In a method of producing a reflector for a headlight, particularly for an automobile, comprising the manufacture of a wall having a core layer, of predetermined volume, intended to give said reflector its characteristics of mechanical strength and a skin layer of predetermined volume, at least partially enclosing said core layer on both sides, whilst defining a smooth concave face intended to form a reflective face of said reflector, by the succession of stages consisting in:
- (a) delimiting a mold for said wall, of a volume substantially corresponding to the sum of said predetermined volumes, by means of a convex mold face having a shape complementary to that of said concave face and of a concave mold face placed opposite said convex mold face and spaced from this latter, whilst arranging an injection aperture opening into said mold,
- (b) injecting into said mold, via said injection aperture a volume of thermoplastic skin material corresponding substantially to said predetermined volume of the skin layer, said thermoplastic material having a predetermined plasto-elasticity temperature and being injected at a temperature greater than this plasto-elasticity temperature,
- (c) injecting into said mold and into said thermoplastic skin material, via said injection aperture a volume of core material in a fluid state corresponding substantially to said predetermined volume of said core layer, whilst maintaining said thermoplastic skin material at a temperature greater than its plasto-elasticity temperature so that said core material in fluid state causes said thermoplastic skin material to progressively migrate against said convex and concave mould surfaces, in the direction of extension with respect to said injection aperture and that said thermoplastic skin material is sandwiched in the mold between on the one hand said core material and on the other hand said convex and concave mold faces,
- (d) permitting or causing a hardening of said thermoplastic skin material, at least, to obtain a rigid wall inside said mold,
- (e) disengaging from said mold said rigid wall thus obtained,
- the improvement comprising:
- during stage a, placing, projecting with respect to said concave mold face, inside said mold, a plurality of points spaced with respect to said injection aperture, mutually spaced and opposite said convex mold face, for preventing the migration of said thermoplastic skin material during stage c, against localised zones of said concave mold face, situated opposite from said injection aperture with respect to said different points, respectively, and then permitting access of said core material to said localised zones of said concave mold face,
- during stage c, injecting by way of core material a thermosetting material having a polycondensation temperature greater than the plasto-elasticity temperature of said thermoplastic skin material, whilst maintaining said mold at a temperature intermediate between said temperatures respectively of polycondensation and of plasto-elasticity and withdrawing said points with respect to said concave mold face at an intermediate stage of said injection of said thermosetting core material,
- preliminarily to stage d, arranging vents opening into said mold through said localised zones of said concave mold face,
- during stage d, causing heating of said mold to a temperature greater than said polycondensation temperature of said thermosetting core material then permitting or causing a cooling of said mold to a temperature lower than said plasto-elasticity temperature of said thermoplastic skin material.