Composition for inhibiting stress cracks in plastic articles and methods of use therefor
AssigneeDiversey, Inc.
InventorsCharles E. Rossio, Theodore E. Anderson
Life of this patent
Estimating the term…
Abstract
Stress cracking in poly(alkylene terephthalate) articles of manufacture is inhibited by applying to the article a stress crack inhibitor which contains an amine having at least 6 carbon atoms. In a preferred embodiment, the stress crack inhibitor is applied to the article in the form of an aqueous fatty acid-based lubricant.
Claims15
A method of inhibiting stress cracking in a poly(alkylene terephthalate) article, comprising the step of applying a composition comprising an amine to a surface of the article, the amine having at least 6 carbon atoms.
A method of inhibiting stress cracking in a poly(alkylene terephthalate) article, comprising a step of applying a composition to a surface of the article, the composition comprising:
- (a) an alkyl amine having from 2-12 carbon atoms, and
- (b) an aryl sulfonate.
A method of inhibiting stress cracking in a poly(alkylene terephthalate) article of manufacture, comprising a step of applying a dilute aqueous-based lubricant use solution to an exterior surface of the article, the use solution comprising an alkyl amine having at least 6 carbon atoms, a fatty acid or a mixture of fatty acids, a sequestrant, and water.
A method of inhibiting stress cracking in a poly(alkylene terephthalate) container, comprising adding an amine having at least 6 carbon atoms to the interior of the container.
An aqueous-based fatty acid lubricant concentrate, comprising:
- (a) a long-chain fatty acid;
- (b) an alkyl amine having at least 6 carbon atoms;
- (c) a sequestrant;
- and
- (d) water.