# US 4,960,683 A · Method for processing a black-and-white photosensitive material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,960,683 A
- Document ID: US4960683A
- Status: Granted
- Kind: A
- Application number: 07/212,995
- Filed: 1988-06-29
- Granted: 1990-10-02
- Earliest claimed: 1987-06-29
- Assignees: Fuji Photo Film Co., Ltd.
- Inventors: Masaki Okazaki; Akihiko Ikegawa; Minoeu Yamada; Kunio Steo
- Web page: https://patentgrep.com/patent/US4960683A

## CPC

- G03C 5/38: Fixing; Developing-fixing; Hardening-fixing (bleach-fixing G03C5/44)
- G03C 5/268: {Processing baths not provided for elsewhere, e.g. pre-treatment, stop, intermediate or rinse baths (colour processing G03C7/3046)}
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)

## Abstract

A method for processing a black-and-white photosensitive material comprising the steps of: (a) exposing a silver halide photosensitive material having been spectrally sensitized with a sensitizing dye; (b) developing the exposed material; (c) fixing the developed material; and (d) thereafter at least one step selected from washing the material and stabilizing the material; at least one of the fixing, washing and stabilizing steps being performed in the presence of at least one compound represented by formula (I) or (II) or a salt thereof; ##STR1## wherein A represents an atomic group necessary for forming a saturated or unsaturated 3-membered to 8-membered ring comprising at least one hetero atom selected from an oxygen atom, a nitrogen atom, a sulfur atom and a selenium atom; and M represents a hydrogen atom or a counter cation; and X--(R.sub.1 --S).sub.n --R.sub.2 --S--R.sub.3 --Y (II) wherein R.sub.1, R.sub.2 and R.sub.3, which may be the same or different, each represents an alkylene group; R.sub.1 and R.sub.3 may be linked to form a ring, R.sub.2 and R.sub.3 may be linked to form a ring; X and Y, which may be the same or different, each represents a hydrogen atom, an alkyl group, an amino group, an ammonio group, a hydroxyl group, a carboxyl group, a sulfo group, an aminocarbonyl group or an aminosulfonyl group, and X and Y may be linked to form a ring; and n is an integer of from 0 to 10.

## Claims

### Claim 1

A method for processing a black-and-white photosensitive material comprising the steps of:
(a) exposing a silver halide photosensitive material having been spectrally sensitized with a sensitizing dye;
(b) developing said exposed material;
(c) fixing said developed material; and
(d) thereafter at least one step selected from the group consisting of washing said material and stabilizing said material;
said fixing step being performed in the presence of at least one compound represented by formula (I) or (II) or a salt thereof: ##STR10## wherein A represents an atomic group necessary for forming a saturated or unsaturated 3-membered to 8-membered ring comprising at least one hetero atom selected from the group consisting of an oxygen atom, a nitrogen atom, a sulfur atom and a selenium atom; and M represents a hydrogen atom or a counter cation; and
X--(R.sub.1 --S).sub.n --R.sub.2 --S--R.sub.3 --Y (II)
wherein R.sub.1, R.sub.2 and R.sub.3, which may be the same or different, each represents an alkylene group; R.sub.1 and R.sub.3 may be linked to form a ring, R.sub.2 and R.sub.3 may be linked to form a ring; X and Y, which may be the same or different, each represents a hydrogen atom, an alkyl group, an amino group, an ammonio group, a hydroxyl group, a carboxyl group, a sulfo group, an aminocarbonyl group or an aminosulfonyl group, and X and Y may be linked to form a ring; and n is an integer of from 0 to 10.

### Claim 2 (depends on 1)

A method as claimed in claim 1, wherein said compound is represented by formula (I).

### Claim 3 (depends on 2)

A method as claimed in claim 2, wherein --SM is linked to a carbon atom contained in the ring formed by A.

### Claim 4 (depends on 2)

A method as claimed in claim 2, wherein said ring formed by A is a nitrogen-containing ring.

### Claim 5 (depends on 2)

A method as claimed in claim 2, wherein said ring formed by A is substituted with at least one substituent selected from the group consisting of a hydroxyl group, an alkoxy group, an amino group, an ammonio group, an alkyl group, a mercapto group, an alkylthio group, a carbamoyl group, a sulfamoyl group, and one of these groups further substituted with a hydroxyl group, an alkoxy group, an amino group, an ammonio group, an alkyl group, a mercapto group, an alkylthio group, a carbomoyl group or a sulfamoyl group.

### Claim 6 (depends on 5)

A method as claimed in claim 5, wherein said substituent is selected from the group consisting of an alkoxy group, an amino group, an ammonio group, an alkyl group, a mercapto group, an alkylthio group, an alkyl group substituted with an amino group, an alkyl group substituted with an ammonio group, an alkylthio group substituted with an amino group and an alkylthio group substituted with an ammonio group.

### Claim 7 (depends on 2)

A method as claimed in claim 2, wherein M represents a hydrogen atom, an alkali metal atom or an organic base.

### Claim 8 (depends on 2)

A method as claimed in claim 2, wherein the total number of carbon atoms contained in said compound represented by formula (I) is 30 or less.

### Claim 9 (depends on 8)

A method as claimed in claim 8, wherein the total number of carbon atoms contained in said compound represented by formula (I) is 20 or less.

### Claim 10 (depends on 1)

A method as claimed in claim 1, wherein said compound is represented by formula (II).

### Claim 11 (depends on 10)

A method as claimed in claim 10, wherein said alkylene group represented by R.sub.1, R.sub.2 or R.sub.3 comprises an ether group.

### Claim 12 (depends on 10)

A method as claimed in claim 10, wherein said alkylene group represented by R.sub.1, R.sub.2 or R.sub.3 contains from 1 to 10 carbon atoms; and X and Y each represents a hydrogen atom or a group containing from 1 to 10 carbon atoms.

### Claim 13 (depends on 12)

A method as claimed in claim 12, wherein said alkylene group represented by R.sub.1, R.sub.2 or R.sub.3 contains from 1 to 6 carbon atoms; and n is an integer of from 1 to 4.

### Claim 14 (depends on 10)

A method as claimed in claim 10, wherein X and Y each represents a hydrogen atom, an amino group or an ammonio group.

### Claim 15 (depends on 10)

A method as claimed in claim 10, wherein said compound represented by formula (II) is a salt of said compound and an inorganic or organic acid.

### Claim 16 (depends on 1)

A method as claimed in claim 1, wherein said method comprises a further step of drying said material after said step (d).

### Claim 17 (depends on 16)

A method as claimed in claim 16, wherein said processing from the beginning of said developing step to the end of said drying step is completed in at most 90 seconds.

### Claim 18 (depends on 17)

A method as claimed in claim 17, wherein said processing from the beginning of said developing step to the end of said drying step is completed in at most 70 seconds.

### Claim 19 (depends on 1)

A method as claimed in claim 1, wherein said compound represented by formula (I) or (II) is present in an amount of from about 5.times.10.sup.-5 to 1.times.10.sup.-1 mol per liter of solution used in said fixing step.

### Claim 20 (depends on 19)

A method as claimed in claim 19, wherein said compound represented by formula (I) or (II) is present in an amount of from about 1.times.10.sup.-4 to 5.times.10.sup.-2 mol per liter of said solution.

### Claim 21 (depends on 20)

A method as claimed in claim 20, wherein said compound represented by formula (I) or (II) is present in an amount of from about 1.times.10.sup.-3 to 5.times.10.sup.-2 mol per liter of said solution.

### Claim 22 (depends on 19)

A method as claimed in claim 19, wherein said method comprises a further step of replenishing said washing solution or said stabilizing solution in an amount up to about 2 liter per m.sup.2 of said photosensitive material processed.

### Claim 23 (depends on 17)

A method as claimed in claim 17, wherein said developing step is conducted at a temperature of from about 25.degree. to 50.degree. C. for a time up to about 20 seconds; said fixing step is conducted at a temperature of from about 20.degree. to 50.degree. C. for a time of from about 6 to 20 seconds; said at least one of the washing and stabilizing steps is conducted at a temperature of from 0.degree. to 50.degree. C. for a time of from about 6 to 20 seconds; and said drying step is conducted at a temperature of from about 40.degree. to 100.degree. C. for a time of from about 5 to 30 seconds.

### Claim 24 (depends on 23)

A method as claimed in claim 23, wherein said developing step is conducted at a temperature of from about 30.degree. to 40.degree. C. for a time up to about 15 seconds; said fixing step is conducted at a temperature of from about 30.degree. to 40.degree. C. for a time of from about 6 to 15 seconds; said at least one of the washing and stabilizing steps is conducted at a temperature of from 15.degree. to 40.degree. C. for a time of from about 6 to 15 seconds; and said drying step is conducted at a temperature of from about 40.degree. to 80.degree. C. for a time of from about 5 to 20 seconds.