Procedure for treatment of fir-wood and leaf-wood
AssigneesRobert Boho, Jozsef Vekony
InventorsRobert Boho, Istvan Pozsar, Jozsef Vekony
Life of this patent
Estimating the term…
Loading patent…
AssigneesRobert Boho, Jozsef Vekony
InventorsRobert Boho, Istvan Pozsar, Jozsef Vekony
Estimating the term…
This invention is concerned with methods for treating wet fir-woods or leaf-woods mainly for reduction of their moisture content and for preservation. The procedure of the invention is conducted in two steps. In the first step, the wet wood is kept in a bath of molten paraffin or a mixture of paraffin with paraffin oil at weight ratios from 90:10 to 10:90 containing 0.05 to 5 percent by weight of colloidal silicon dioxide at 80.degree. to 180.degree. C. for 10 to 50 minutes. In the second step, the wood is transferred into another bath of an emulsion consisting of 10 to 30 parts by weight of an aqueous urea/formaldehyde resin with solid content of 30 to 50 percent by weight in term of the solid content of the resin, 0.1 to 0.8 percent by weight of catalyst, 90 to 70 parts by weight of paraffin or a mixture of paraffin with paraffin oil at weight ratios from 90:10 to 10:90, and optionally 1 to 8 parts by weight of additives, preferably emulsifier, pigment, fungicide, and insecticide. The treatment is performed at 60.degree. to 100.degree. C. for 20 to 150 minutes. After the wood has been removed and the excess of liquid has drained off, the wood is kept at room temperature for 24 to 48 hours.
Procedure for treatment of wet fir-wood or leaf-wood in a bath containing paraffin or paraffin and paraffin oil at elevated temperature wherein, as a first step, the wet woods or woodwares are kept in a bath containing paraffin or a mixture of paraffin with paraffin oil at weight ratios from 90:10 to 10:90 and 0.05 to 5 percent by weight of colloidal silicon dioxide at 80.degree. to 180.degree. C. for 10 to 50 minutes then the wood is removed and, as a second step, immersed into another bath of an emulsion containing 10 to 30 parts by weight of an aqueous urea/formaldehyde resin with a solid content of 30 to 50 percent by weight, a catalyst at 0.1 to 0.8 percent by weight in term of the solid content of the resin, 90 to 70 parts by weight of paraffin or a mixture of paraffin with paraffin oil at weight ratios from 90:10 to 10:90, up to 8 wt % additive of an preferably emulsifier, pigment, fungicide, and insecticide, kept at 60.degree. to 100.degree. C. for 20 to 150 minutes, followed by the removal of the wood from the bath, draining the excess of liquid off and the treated wood is kept at room temperature for 24 to 48 hours.
Dependencies are inferred from the claim text.