# US 4,882,373 A · Asphaltic composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,882,373 A
- Document ID: US4882373A
- Status: Granted
- Kind: A
- Application number: 07/232,210
- Filed: 1988-08-15
- Granted: 1989-11-21
- Earliest claimed: 1987-07-24
- Assignees: Exxon Research & Engineering Co.
- Inventors: Lyle E. Moran
- Web page: https://patentgrep.com/patent/US4882373A

## CPC

- C10C 3/026: {with organic compounds}
- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- C10C: WORKING-UP PITCH, ASPHALT, BITUMEN, TAR; PYROLIGNEOUS ACID (compositions of bituminous materials C08L95/00; carbon filaments by decomposition of organic filaments D01F9/14)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

An asphaltic composition having improved tensile properties is disclosed. Also disclosed is a method for producing said composition which comprises: A. contacting an asphalt with a mineral acid; B. contacting the acid modified asphalt thus formed with an oxygen-containing gas; C. adding a thermoplastic elastomer to the acid/oxygen modified asphalt thus formed; and D. adding an unsaturated functional monomer to the polymer modified asphalt. In a preferred embodiment, the asphalt is contacted with an oxygen-containing gas prior to and during contact with the mineral acid.

## Claims

### Claim 1

An asphaltic composition having improved tensile properties that is produced by the method comprising:
(a) contacting asphalt with from about 0.25 to about 4 wt. % of a mineral acid to form an acid modified asphalt,
(b) contacting said acid modified asphalt with an oxygen-containing gas to form an acid/oxygen modified asphalt, the temperature of the asphalt during said contacting in (a) and (b) being maintained between about 200.degree. C. and about 300.degree. C.,
(c) contacting said acid/oxygen modified asphalt with from about 5 to about 25 wt. % of a thermoplastic elastomer at a temperature between about 160.degree. C. to form a polymer modified asphalt, and
(d) contacting said polymer modified asphalt with from about 0.3 to about 15 wt. % of an unsaturated functional monomer selected from the group consisting of an unsaturated carboxylic acid, an unsaturated dicarboxylic acid, an unsaturated anhydride, an unsaturated ester, an unsaturated imide and mixtures thereof at a temperature above about 120.degree. C. but not more than about 200.degree. C.

### Claim 2 (depends on 1)

The composition of claim 1 wherein the mineral acid is selected from the group consisting of phosphoric acid, sulfuric acid, and mixtures thereof.

### Claim 3 (depends on 2)

The composition of claim 2 wherein the mineral acid comprises phosphoric acid.

### Claim 4 (depends on 1)

The composition of claim 1 wherein the asphalt is contacted with an oxygen-containing gas prior to contact with said mineral acid.

### Claim 5 (depends on 4)

The composition of claim 4 wherein said oxygen-containing gas is air.

### Claim 6 (depends on 2)

The composition of claim 2 wherein the thermoplastic elastomer is based on styrenics, olefins, urethanes, copolyesters, or mixtures, thereof.

### Claim 7 (depends on 3)

The composition of claim 3 wherein the thermoplastic elastoner comprises styrene-butadiene-styrene, the unsaturated functional monomer is selected from the group consisting of maleic acid, maleic anyhydride and mixtures thereof, and the oxygen-containing gas is air.

### Claim 8 (depends on 6)

The composition of claim 6 wherein the thermoplastic elastomer is based on styrenics.

### Claim 9 (depends on 8)

The composition of claim 8 wherein the thermoplastic elastomer comprises styrene-butadiene-styrene.

### Claim 10 (depends on 6)

The composition of claim 6 wherein the unsaturated functional monomer comprises an unsaturated carboxylic acid selected from the group consisting of acrylic acid, crotonic acid, methacrylic acid, and mixtures thereof.

### Claim 11 (depends on 6)

The composition of claim 6 wherein the unsaturated functional monomer comprises an unsaturated dicarboxylic acid selected from the group consisting of maleic acid, fumaric acid, cis-4-cyclohexene-1,2-dicarboxylic acid, endo-cis-bicyclo (2,2,1) 5 heptane-2,3 dicarboxylic acid, itaconic acid, and mixtures thereof.

### Claim 12 (depends on 6)

The composition of claim 6 wherein the unsaturated functional monomer comprises an unsaturated anhydride selected from the group consisting of maleic anhydride, citraconic anhydride, 2,3 dimethylmaleic anhydride, endo bicyclo (2,2,2) oct-5-ene-2,3 dicarboxylic anhydride and mixtures thereof.

### Claim 13 (depends on 6)

The composition of claim 6 wherein the unsaturated functional monomer comprises an unsaturated imide selected from the group consisting of maleimide, methyl maleimide, ethylmaleimide, phenylmaleimide and mixtures thereof.

### Claim 14 (depends on 6)

The composition of claim 6 wherein said unsaturated functional monomer is selected from the group consisting of maleic acid, maleic anhydride and mixtures thereof.

### Claim 15 (depends on 14)

The composition of claim 14 wherein from about 1.25 to about 2.5 wt. % of said mineral acid is present therein.

### Claim 16 (depends on 15)

The composition of claim 15 wherein from about 5 to about 15 wt. % of said thermoplastic elastomer is present therein.

### Claim 17 (depends on 16)

The composition of claim 16 wherein from about 0.3 to about 5 wt. % of said unsaturated functional monomer is present therein.

### Claim 18

A method for producing an asphaltic composition having improved tensile properties which comprises:
(a) contacting asphalt with from about 0.25 to about 4 wt. % of a mineral acid to form an acid modified asphalt,
(b) contacting said acid modified asphalt with an oxyqen-containing gas to form an acid/oxygen modified asphalt, the temperature of the asphalt during said contacting in (a) and (b) being maintained between about 200.degree. and about 300.degree. C.,
(c) contacting said acid/oxygen modified asphalt with from about 5 to about 25 wt. % of a thermoplastic elastomer at a temperature between about 160.degree. and about 220.degree. C. to form a polymer modified asphalt, and
(d) contacting said polymer modified asphalt with from about 0.3 to about 15 wt. % of an unsaturated functional monomer selected from the group consisting of an unsaturated carboxylic acid, an unsaturated dicarboxylic acid, an unsaturated anhydride, an unsaturated ester, an unsaturated imide and mixtures thereof at a temperature above about 120.degree. C. but no more than about 200.degree. C.

### Claim 19 (depends on 18)

The method of claim 18 wherein the asphalt is contacted with an oxygen-containing gas prior to contact with said mineral acid.

### Claim 20 (depends on 19)

The method of claim 19 wherein said oxygen-containing gas is air.

### Claim 21 (depends on 18)

The method of claim 18 wherein said mineral acid is selected from the group consisting of phosphoric acid, sulfuric acid and mixtures thereof.

### Claim 22 (depends on 21)

The method of claim 21 wherein said mineral acid comprises phosphoric acid.

### Claim 23 (depends on 21)

The method of claim 21 wherein the thermoplastic elastomer is based on styrenics, olefinics, urethanes, copolyesters, or mixtures thereof.

### Claim 24 (depends on 23)

The method of claim 23 wherein the thermoplastic elastomer is based on styrenics.

### Claim 25 (depends on 24)

The method of claim 24 wherein the thermoplastic elastomer comprises styrene-butadiene-styrene.

### Claim 26 (depends on 23)

The method of claim 23 wherein the unsaturated functional monomer comprises an unsaturated carboxylic acid selected from the group consisting of acrylic acid, crotonic acid, methacrylic acid, and mixtures thereof.

### Claim 27 (depends on 23)

The method of claim 23 wherein the unsaturated functional monomer comprises an unsaturated dicarboxylic acid selected from the group consisting of maleic acid, fumaric acid, cis-4-cyclohexene-1,2-dicarboxylic acid, endo-cis-bicyclo (2,2,1) 5 heptane2,3 dicarboxylic acid, itaconic acid, and mixtures thereof.

### Claim 28 (depends on 23)

The method of claim 23 wherein the unsaturated functional monomer comprises an unsaturated anhydride selected from the group consisting of maleic anhydride, citraconic anhydride, 2,3 dimethylmaleic anhydride, endo bicyclo (2,2,2) oct-5-ene-2,3 dicarboxylic anhydride and mixtures thereof.

### Claim 29 (depends on 23)

The method of claim 23 wherein the unsaturated functional monomer comprises an unsaturated imide selected from the group consisting of maleimide, methyl maleimide, ethylmaleimide, phenylmaleimide and mixtures thereof.

### Claim 30 (depends on 23)

The method of claim 23 wherein said unsaturated functional monomer is selected from the group consisting of maleic acid, maleic anhydride and mixtures thereof.

### Claim 31 (depends on 18)

The method of claim 18 wherein the temperature in (c) is between about 180.degree. and about 210.degree. C.

### Claim 32 (depends on 31)

The method of claim 31 wherein the temperature in (d) is between 150.degree. and about 180.degree. C.

### Claim 33

A method for producing an asphaltic composition having improved tensile properties which comprises:
(a) passing air through an asphalt having an atmospheric boiling point of at least 380.degree. C., which is maintained at a temperature of about 200.degree. C. to about 280.degree. C. for a period of time ranging between about 0.5 to about 2 hours to form an air blown asphalt;
(b) subsequently adding between about 0.25 and about 4 wt. % phosphoric acid to the air blown asphalt and passing air through said air blown asphalt for an additional period of time ranging from about 1 to about 12 hours to form an acid/air modified asphalt;
(c) adding between about 5 to about 25 wt. % styrene-butadiene-styrene block copolymer to said acid/air modified asphalt at a temperature between about 160.degree. and about 220.degree. C. to form a polymer modified asphalt; and
(d) adding between about 0.3 and about 15 wt. % of an unsaturated functional monomer selected from the group consisting of maleic acid, maleic anhydride and mixtures thereof to said polymer modified asphalt at a temperature above about 120.degree. C. but no more than about 200.degree. C.

### Claim 34 (depends on 33)

The method of claim 33 wherein between about 5 to about 15 wt. % of said styrene-butadiene-styrene block copolymer is added to said acid/air modified asphalt in (c) and from about 0.3 to about 5 wt. % of said unsaturated functional monomer is added to said polymer modified asphalt in (d).

### Claim 35 (depends on 33)

The composition formed according to the method of claim 33.

### Claim 36 (depends on 34)

The composition formed according to the method of claim 34.