Methods of making cementitious compositions from waste products
AssigneeO'Okiep Copper Company Limited
InventorsT. Peter Philip, Anthony L. Hannaford, Ernst Konick
Life of this patent
Estimating the term…
Abstract
Methods for producing cementitious compositions from waste products, such as non-ferrous slags, or fossil fuel combustion residue, or ferrous slags, whereby the CaO and alumina contents of the waste products are adjusted as necessary to enable them to combine with a sulphate additive at elevated pH and so couple the faster reactions of the mineral Ettringite with the slower ones of the calcium silicates.
Claims22
A method for making a cementitious composition which comprises:
- adding to a waste residue of a non-ferrous slag, a fossil fuel combustion residue or a mixture thereof during its formation in a furnace or burner a compound containing CaO and a compound containing Al.sub.2 O.sub.3 to form a first mixture having a sufficient CaO and Al.sub.2 O.sub.3 content to enable said first mixture to react with a composition comprising a sulfate anion, added therto during a subsequent treatment step, to form a composition having pozzolanic qualities attainable with ettringite;
- increasing the pH of the first mixture to a sufficiently alkaline value to activate the alumina component of said first mixture;
- and
- treating said first mixture by the additive thereto of a compound containing a sulphate anion so as to form a second mixture, the proportional relationship among the CaO, Al.sub.2 O.sub.3 and sulphate components in said second mixture being such that the ratio thereamong approaches the stoichiometric relation of the components of the mineral ettringite so as to obtain the pozzolanic qualities of ettrigite, thus forming a cementitious composition.
A method for making a cementitious composition which comprises:
- adding to a waste residue of a non-ferrous slag, a fossil fuel combustion residue or a mixture thereof during its formation in a furnace or burner a compound containing CaO and a compound containing Al.sub.2 O.sub.3 to form a first mixture having a sufficient CaO and Al.sub.2 O.sub.3 content to enable said first mixture to react with a composition comprising a sulphate anion, added thereto during a subsequent treatment step, to form a composition having pozzolanic qualities attainable by ettringite;
- grinding said first mixture so as to reduce the particle size thereof;
- increasing the pH of the first mixture to a sufficiently alkaline value by the addition of an alkaline compound to activate the alumina component of said first mixture and thus to provide said first mixture with a high early strength;
- adding to said first mixture a compound containing a sulphate anion and an additional amount of said compound containing CaO to form a second mixture;
- hydrating said second mixture with a sufficient quantity of water such that the proportional relationship among the CaO, Al.sub.2 O.sub.3 and sulphate components in said second mixture is such that the ratio thereamong approaches the stoichiometric relation of the components of the mineral ettringite;
- and
- allowing the second mixture to cure to a solid cementitious composition having the pozzolanic qualities of ettringite.
A method for making a cementitious composition which comprises:
- adding to a waste residue of a non-ferrous slag, a fossil fuel combustion residue or a mixture thereof during its formation in a furnace or burner a compound containing CaO and a compound containing Al.sub.2 O.sub.3 having a sufficient CaO and Al.sub.2 O.sub.3 content to enable said first mixture to react with a composition comprising a sulphate anion, added thereto during subsequent treatment step, to form a composition having increased pozzolanic qualities compared to the untreated waste residue;
- increasing the pH of the first mixture to a sufficiently alkaline value to activate the alumina component of said first mixture;
- and
- treating said first mixture by the addition thereto of a compound containing a sulphate anion so as to form a second mixture, the proportional relationship among the CaO, Al.sub.2 O.sub.3 and sulphate components in said second mixture forms a cementitious composition capable of being hydrated to a higher-grade pozzolanic material as compared to the untreated waste residue.
A method for making a cementitious composition which comprises:
- adding to a waste residue of a non-ferrous slag, a fossil fuel combustion residue or a mixture thereof during its formation in a furnace or burner, a compound containing CaO and a compound containing Al.sub.2 O.sub.3 to form a first mixture having a sufficient CaO and Al.sub.2 O.sub.3 content to enable said first mixture to react with a composition comprising a sulfate anion, added thereto during a subsequent treatment step, to form a composition having increased pozzolanic qualities as compared to the untreated waste residue;
- grinding said first mixture so as to reduce the particle size thereof;
- increasing the pH of the first mixture to a sufficiently alkaline value by the addition of an alkaline compound to activate the alumina component of said first mixture and thus to provide said first mixture with a high early strength;
- adding to said first mixture a compound containing a sulphate anion and an additional amount of said compound containing CaO to form a second mixture;
- hydrating said second mixture with a sufficient quantity of water such that the proportional relationship among the CaO, Al.sub.2 O.sub.3 and sulphate components in said second mixture forms a cementitious composition of a higher-grade pozzolanic material as compared to that obtainable from the untreated waste residue;
- and
- allowing said second mixture to cure so as to form a solid cementitious composition.