Preparation and renovation of a fusion roller for a xerographic machine, fusion roller and vulcanizable composition
AssigneeAteliers de Conceptions et d'Innovations Industrielles
InventorLucien P. Michel
Life of this patent
Estimating the term…
Loading patent…
AssigneeAteliers de Conceptions et d'Innovations Industrielles
InventorLucien P. Michel
Estimating the term…
The invention relates to a method of preparation of an outer cover of a fusion roller for a xerographic machine, this cover being constituted by a homogeneous layer covering a hollow metal core receiving heating means. According to the invention, this method comprises the steps of (a) cold kneading a mixture having, for 100 parts of fluorine-containing rubber, 55 to 60 parts of carbon black, 2 to 6 parts of magnesium oxide, 4 to 8 parts of calcium hydroxyde and 0 to 2 parts of polyethylene wax; (b) forming the covering material by extrusion or calendering of this mixture; (c) application of this material in a homogeneous layer to the surface of the metallic core of the roller; (d) vulvanization at elevated temperature and under pressure of the material thus applied to the core; (e) dressing of the cover to a constant thickness.
A method of preparation of an external cover of a fusion roller for a xerographic machine, said cover being constituted by a homogeneous layer covering a hollow core receiving heating means, said method comprising the stages of:
A method of renovation of fusion rollers or a xerographic machine comprising the stages of:
A vulcanisable composition for a covering material for a fusion roller for a xerographic machine, said vulcanisable composition formed of a mixture having, for 100 parts of rubber of a fluorine-and-hydrogen-containing elastomer, 55 to 60 parts of carbon black, 2 to 6 parts of magnesium oxide, 4 to 8 parts of calcium hydroxide and 0 to 2 parts of polyethylene wax.
A vulcanizable composition for a covering material for a fusion roller for a xerographic machine, said vulcanizable composition formed of a mixture having, for 100 parts of rubber of a fluorine-containing elastomer, 55 to 60 parts of carbon black, 2 to 6 parts of magnesium oxide, 4 to 8 parts of calcium hydroxide and 1/2 to 2 parts of polyethylene wax.
Dependencies are inferred from the claim text.