, caustic, and starch, modified starch or dextrin. The carrier phase is admixed with a boron containing compound and a suspension of water and starch to prepare the corrugating adhesive for use in a corrugating machine.

## Claims

### Claim 1

A corrugating adhesive composition which in an aqueous emulsion comprises water; about 0.04 to about 3 parts per 100 parts of adhesive of a cold water soluble polyvinyl alcohol which has been hydrolyzed in situ to a degree of hydrolysis of more than about 95%; about 2 to about 10 parts per 100 parts of the corrugating adhesive composition of a component selected from the group consisting of starch, modified starch and dextrin; sufficient caustic to provide an alkaline pH; about 10 to about 30 parts of starch per 100 parts of the corrugating adhesive composition; and about 0.3 to about 1 part of a boron containing compound .per 100 parts of the corrugating adhesive composition.

### Claim 2 (depends on 1)

The composition of claim 1 wherein the polyvinyl alcohol has a degree of hydrolysis of less than about 92% prior to hydrolysis in situ.

### Claim 3 (depends on 1)

The composition of claim 1 wherein the polyvinyl alcohol has a degree of hydrolysis of less than about 88% prior to hydrolysis in situ.

### Claim 4 (depends on 3)

The composition of claim 3 wherein the polyvinyl alcohol has a molecular weight of less than about 15,000 molecular weight units.

### Claim 5 (depends on 4)

The composition of claim 4 further including a resin for waterproofing or water resistance in an amount from about 0.5 to about 5 parts resin per 100 parts of adhesive.

### Claim 6

A carrier phase composition for use in a corrugating adhesive composition which in an aqueous emulsion comprises water; about 0.1 to about 10 parts per 100 parts of the carrier phase composition of a cold water soluble polyvinyl alcohol which has been hydrolyzed in situ to a degree of hyrdolysis of more than about 95%; about 5 to about 30 parts per 100 parts of the carrier phase composition of a component selected from the group consisting of starch, modified starch and dextrin; and sufficient caustic to provide an alkaline pH.

### Claim 7 (depends on 6)

The composition of claim 6, further comprising from about 0.03 to about 1 part of a boron containing compound per 100 parts of the carrier phase composition.

### Claim 8 (depends on 4)

The composition of claim 4 wherein the polyvinyl alcohol has a degree of hydrolysis of less than about 92% prior to hydrolysis in situ.

### Claim 9 (depends on 7)

The composition of claim 7 wherein the polyvinyl alcohol has a degree of hydrolysis of less than about 88% prior to hydrolysis in situ.

### Claim 10 (depends on 9)

The composition of claim 9 wherein the polyvinyl alcohol has a molecular weight of less than about 15,000 molecular weight units.