# US 4,923,573 A · Method for the electro-deposition of a zinc-nickel alloy coating on a steel band

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,923,573 A
- Document ID: US4923573A
- Status: Granted
- Kind: A
- Application number: 07/343,528
- Filed: 1989-04-26
- Granted: 1990-05-08
- Earliest claimed: 1988-05-13
- Assignees: Rasselstein AG
- Inventors: Theodor Florian
- Web page: https://patentgrep.com/patent/US4923573A

## CPC

- C25D 3/565: {containing more than 50% by weight of zinc}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

In the method for the electro-deposition of a zinc-nickel alloy coating on a steel band, electrolytic nickel anodes and an electrolyte as free from chloride as possible and containing Zn.sup.2+ and Ni.sup.2+ ions is used. Operation is at current densities of at least 10 A/dm.sup.2, the metal content removed being replaced constantly during operation.

## Claims

### Claim 1

A method for the electro-deposition of a zinc-nickel alloy coating on a steel band in an electrolyte containing Zn.sup.2+ and Ni.sup.2+ ions at a current density of at least 10 A/dm.sup.2 comprising the steps of:
(1) adjusting the chloride content of the electrolyte to less than 300 mg/l;
(2) passing the steel band through a plating tank containing said electrolyte and at least one metal anode consisting of electrolytic nickel having a nickel content of at least 99.5%;
(3) depositing a zinc-nickel alloy coating on said steel band from said electrolyte in said plating tank thereby depleting the content of Zn.sup.2+ and Ni.sup.2+ ions in said electrolyte;
(4) providing a regeneration tank in fluid communication with said plating tank, said regeneration tank containing at least one zinc anode and one nickel anode;
(5) removing said depleted electrolyte from said plating tank and introducing it into said regeneration tank;
(6) replenishing said depleted electrolyte in said regeneration tank by galvanic dissolution of said at least one zinc anode and one nickel anode; and
(7) reintroducing said replenished electrolyte into said plating tank.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the chloride content of the electrolyte is adjusted to below 50 mg/l.

### Claim 3 (depends on 1)

According to claim 1, wherein the electrolyte contains zinc sulfate, nickel sulfate and a conducting salt.

### Claim 4 (depends on 3)

A method according to claim 3, wherein the pH of the electrolyte is adjusted to approximately 1.5.

### Claim 5 (depends on 1)

A method according to claim 1, wherein said at least one nickel anode in the regeneration tank is activated with sulfur.

### Claim 6 (depends on 5)

A method according to claim 5, wherein said at least one nickel anode contains approximately 0.03% sulfur.

### Claim 7 (depends on 1)

A method according to claim 1, wherein said galvanic dissolution in said regeneration chamber is carried out at current densities of up to 8 A/dm.sup.2.

### Claim 8 (depends on 1)

A method according to claim 1, wherein said replenished electrolyte filtered prior to being reintroduced into said plating tank.

### Claim 9 (depends on 1)

A method according to claim 1, wherein only one plating tank is used.

### Claim 10 (depends on 1)

A method according to claim 1, wherein said at least one nickel anode in said regeneration chamber has a greater solubility in said electrolyte than said at least one metal anode consisting of electrolytic nickel.

### Claim 11 (depends on 1)

A method according to claim 1, wherein said at least one metal anode consisting of electrolytic nickel forms a protective layer in said electrolyte.

### Claim 12

A method for the electro-deposition of a zinc-nickel alloy coating on a steel band in an electrolyte containing Zn.sup.2+ and Ni.sup.2+ ions at a current density of at least 10 A/dm.sup.2 comprising the steps of:
(1) adjusting the chloride content and the pH of the electrolyte to less than 50 mg/l and approximately 1.5 respectively;
(2) passing the steel band through a plating tank containing said electrolyte and at least one metal anode consisting of electrolyte nickel having a nickel content of at least 99.5%, said at least one metal anode forming a protective layer in said electrolyte;
(3) depositing a zinc-nickel alloy coating on said steel band from said electrolyte in said plating tank thereby depleting the content of Zn.sup.2+ and Ni.sup.2+ ions in said electrolyte;
(4) providing a regeneration tank in fluid communication with said plating tank, said regeneration tank containing at least one zinc anode and one nickel anode, said at least one nickel anode in said regeneration tank containing approximately 0.03% sulfur and having a higher solubility in said electrolyte than said at least one metal anode consisting of electrolytic nickel;
(5) removing said depleted electrolyte from said plating tank and introducing it into said regeneration tank;
(6) replenishing said depleted electrolyte in said regeneration tank by galvanic dissolution of said at least one zinc anode and one nickel anode, said galvanic dissolution being carried out at current densities of up to 8 A/dm.sup.2 ;
(7) removing said replenished electrolyte from said regeneration tank and passing it through a filter; and
(8) reintroducing said filtered replenished electrolyte into said plating tank.