Abstract
A method for increasing the bulk density and decreasing the time of wetting with water of a substantially anhydrous kaolin clay powder, comprising dry milling said powder in a media mill wherein the media is at least +5 mesh, and using work inputs of from about 5 to about 40 HP-hrs/ton of dry clay. The process enables improved handling characteristics for the treated clay with respect to bulk material handling systems.
Claims9
A method of preparing a calcined kaolin clay powder having increased bulk density and decreased wet-out time comprising:
- (a) heating a kaolin clay powder of fine particle size to at least 400.degree. C. to render same at least substantially anhydrous;
- and
- (b) dry milling said anhydrous clay powder in a media mill using media having a particle size of at least +5 mesh, and using a work input in the range of from about 5 to about 40 HP-hrs/ton of dry clay.