Multilayer composite structure for smooth surfaces
AssigneeGeneral Electric Company
InventorBang M. Kim
Life of this patent
Estimating the term…
Abstract
Composite sheets with layers possessing different properties are provided which can be compression molded to produce molded panels with smooth glossy surfaces. A fiber free outer layer is laminated to a bulk layer comprising fiber mat compounded with thermoplastic resin filled with chopped fibers. The fiber free layer has a higher melt viscosity than the bulk layer.
Claims14
A composite sheet comprising:
- a fiber free layer of thermoplastic material;
- and
- a bulk layer comprising fiber mat compounded with thermoplastic resin, the fiber free layer laminated to the bulk layer, said thermoplastic material in the fiber free layer having a higher melt viscosity than the thermoplastic resin in the bulk layer to limit the movement of fibers from the bulk layer to the fiber free layer.
A composite sheet comprising fiber mat and
- a fiber free outer layer of thermoplastic material;
- a bulk layer comprising fiber mat and thermoplastic resin;
- barrier means situated between said fiber free layer and said bulk layer, said fiber free layer, bulk layer and barrier means laminated together, said barrier means limiting movement of fibers from said bulk layer to the fiber free layer.
A composite sheet comprising:
- a fiber free layer of thermoplastic material;
- and
- a bulk layer comprising woven glass fiber mat compounded with thermoplastic resin containing glass fibers, the fiber free layer laminated to the bulk layer, said thermoplastic material in the fiber free layer having a higher melt viscosity than the thermoplastic resin the bulk layer.
A method of making fiber reinforced composite sheets, comprising the steps of:
- (a) heating a fiber free thermoplastic resin layer to a temperature greater than the melting point.
- (b) heating a fiber mat and thermoplastic resin to a temperature higher than the fiber free thermoplastic resin layer, the fiber free thermoplastic resin layer and thermoplastic resin layer heated with the mat having substantially the same melting point, the fiber free thermoplastic resin being heated sufficiently less so that the resin in the fiber layer is more viscous than the resin heated with the mat;
- and
- (c) pressing the fiber free resin layer, the fiber mat and resin together so that the fiber free resin layer is on the exterior of the sheet.