# US 4,904,554 A · Gas phase hardening of gelatin holograms

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,904,554 A
- Document ID: US4904554A
- Status: Granted
- Kind: A
- Application number: 07/170,951
- Filed: 1988-03-21
- Granted: 1990-02-27
- Earliest claimed: 1988-03-21
- Assignees: Hughes Aircraft Company
- Inventors: John E. Wreede
- Web page: https://patentgrep.com/patent/US4904554A

## CPC

- G03C 5/22: Direct chromate processes, i.e. without preceding silver picture, or agents therefor
- G03H 1/182: {Post-exposure processing, e.g. latensification}
- G03H 2001/185: {Applying a curing step}
- G03H 2260/10: Dichromated gelatine or equivalents
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)
- G03H: HOLOGRAPHIC PROCESSES OR APPARATUS (holograms, e.g. point holograms, used as ordinary optical elements G02B5/32; producing stereoscopic or other three-dimensional effects G02B30/00; diffraction-grating systems G02B27/44; systems using moiré fringes G02B27/60; optical logic elements G02F3/00; stereo-photography G03B35/00; photosensitive materials or processes for photographic purposes G03C; {stereo-photographic or similar processes G03C9/00}; apparatus for processing exposed photographic materials G03D; analogue computers performing mathematical operations with the aid of optical elements G06E3/00; authentication by radiation, of concealed information carried by holograms or diffraction gratings G06K19/16; holographic storage G11B7/0065, G11C13/04; {stereoscopic or other three dimensional effects in television systems H04N13/00})

## Abstract

A process for hardening gelatin holograms after dehydration involving subjecting the hologram to an atmosphere containing aldehyde vapor and water vapor. The process provides hardening of the gelatin hologram to increase resistance to moisture and heat without adversely affecting diffraction efficiency. Monitoring of the diffraction efficiency during the aldehyde-water vapor treatment allows fine tuning of the hologram efficiency and evenness.

## Claims

### Claim 1

A process for hardening gelatin holograms after dehydration and removing the dehydration agent comprising the step of treating a dehydrated hologram with a sufficient amount of aldehyde vapor along with and in the presence of a sufficient amount of water
vapor and for a sufficient time to harden said dehydrated hologram.

### Claim 2 (depends on 1)

A process for hardening gelatin holograms according to claim 1 wherein said aldehyde vapor comprises an aldehyde selected from the group consisting of formaldehyde, acetaldehyde, propionaldehyde and butyraldehyde.

### Claim 3 (depends on 2)

A process for hardening gelatin holograms according to claim 2 wherein said aldehyde is formaldehyde.

### Claim 4

A process for hardening gelatin holograms according to claim wherein the concentration of aldehyde vapor in the atmosphere surrounding said dehydrated hologram is between about 5 to 20 volume percent.

### Claim 5 (depends on 4)

A process for hardening gelatin holograms according to claim 4 wherein the concentration of said aldehyde vapor in the atmosphere surrounding said dehydrated hologram is about 8 volume perecent.

### Claim 6 (depends on 1)

A process for hardening gelatin holograms according to claim 1 wherein the amount of water vapor in the atmosphere surrounding said dehydrated hologram provides said atmosphere with a relative humidity of between about 10 to 30.

### Claim 7 (depends on 6)

A process for hardening gelatin holograms according to claim 6 wherein the relative humidity of the atmosphere surrounding said dehydrated hologram is about 20.

### Claim 8 (depends on 1)

A process for hardening gelatin holograms according to claim 1 wherein the transmission characteristics of said dehydrated hologram are measured during said hardening process in order to monitor the extent of hardening.

### Claim 9

In a process for making a gelatin hologram which includes the steps of dehydrating the gelatin hologram in alcohol after development of the gelatin hologram and then removing the alcohol from the gelatin to provide an alcohol evaporated gelatin hologram, wherein the improvement comprises treating said alcohol-evaporated gelatin with a sufficient amount of aldehyde vapor along with and in the presence of a sufficient amount of water vapor and for a sufficient time to harden said alcohol evaporated gelatin hologram.

### Claim 10 (depends on 9)

The improved process according to claim 9 wherein said aldehyde vapor comprises an aldehyde selected from the group consisting of formaldehyde, acetaldehyde, propionaldehyde and butyraldehyde.

### Claim 11 (depends on 10)

The improved process according to claim 10 wherein said aldehyde is formaldehyde.

### Claim 12 (depends on 8)

The improved process according to claim 8 wherein the concentration of aldehyde vapor in the atmosphere surrounding said dehydrated gelatin hologram is between about 5 to 20 volume percent.

### Claim 13 (depends on 12)

The improved process according to claim 12 wherein the concentration of aldehyde vapor in the atmosphere surrounding said dehydrated gelatin hologram is about 8 volume percent.

### Claim 14 (depends on 9)

The improved process according to claim 9 wherein the amount of water vapor in the atmosphere surrounding said alcohol-evaporated gelatin hologram provides said atmosphere with a relative humidity of between about 10 to 30.

### Claim 15 (depends on 14)

The improved process according to claim 14 wherein the relative humidity of the atmosphere surround said alcohol-evaporated gelatin hologram is about 20.

### Claim 16 (depends on 9)

The improved process according to claim 9 including the additional step of measuring the transmission characteristics of said alcohol-evaporated gelatin hologram during treatment with said aldehyde vapor to monitor the extent of hardening.

### Claim 17 (depends on 1)

A process for hardening gelatin holograms according to claim 1 wherein said gelatin hologram is a dichromated gelatin hologram.

### Claim 18 (depends on 9)

The improved process for hardening gelatin holograms according to claim 9 wherein said gelatin hologram is a dichromated gelatin hologram.