# US 5,019,311 A · Process for the production of materials characterized by a continuous web matrix or force point bonding

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 5,019,311 A
- Document ID: US5019311A
- Status: Granted
- Kind: A
- Application number: 07/455,997
- Filed: 1989-12-22
- Granted: 1991-05-28
- Earliest claimed: 1989-02-23
- Assignees: Koslow Technologies Corporation
- Inventors: Evan E. Koslow
- Web page: https://patentgrep.com/patent/US5019311A

## CPC

- B29C 70/58: comprising fillers only {, e.g. particles, powder, beads, flakes, spheres (B29C70/025 takes precedence, agglomerating hollow spheres to produce synthetic foam B29C70/66; compounding ingredients per se C08K)}
- B29C 67/243: {for making articles of definite length}
- B29C 43/00: Compression moulding, i.e. applying external pressure to flow the moulding material; Apparatus therefor {(by liberation of internal stresses B29C61/006)}
- B29K 2105/251: {Particles, powder or granules (expandable particles B29K2105/046)}
- Y10S 264/48: Processes of making filters
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- Y10T 428/2991: Coated
- Y10T 428/2993: Silicic or refractory material containing [e.g., tungsten oxide, glass, cement, etc.]
- Y10T 428/2996: Glass particles or spheres
- Y10T 428/2998: including synthetic resin or polymer
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method of forming a composite material by providing a quantity of first particles of a binder material and a quantity of second particles of a primary material having softening temperature substantially in excess of the softening temperature of the binder material. The first and second quantities of particles are combined into a substantially uniform mixture. The uniform mixture is heated in the absence of pressure or shear sufficient to convert the binder particles, to a temperature substantially above the softening point of the binder material but less than the softening temperature of the primary material. Thereafter, pressure and shear are applied to the heated mixture sufficient substantially immediately to convert at least a portion of the binder material particles into a substantially continuous webbing structure or force the formation of point-bonds. Substantially immediately after formation of the binder particles into this unique structure, the mixture is rapidly cooled to below the softening point of the binder material to retain the converted binder material in its continuous form or forced point-bonded condition. This produces the composite material composed of primary particles, a binder resin phase forming a continuous web matrix or point bonds, and a volume of empty pores. Also disclosed are products formed by the method.

## Claims

### Claim 1

A method of forming a composite material which comprises:
providing a quantity of first particles of a binder material, said first particles having diameters between about 0.1 and about 150 micrometers;
providing a quantity of second particles of a primary material having a softening temperature substantially greater than the softening temperature of said binder material, said second particles having diameters between about 0.1 and about 3,000 micrometers;
combining the first and second quantities of particles in a substantially uniform mixture wherein said binder material is present in an amount of at least about 3% by weight of the mixture;
heating said substantially uniform mixture, in the absence of pressure or shear sufficient to convert the binder particles into a continuous phase through the composite material, to a temperature substantially above the softening temperature of said binder material but to a temperature less than the softening temperature of said primary material;
thereafter applying pressure and shear to the heated mixture sufficient substantially immediately to convert at least a portion of the binder material particles into a substantially continuous webbing structure through the composite material; and
substantially immediately after formation of said continuous binder structure, rapidly cooling said mixture to below the softening point of the binder material to retain said converted binder material in its continuous webbing structure condition to produce the composite material.

### Claim 2 (depends on 1)

The method of claim 1 wherein said binder material is present in the mixture in an amount of about 3 to about 30% by weight of the total composition.

### Claim 3 (depends on 2)

The method of claim 2 wherein said binder material is present in an amount of about 4 to about 8% by weight.

### Claim 4 (depends on 1)

The method of claim 1 wherein said substantially uniform mixture is heated to a temperature at least about 25.degree. C. above the softening temperature of said binder material.

### Claim 5 (depends on 4)

The method of claim 4 wherein said substantially uniform mixture is heated to at least about 50.degree. C. above the softening temperature of the binder material.

### Claim 6 (depends on 1)

The method of claim 1 wherein the pressure applied to the heated mixture is at least about 500 psi (35 kg/cm.sup.2).

### Claim 7 (depends on 6)

The method of claim 6 wherein said pressure is at least about 6,000 psi (422 kg/cm.sup.2).

### Claim 8 (depends on 2)

The method of claim 2 wherein said substantially uniform mixture is heated to a temperature at least about 25.degree. C. above the softening temperature of said binder material.

### Claim 9 (depends on 8)

The method of claim 8 wherein said pressure is at least about 6000 psi (422 kg/cm.sup.2).

### Claim 10 (depends on 3, 7, 8, 9)

The method of claims 3, 7, 8 or 9 wherein the substantially uniform mixture is heated to a temperature at least about 50.degree. C. above the softening temperature of the binder material.

### Claim 11 (depends on 1, 3, 5, 7, 9)

The method of claims 1, 3, 5, 7 or 9 wherein said binder material is a crystalline polymer.

### Claim 12 (depends on 1, 3, 5, 7, 9)

The method of claims 1, 3, 5, 7 or 9 wherein said binder material is a thermoplastic polymer.

### Claim 13 (depends on 1, 3, 5, 7, 9)

The method of claims 1, 3, 5, 7 or 9 wherein said binder material is a crystalline thermoplastic polymer.

### Claim 14 (depends on 1, 3, 5, 7, 9)

The method of claims 1, 3, 5, 7 or 9 wherein said binder material is a crystalline thermoplastic polymer selected from the group consisting of polyolefins, polyvinyls, polyvinyl esters, polyvinyl ethers, polyvinyl sulfates, polyvinyl phosphates, polyvinyl amines, polyoxidiazoles, polytriazols, polycarbodiimides, ethylene-vinyl acetate copolymers, polysulfones, polycarbonates, polyethers, polyarylene oxides, and polyesters.

### Claim 15 (depends on 8)

The method of claim 8 wherein said binder material is a crystalline thermoplastic polymer selected from the group consisting of polyolefins, polyvinyls, polyvinyl esters, polyvinyl ethers, polyvinyl sulfates, polyvinyl phosphates, polyvinyl amines, polyoxidiazoles, polytriazols, polycarbodiimides, ethylene-vinyl acetate copolymers, polysulfones, polycarbonates, polyethers, polyarylene oxides, and polyesters.

### Claim 16 (depends on 15)

The method of claim 15 wherein said binder material is polyethylene.

### Claim 17 (depends on 15)

The method of claim 15 wherein said binder material is polypropylene.

### Claim 18 (depends on 15)

The method of claim 15 wherein said binder material is polybutene-1.

### Claim 19 (depends on 15)

The method of claim 15 wherein said binder material is poly4-methylpentene-1.

### Claim 20 (depends on 15)

The method of claim 15 wherein said binder material is polyvinyl chloride.

### Claim 21 (depends on 15)

The method of claim 15 wherein said binder material is polyvinyl fluoride.

### Claim 22 (depends on 15)

The method of claim 15 wherein said binder material is polyvinylidene chloride.

### Claim 23 (depends on 15)

The method of claim 15 wherein said binder material ester is polyvinyl acetate.

### Claim 24 (depends on 15)

The method of claim 15 wherein said binder material ester is polyvinyl proportionate.

### Claim 25 (depends on 15)

The method of claim 15 wherein said binder material ester is polyvinyl pyrrolidone.

### Claim 26 (depends on 15)

The method of claim 15 wherein said binder material is an ethylene polymer selected from the group consisting of polyethylene or an ethylene-vinyl acetate copolymer.

### Claim 27 (depends on 3)

The method of claim 3 wherein said binder material is an ethylene polymer selected from the group consisting of polyethylene or an ethylene-vinyl acetate copolymer.

### Claim 28 (depends on 5)

The method of claim 5 wherein said binder material is an ethylene polymer selected from the group consisting of polyethylene or an ethylene-vinyl acetate copolymer.

### Claim 29 (depends on 7)

The method of claim 7 wherein said binder material is an ethylene polymer selected from the group consisting of polyethylene or an ethylene-vinyl acetate copolymer.

### Claim 30 (depends on 9)

The method of claim 9 wherein said binder material is an ethylene polymer selected from the group consisting of polyethylene or an ethylene-vinyl acetate copolymer.

### Claim 31 (depends on 15)

The method of claim 15 wherein said binder material is a polysulfone.

### Claim 32 (depends on 15)

The method of claim 15 wherein said binder material is a polycarbonate.

### Claim 33 (depends on 15)

The method of claim 15 wherein said binder material is polyethylene oxide.

### Claim 34 (depends on 15)

The method of claim 15 wherein said binder material is polymethylene oxide.

### Claim 35 (depends on 15)

The method of claim 15 wherein said binder material is polypropylene oxide.

### Claim 36 (depends on 15)

The method of claim 15 wherein said binder material is a polyarylate.

### Claim 37 (depends on 15)

The method of claim 15 wherein said binder material is polyethylene terephthalate.

### Claim 38 (depends on 15)

The method of claim 15 wherein said binder material is a polyimide.
substantially immediately after formation of the binder continuous phase, rapidly cooling said mixture to below the softening point of the binder material to retain said converted binder material in its continuous condition to produce the composite material.

### Claim 39 (depends on 15)

The method of claim 15 wherein said primary material is metal.

### Claim 40 (depends on 39)

The method of claim 39 wherein said metal is ferromagnetic material.

### Claim 41 (depends on 40)

The method of claim 40 wherein said material is a stainless steel.

### Claim 42 (depends on 15)

The method of claim 15 wherein said primary material comprises a silica gel.

### Claim 43 (depends on 42)

The method of claim 42 wherein said primary material comprises a magnetic stainless steel.

### Claim 44 (depends on 15)

The method of claim 15 wherein said primary material comprises an ion-exchange resin.

### Claim 45 (depends on 44)

The method of claim 44 wherein said primary material comprises a magnetic stainless steel.

### Claim 46 (depends on 44)

The method of claim 44 wherein said primary material comprises organic fibers.

### Claim 47 (depends on 46)

The method of claim 46 wherein said fibers are cellulose.

### Claim 48 (depends on 46)

The method of claim 46 wherein said fibers are acrylic.

### Claim 49 (depends on 15)

The method of claim 15 wherein said primary material comprises a diatomaceous earth.

### Claim 50 (depends on 49)

The method of claim 49 wherein said primary material comprises organic fibers.

### Claim 51 (depends on 50)

The method of claim 50 wherein said fibers are acrylic.

### Claim 52 (depends on 50)

The method of claim 50 wherein said fibers are cellulose.

### Claim 53 (depends on 15)

The method of claim 15 wherein said primary material comprises an abrasive.

### Claim 54 (depends on 53)

The method of claim 53 wherein said abrasive is glass.

### Claim 55 (depends on 53)

The method of claim 53 wherein said abrasive is selected from the group consisting of silicon carbide or alumina.

### Claim 56 (depends on 53)

The method of claim 53 wherein said primary material comprises a silica.

### Claim 57 (depends on 15)

The method of claim 15 wherein said primary material comprises a polyketone.

### Claim 58 (depends on 57)

The method of claim 57 wherein said primary material comprises organic fibers.

### Claim 59 (depends on 58)

The method of claim 58 wherein said fibers are acrylic.

### Claim 60 (depends on 57)

The method of claim 57 wherein said primary material comprises a ferromagnetic metal.

### Claim 61 (depends on 60)

The method of claim 60 wherein said metal comprises a steel.

### Claim 62 (depends on 61)

The method of claim 61 wherein said metal comprises a stainless steel.

### Claim 63 (depends on 15)

The method of claim 15 wherein said primary material comprises carbon.

### Claim 64 (depends on 63)

The method of claim 63 wherein said carbon comprises activated carbon.

### Claim 65 (depends on 15)

The method of claim 15 wherein said primary material comprises metal and wherein the pressure and shear are applied to the substantially uniform mixture in a roll compactor.

### Claim 66 (depends on 65)

The method of claim 65 wherein said metal comprises a ferromagnetic steel.

### Claim 67 (depends on 66)

The method of claim 66 wherein said steel comprises a stainless steel.

### Claim 68 (depends on 65)

The method of claim 65 wherein the pressure applied to the substantially uniform mixture by said roll compactor is at least approximately 10,000 psi (703 kg/cm.sup.2).

### Claim 69 (depends on 15)

The method of claim 15 wherein said primary material comprises metal and wherein the cooling step is followed by a sintering step to substantially remove the binder material.

### Claim 70 (depends on 69)

The method of claim 69 wherein said metal comprises a steel.

### Claim 71 (depends on 70)

The method of claim 70 wherein said steel comprises a stainless steel.

### Claim 72 (depends on 70)

The method of claim 70 wherein said pressure and shear step are applied to the substantially uniform mixture by a roll compactor.

### Claim 73 (depends on 72)

The method of claim 72 wherein said metal comprises a steel.

### Claim 74 (depends on 73)

The method of claim 73 wherein said metal comprises a stainless steel.

### Claim 75 (depends on 69)

The method of claim 69 wherein said pressure and shear are applied to the substantially uniform mixture in a roll compactor and wherein said sintering step is preceded by or followed by layering the produced composite fibrous material with layers of substantially similarly produced material to form a complex material.

### Claim 76 (depends on 75)

The method of claim 75 wherein the average particle size of the primary particles in at least one layer differs from the average particle size of the primary particles in at least one other layer.

### Claim 77 (depends on 15)

The method of claim 15 wherein said primary material comprises at least two materials that are normally incompatible.

### Claim 78 (depends on 77)

The method of claim 77 wherein one of said materials comprises a ferromagnetic material.

### Claim 79 (depends on 78)

The method of claim 78 wherein another of said materials comprises an ion-exchange material.

### Claim 80 (depends on 79)

The method of claim 79 wherein said ferromagnetic material comprises a steel.

### Claim 81 (depends on 80)

The method of claim 80 wherein said steel is a stainless steel.

### Claim 82 (depends on 79)

The method of claim 79 wherein said pressure and shear are applied to the substantially uniform mixture in a roll compactor.

### Claim 83 (depends on 82)

The method of claim 82 wherein said composite material is granulated.

### Claim 84 (depends on 82)

The method of claim 82 wherein said pressure is at least approximately 10,000 psi (703 kg/cm.sup.2).

### Claim 85 (depends on 84)

The method of claim 84 wherein said composite material is granulated.

### Claim 86 (depends on 1, 3, 5, 7, 9, 15)

The method of claims 1, 3, 5, 7, 9 or 15 wherein the substantially uniform mixture is heated in the absence of significant pressure and shear.

### Claim 87 (depends on 1, 3, 5, 7, 9, 15)

The method of claims 1, 3, 5, 7, 9 or 15 wherein the heat, pressure and shear are applied in an extrusion process.

### Claim 88 (depends on 1)

The method of claim 1 wherein the method is carried out in an extrusion process in which an auger screw transports the substantially uniform mixture under essentially non-heated conditions to a first section of the die where the mixture undergoes heating, pressure and shear sufficient to convert the binder particles to a substantially continuous webbing structure and thereafter the resulting product enters a second section of the die where the product is swaged and intensively cooled.

### Claim 89 (depends on 1, 3, 5, 7)

The method of claims 1, 3, 5, 7, or 9 wherein the binder material is an amorphous or non-crystalline polymer selected from the group consisting of polystyrenes, acrylonitrile-styrene copolymers, and styrene-butadiene copolymers.

### Claim 90 (depends on 8)

The method of claim 8 wherein the binder material is an amorphous or non-crystalline polymer selected from the group consisting of polystyrenes, acrylonitrile-styrene copolymers, and styrene-butadiene copolymers.

### Claim 91 (depends on 1)

The method of claim 1 wherein the method is carried out in an extrusion process in which an auger screw transports the substantially uniform mixture under essentially non-heated conditions to a first section of the die where the mixture undergoes heating, pressure and shear sufficient to convert the binder particles to a substantially forced point-bonded structure and thereafter the resulting product enters a second section of the die where the product is swaged and intensively cooled.

### Claim 92

A method of forming a composite material which comprises:
providing a quantity of first particles of a binder material, said first particles having diameters between about 0.1 and about 150 micrometers;
providing a quantity of second particles of a primary material having a softening temperature substantially in excess of the softening temperature of said binder material, said second particles having diameters between about 0.1 and about 3,000 micrometers;
combining the first and second quantities of particles in a substantially uniform mixture wherein said binder material is present in an amount of at least about 3% by weight of the mixture;
heating said substantially uniform mixture, in the absence of pressure or shear sufficient to convert the binder particles, to a temperature about 25-100.degree. C. above the softening temperature of said binder material but less than the softening temperature of said primary material;
thereafter applying pressure of at least 4000 psi (283 kg/cm.sup.2) and shear to the heated mixture sufficient to substantially immediately convert at least a portion of the thermoplastic binder material particles into a continuous phase; and
substantially immediately after formation of the binder continuous phase, rapidly cooling said mixture to below the softening point of the binder material to retain said converted binder material in its continuous condition to produce the composite material.

### Claim 93 (depends on 1, 3, 5, 7, 9, 15, 92)

The method of claims 1, 3, 5, 7, 9, 15 or 92 wherein the pressure and shear sufficient to convert the binder particles are applied by a compression molding process.

### Claim 94

A method of forming a composite material which comprises:
providing a quantity of first particles of a binder material, said first particles having diameters between about 0.1 and about 150 micrometers;
providing a quantity of second particles of a primary material having a softening temperature substantially greater than the softening temperature of said binder material, said second particles having diameters between about 0.1 and about 3,000 micrometers;
combining the first and second quantities of particles in a substantially uniform mixture wherein said binder material is present in an amount of at least about 3% by weight of the mixture;
heating said substantially uniform mixture, in the absence of pressure or shear sufficient to convert the binder particles, to a temperature substantially above the softening temperature of said binder material but to a temperature less than the softening temperature of said primary material;
thereafter applying pressure and shear to the heated mixture sufficient to substantially immediately convert at least a portion of the binder material particles into a substantially continuous webbing structure or cause forced point-bonding of the particles of the primary material by the binder material; and
substantially immediately after formation of said binder particles into a webbing structure or forced point-bonds, rapidly cooling said mixture to below the melting point of the binder material to retain said converted binder material in its continuous webbing structure or forced point-bonded condition to produce the composite material.

### Claim 95 (depends on 94)

The method of claim 94 wherein the pressure applied causes forced point-bonding of the particles of primary material by the binder material.

### Claim 96 (depends on 95)

The method of claim 95 wherein the substantially uniform mixture is heated to a temperature at least about 25.degree. C. above the softening temperature of the binder material.

### Claim 97 (depends on 95)

The method of claim 95 wherein the pressure applied to the heated mixture is in the range of from about 500 psi (35 kg/cm.sup.2) to about 6000 psi (422 kg/cm.sup.2).

### Claim 98 (depends on 97)

The method of claim 97 wherein the pressure applied is in the range of from about 500 psi (35 kg/cm.sup.2) to about 1000 psi (70 kg/cm.sup.2).

### Claim 99 (depends on 95)

The method of claim 95 wherein the binder material is a resin that is resistant to conversion.

### Claim 100 (depends on 96)

The method of claim 96 wherein the binder material is resin selected from the group consisting of acrylic and nylon resins.

### Claim 101 (depends on 95)

The method of claim 95 wherein the binder material is a noncrystalline or amorphous polymer.

### Claim 102 (depends on 95)

The method of claim 95 wherein the primary particles are granular or powdered carbon.

### Claim 103 (depends on 102)

The method of claim 102 wherein the binder material is an ethylene polymer selected from the group consisting of polyethylene or an ethylene-vinyl acetate copolymer.

### Claim 104 (depends on 95)

The method of claim 95 wherein the primary particles are stainless steel.

### Claim 105 (depends on 100)

The method of claim 100 wherein the primary particles are stainless steel.

### Claim 106 (depends on 101)

The method of claim 101 wherein the primary particles are stainless steel.

### Claim 107

A method of forming a composite material which comprises:
providing a quantity of first particles of a binder material, said first particles having diameters between about 0.1 and about 150 micrometers;
providing a quantity of second particles of a primary material having a softening temperature substantially greater than the softening temperature of said binder material, said second particles having diameters between about: 0 1 and about 3,000 micrometers;
combining the first and second quantities of particles in a substantially uniform mixture wherein said binder material is present in an amount of at least about 3% by weight of the mixture;
heating said substantially uniform mixture, in the absence of pressure or shear sufficient to convert the binder particles into a continuous phase through the composite material, to a temperature substantially above the softening temperature of said binder material but to a temperature less than the softening temperature of said primary material;
thereafter applying pressure and shear to the heated mixture sufficient substantially immediately to convert at least a portion of the binder material particles into a substantially continuous webbing structure through the composite material;
substantially immediately after formation of said continuous binder structure, rapidly cooling said mixture to below the softening point of the binder material to retain said converted binder material in its continuous webbing structure condition to produce the composite material; and
thereafter applying stress to said composite material to convert at least a portion of the binding material from a continuous webbing structure to fibers.

### Claim 108 (depends on 107)

The method of claim 107 wherein said binder material is present in the mixture in an amount of about 3 to about 30% by weight of the total composition.

### Claim 109 (depends on 108)

The method of claim 108 wherein said binder material is present in an amount of about 4 to about 8% by weight.

### Claim 110 (depends on 108)

The method of claim 108 wherein said substantially uniform mixture is heated to a temperature at least about 25.degree. C. above the softening temperature of said binder material.

### Claim 111 (depends on 110)

The method of claim 110 wherein said substantially uniform mixture is heated to at least about 50.degree. C. above the softening temperature of the binder material.

### Claim 112 (depends on 107)

The method of claim 107 wherein the pressure applied to the heated mixture is at least about 500 psi (35 kg/cm.sup.2).

### Claim 113 (depends on 112)

The method of claim 112 wherein said pressure is at least about 4,000 psi (283 kg/cm.sup.2).

### Claim 114 (depends on 108)

The method of claim 108 wherein said substantially uniform mixture is heated to a temperature at least about 25.degree. C. above the softening temperature of said binder material.

### Claim 115 (depends on 114)

The method of claim 114 wherein said pressure is at least about 4000 psi (283 kg/cm.sup.2).

### Claim 116 (depends on 109, 113, 114, 115)

The method of claims 109, 113, 114 or 115 wherein the substantially uniform mixture is heated to a temperature at least about 50.degree. C. above the softening temperature of the binder material.

### Claim 117 (depends on 107, 109, 111, 113, 115)

The method of claims 107, 109, 111, 113 or 115 wherein said binder material is a crystalline polymer.

### Claim 118 (depends on 102, 104, 106)

The method of claims 102, 104, 106 108 or 115 wherein said binder material is a crystalline thermoplastic polymer.