# US 4,819,458 A · Heat shrunk fabrics provided from ultra-high tenacity and modulus fibers and methods for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,819,458 A
- Document ID: US4819458A
- Status: Granted
- Kind: A
- Application number: 06/429,942
- Filed: 1982-09-30
- Granted: 1989-04-11
- Earliest claimed: 1982-09-30
- Assignees: Allied-Signal Inc.
- Inventors: Sheldon Kavesh; Dusan C. Prevorsek; Gary A. Harpell
- Web page: https://patentgrep.com/patent/US4819458A

## CPC

- D06C 7/02: Setting
- Y10S 428/902: High modulus filament or fiber
- D06C: FINISHING, DRESSING, TENTERING OR STRETCHING TEXTILE FABRICS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

Ultrahigh molecular weight polyethylene fibers of high tenacity and modulus shrink controlled amounts at temperatures in the range of 100.degree.-145.degree. C. Fabrics and twisted multifilament yarns of these fibers are heat-shrunk or heat-set at these temperatures.

## Claims

### Claim 1

A method for preparing fabrics which comprises the steps:
(a) forming a fabric from stretched fibers of tenacity at least about 20 g/denier and tensile modulus at least about 600 g/denier containing polyethylene of weight average molecular weight at least about 500,000, and
(b) heating the fabric at a temperature between about 120.degree. C. and about 145.degree. C. sufficient and for a time sufficient for the fibers to shrink between about 1% and about 10% of their length in the fabric formed in step a.

### Claim 2 (depends on 1)

The method of claim 1 wherein said polyethylene is of weight average molecular weight at least 1,000,000.

### Claim 3 (depends on 2)

The method of claim 2 wherein said fibers have a tenacity of at least about 30 g/denier and a tensile modulus at least about 1000 g/denier.

### Claim 4 (depends on 3)

The method of claim 3 wherein said fibers have a tensile modulus of at least about 1600 g/denier.

### Claim 5 (depends on 1)

The method of claim 1 wherein step (b) is performed at a temperature and for a period of time sufficient for the fibers to shrink between about 2% and about 5%.

### Claim 6 (depends on 1)

The method of claim 1 wherein said forming step (a) includes knitting.

### Claim 7 (depends on 1)

The method of claim 1 wherein said forming step (a) includes weaving.

### Claim 8 (depends on 1)

The method of claim 1 wherein said fibers are twisted multifilament yarns.

### Claim 9 (depends on 8)

The method of claim 8 wherein the twisted multifilament yarn is heat set at a temperature between 100.degree. C. and 130.degree. C. prior to forming the fabric, and the temperature of said heating step (b) is higher than the temperature at which the twisted multifilament yarn is heat set.

### Claim 10 (depends on 1)

A heat-shrunk fabric produced by the method of claim 1.