Flocculating agent combinations for mineral slime filtration systems
AssigneeEnvirotech Corporation
InventorTimothy J. Laros
Life of this patent
Estimating the term…
Abstract
An improved method for dewatering thin slurries of very fine clay or clay-like material to yield high solids content filter cake, for example, 40% solids and greater, by the use of flocculating agent combinations involving polyethylene oxide-type flocculating agents and polyacarylamide-type flocculating agents. The method generally involves admixing the combination of flocculating agents with the slurry, dewatering the slurry by means of a mechanical dewatering apparatus and feeding the thickened slurry to a belt press filter.
Claims8
In a method of dewatering phosphate slimes containing about 3% to 8% by weight solids on a belt press filter, the improvement comprising adding to said slime prior to its introduction to said belt press filter a combination of flocculating agents comprising a high molecular weight anionic polyacrylamide and a high molecular weight nonionic polyethylene oxide flocculating agent having a molecular weight of about five million to about eight million, said polyethylene oxide flocculating agent added to be present at a concentration of about 0.001% to about 0.1% by weight and said polyacrylamide added to be present as about 0.02% to about 0.01% by weight based upon the weight of said slime, wherein the weight ratio of polyacrylamide to polyethylene oxide is about 2:1 to about 25:1, and no more than a total of about 1.2 pounds of flocculating agent per ton of slime is added, and passing said slime through a mechanical dewatering apparatus to remove free water.
In a method of dewatering a clay-containing slime having a solids concentration of less than about 6% by weight by passing same first through a mechanical dewatering apparatus to remove free water and then through a belt press filter, the improvement comprising adding to said slime before it enters said mechanical dewatering apparatus a combination of flocculating agents comprising about 0.002% to about 0.008% by weight of a high molecular weight nonionic polyethylene oxide flocculating agent having a molecular weight of about five million to about eight million, and about 0.03% to about 0.08% by weight of a high molecular weight anionic polyacrylamide flocculating agent, wherein the weight ratio of polyacrylamide to polyethylene oxide is about 2:1 to about 25:1 and no more than a total of about 1.2 pounds of flocculating agent per ton of slime is added.
A method for dewatering thin slurries of very fine clay or clay-like particles having a solids content of less than about 10% by weight to yield filter cakes having approximately 40% by weight solids content comprising:
- adding a mixture of flocculating agents to said slurries of very fine clays, said mixture consisting essentially of about 0.02% to about 0.1% by weight of high molecular weight anionic polyacrylamide flocculating agent and about 0.002% to about 0.008% by weight of a polyethylene oxide flocculating agent having a molecular weight of about five million to eight million, said weight percent being based upon the weight of slurry being treated, wherein the weight ratio of polyacrylamide to polyethylene oxide is about 2:1 to about 25:1 and no more than a total of about 1.2 pounds of flocculating agent per ton of slime is added, to form a flocculated slurry;
- passing said flocculated slurry over a mechanical dewatering apparatus to remove free water and form a thickened slurry;
- dewatering said thickened slurry by passing it through a dual belt press filter having felt surfaced filter belts;
- and
- collecting filter cake having a solids content of greater than about 40% by weight.
Dependencies are inferred from the claim text.