# US 4,855,021 A · Method for electroplating a steel strip with a coating metal, in particular zinc or a zinc-containing alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,855,021 A
- Document ID: US4855021A
- Status: Granted
- Kind: A
- Application number: 07/222,187
- Filed: 1988-07-21
- Granted: 1989-08-08
- Earliest claimed: 1987-08-15
- Assignees: Rasselstein AG
- Inventors: Horst Bersch; Karl-Heinz Kilian; Hans U. Weigel
- Web page: https://patentgrep.com/patent/US4855021A

## CPC

- C25D 5/028: {one side electroplating, e.g. substrate conveyed in a bath with inhibited background plating}
- C25F 5/00: Electrolytic stripping of metallic layers or coatings
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C25F: PROCESSES FOR THE ELECTROLYTIC REMOVAL OF MATERIALS FROM OBJECTS; APPARATUS THEREFOR

## Abstract

In a method for electroplating a steel strip with a coating metal, in particular, zinc or a zinc-containing alloy, a thin protective layer consisting of the coating metal is temporarily electrodeposited on one side of the steel strip. After complete coating of the other side, this protective layer is completely or essentially removed in a stripping step in which the coated steel strip as the anode is moved through a stripping electrolyte. The stripping electrolyte contains a sequestering agent, advantageously sodium gluconate.

## Claims

### Claim 1

In a method for electrodepositing a single-sided metal coating on a steel strip wherein a protective layer of the metal to be coated is first deposited on one side of the steel strip and, after the application of the metal coating to the other side of the steel strip, the steel strip is made anodic and contacted with a stripping electrolyte in order to remove said protective layer from said one side, the improvement comprising the protective layer being deposited in a thickness of 20-100 mg/m.sup.2 and at a current density of from 1-30 A/dm.sup.2 and the stripping of said protective layer being carried out in a stripping electrolyte having an organic sequestering agent and at a current density of 5-30 A/dm.sup.2.

### Claim 2 (depends on 1)

The method according to claim 1 characterised in that in the stripping electrolyte are used, as sequestering agents, aqueous solutions of alkali metal salts, of one or more of the following acids;
aldonic acids
diethylene triamine pentaacetic acid
ethylene diamine tetraacetic acid
hydroxycarboxylic acids
nitrilotriacetic acid
polycarboxylic acids.

### Claim 3 (depends on 2)

The method according to claim 2, characterised in that the sodium salt of a polycarboxylic acid is used as the sequestering agent in the stripping electroyte.

### Claim 4 (depends on 2)

The method according to claim 2, characterised in that the stripping electrolyte contains a sodium salt of dextronic acid as the sequestering agent.

### Claim 5 (depends on 2)

The method according to claim 2, characterised in that the stripping electrolyte contains a sodium salt of nitrilotriacetic acid as the sequestering agent.

### Claim 6 (depends on 1)

The method according to claim 1, characterised in that the stripping electrolyte contains a substance which increases its conductivity.

### Claim 7 (depends on 6)

The method according to claim 6, characterised in that sodium sulphate is used as said substance.

### Claim 8 (depends on 1)

The method according to claim 1, characterised in that the pH value in the stripping electrolyte is adjusted to from 8-10.

### Claim 9 (depends on 1)

The method according to claim 1, characterised in that the temperature of the stripping electrolyte is maintained at 30.degree.-70.degree. C.

### Claim 10 (depends on 1)

The method according to claim 1, characterised in that said stripping is carried out within 10 sec.

### Claim 11 (depends on 15)

The method according to claim 15, characterized in that the protective layer is removed from said one side to such an extent that a residual coating of said protective layer of up to 50 mg/m.sup.2 remains.

### Claim 12 (depends on 1)

Method according to claim 1, characterised in that electrodeposition of the protective layer is carried out in a layer thickness of 20-30 mg/m.sup.2.

### Claim 13 (depends on 1)

The method according to claim 1, characterized in that electrodeposition of the protective layer on said one side is carried out simultaneously with the commencement of the electrodeposition of a preliminary coating on said other side in the same coating electrolyte.

### Claim 14 (depends on 1)

The method according to claim 1, characterised in that before electrodeposition of the protective layer, short-term electroless wetting of the steel strip with the coating electrolyte is carried out.

### Claim 15 (depends on 1)

The method according to claim 1, characterized in that in the stripping electrolytes are used, as sequestering agents, aqueous solutions of sodium salts of one or more acids selected from the group consisting of aldonic acids, diethylene triamine pentaacetic acid, ethylene diamine tetraacetic acid, hydroxycarboxylic acids, nitrilotriacetic acid, and polycarboxylic acids.

### Claim 16 (depends on 1)

The method according to claim 1, characterized in that said protective layer is deposited in a thickness of about 20-30 mg/m.sup.2.

### Claim 17 (depends on 1)

The method according to claim 1, characterized in that said stripping electrolyte is maintained at a temperature of about 30.degree.-70.degree. C.

### Claim 18 (depends on 1)

The method according to claim 1, characterized in that said metal to be coated is selected from the group consisting of zinc and zinc alloys.

### Claim 19 (depends on 1)

The method according to claim 1, characterized in that said organic sequestering agent is sodium gluconate.