Method for producing torrefied wood, product obtained thereby, and application to the production of energy
OwnerJacques Leclerc de Bussyinventor
Life of this patent
Estimating the term…
Abstract
New product consisting of wood which is torrefied between 250.degree. and 280.degree. C. in a non oxidizing atmosphere, in the form of sticks of uniform length: 15 mm for example and having a diameter comprised between 5 and 20 mm, which are not disbarked. The preparation of the method comprised the obtention by culture of rectilinear ligneous rejections, the cutting, drying and torrefaction thereof preferably in a vertical reactor (101) where the material to be torrefied (115) is traversed by a gas stream circulating at high speed.
Claims18
A process for producing torrefied wood products which can be burned to produce thermal energy from plants which produce substantially straight, unbarked woody suckers having diameters of 5 to 20 mm, said process comprising the steps of
- (a) cutting said substantially straight, unbarked woody suckers having diameters of 5 to 20 mm from said plants,
- (b) sectioning said substantially straight, unbarked woody suckers so as to produce unbarked green sticks of a uniform length, said uniform length being between about 10 and 25 mm,
- (c) placing said unbarked green sticks provided in step (b) in a reactor so as to form a bed therein,
- (d) passing a hot, non-oxidizing gas having a temperature greater than 280.degree. C. through said bed so as to first dry and then torrify the unbarked green sticks therein, thus providing torrefied wood products, the velocity of said hot, non-oxidizing gas being sufficiently low to avoid conveying of torrefied wood products away from said bed yet sufficiently high to raise the temperature of the unbarked green sticks from 100.degree. C. to a torrification temperature of 250.degree. to 280.degree. C. in no more than 10 minutes, and
- (e) cooling said torrefied wood products.
Torrefied, unbarked wood products which are generally cylindrical in shape and which have diameters between 5 and 20 mm and uniform lengths of about 10 and 25 mm, said torrefied, unbarked wood products being made by the steps of
- (a) cutting substantially straight, unbarked woody suckers having diameters of 5 to 20 mm from plants,
- (b) sectioning said substantially straight, unbarked woody suckers so as to produce unbarked green sticks of a uniform length, said uniform length being between about 10 and 25 mm,
- (c) placing said unbarked green sticks provided in step (b) in a reactor so as to form a bed therein,
- (d) passing a hot, non-oxidizing gas having a temperature greater than 280.degree. C. through said bed so as to first dry and then torrify the unbarked green sticks therein, thus providing torrefied wood products, the velocity of said hot, non-oxidizing gas being sufficiently low to avoid conveying of torrefied wood products away from said bed yet sufficiently high to raise the temperature of the unbarked green sticks from 100.degree. C. to a torrification temperature of 250.degree. to 280.degree. C. in no more than 10 minutes, and
- (e) cooling said torrefied wood products.
Dependencies are inferred from the claim text.