Process for the dyeing of polymers of propylene, butene-1 and 4-methyl-pentene-1 using basic dye in an aqueous dye bath
AssigneeDuPont Canada Inc.
InventorJohn R. B. Boocock
Life of this patent
Estimating the term…
Abstract
A process for the dyeing of polymers of propylene, butene-1 and 4-methyl-pentent-1 is disclosed. The process involves contacting articles of the polymer with an aqueous dyebath containing a basic dye in a concentration of at least 0.4 g/l and at a pH of at least 5.0. The temperature of the aqueous dyebath is at least 90.degree. C. The article is maintained in contact with the dyebath for at least 10 minutes. The polymer of propylene is preferably a blend of 50-99 parts of a homopolymer of propylene or copolymer of propylene and ethylene with 1-50 parts of a zinc ionomer or graft copolymer of a hydrocarbon alpha-olefin with an alpha-olefin having carboxylic acid or carboxylic acid anhydride. Dyed polymers are obtained.
Claims7
A process for dyeing a polyolefin article, comprising the steps of:
- (A) contacting the polyolefin article with an aqueous dyebath, said polyolefin being a blend comprising (i) 50-99 parts by weight of at least one polymer selected from the group consisting of homopolymers of propylene, butene-1 or 4-methyl-pentene-1 and copolymers of propylene, butene-1 or 4-methyl-pentene-1 with a minor amount of a hydrocarbon alpha-olefin, and mixtures thereof, and (ii) 1-50 parts by weight of a copolymer selected from the group consisting of direct copolymers or graft copolymers wherein (a) said direct copolymer is a zinc ionomer of a copolymer of an alpha-olefin having the formula R--CH.dbd.CH.sub.2, where R is a radical selected from the class consisting of hydrogen and alkyl radicals having from 1 to 8 carbon atoms, with at least one alpha-beta-ethylenically unsaturated carboxylic acid having from 3 to 8 carbon atoms, the acid moieties being randomly or non-randomly distributed in the polymer chain, the carboxylic acid content being 0.5-50% by weight of the direct copolymer, any other copolymerized monomer being monoethylenically unsaturated, and (b) said graft copolymer is obtained by grafting 0.1 to 20 percent by weight of at least one alpha,beta-unsaturated carboxylic acid having 3 to 8 carbon atoms or unsaturated carboxylic acid anhydride onto a preformed polyolefin backbone derived from at least one of homopolymers of C.sub.2 to C.sub.8 hydrocarbon alpha-olefins, copolymers of ethylene and at least one C.sub.3 to C.sub.8 hydrocarbon alpha-olefin and copolymers of ethylene and unsaturated carboxylic acids, in which polyolefin backbone any other optionally copolymerized monomer component is monoethylenically unsaturated, said aqueous dyebath containing basic dye in a concentration of at least 0.4 g/1 and at a pH of at least 5.0, the temperature of the aqueous dyebath being at least 90.degree. C.,
- (B) maintaining said polyolefin article in contact with the aqueous dyebath for a period of at least 10 minutes, and
- (C) removing the polyolefin article so dyed from the aqueous dyebath.
Dependencies are inferred from the claim text.