# US 4,746,576 A · Writing screen

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,746,576 A
- Document ID: US4746576A
- Status: Granted
- Kind: A
- Application number: 06/945,852
- Filed: 1986-12-23
- Granted: 1988-05-24
- Earliest claimed: 1985-12-25
- Assignees: Mitsubishi Petrochemical Co., Ltd.
- Inventors: Takahiro Ozu; Keizo Abe; Masayoshi Tsujii
- Web page: https://patentgrep.com/patent/US4746576A

## CPC

- B43L 1/002: {chemical details}
- Y10T 428/24901: including coloring matter
- Y10T 428/3154: Of fluorinated addition polymer from unsaturated monomers
- Y10T 428/31544: Addition polymer is perhalogenated
- B43L: ARTICLES FOR WRITING OR DRAWING UPON; {WRITING OR DRAWING AIDS;} ACCESSORIES FOR WRITING OR DRAWING (workshop equipment for marking-out work B25H7/00; teaching hand-writing or drawing G09B11/00)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A writing screen comprising a substrate and an overlayer on the surface thereof of a film comprising a vinylidene fluoride copolymer resin having a ratio of the existing amount of fluorine atoms (F) and that of carbon atoms (C), F/C, on the surface in the range of 0.6 to 1.5. The screen has excellent marker suitability and resistance to surface damage.

## Claims

### Claim 1

A writing screen, on which writing with a marker and erasing an ink of the marker with an eraser can be carried out, comprising a substrate structure and an overlayer on the surface thereof of a film comprising a vinylidene fluoride copolymer resin having a ratio of the existing amount of fluorine atoms (F) and that of carbon atoms (C), F/C, on the surface in the range of 0.7 to 1.5, which ratio is measured by X-ray photoelectron spectroscopy, which copolymer resin consists of 95 to 70% by weight of vinylidene fluoride and 5 to 30% by weight of hexafluoropropylene, said film being produced by melt molding.

### Claim 2 (depends on 1)

A writing screen according to claim 1 wherein the copolymer resin has an F/C in the range of 0.7 to 1.0.