Amorphous, iron promoted Mo and W sulfide hydroprocessing catalysts and uses thereof
AssigneeExxon Research & Engineering Co.
InventorsAllan J. Jacobson, Teh C. Ho, Russel R. Chianelli, Theresa A. Pecoraro
Life of this patent
Estimating the term…
Loading patent…
AssigneeExxon Research & Engineering Co.
InventorsAllan J. Jacobson, Teh C. Ho, Russel R. Chianelli, Theresa A. Pecoraro
Estimating the term…
Hydrocarbon feeds are upgraded by contacting a feed, at elevated temperature and in the presence of hydrogen, with a catalyst comprising an amorphous sulfide of iron and a metal selected from the group consisting of Mo, W and mixture thereof. The catalysts are prepared by heating one or more catalyst precursor salts under oxygen-free conditions in the presence of sulfur at a temperature of at least about 250.degree. C. The precursor salts will contain a thiometallate anion of Mo, W or mixture thereof and a cation comprising iron as a promoter metal and, optionally, additional divalent promoter metals, wherein said promoter metal or metals are chelated by at least one neutral, nitrogen-containing polydentate liquid and wherein said additional promoter metal is selected from the group consisting of Ni, Co, Mn, Zn, Cu and mixture thereof.
A composition of matter comprising a mixture of (a) an amorphous sulfide of iron and a metal selected from the group consisting of Mo, W and mixture thereof and, (b) metal sulfide of at least one promoter metal selected from the group consisting of Ni, Co, Mn, Zn, Cu and mixture thereof.
A process for preparing a catalyst composition comprising a mixture of (i) an amorphous sulfide of iron and at least one metal selected from the group consisting of Mo, W and mixture thereof and, (ii) metal sulfide of at least one promoter metal selected from the group consisting of Ni, Co, Mn, Zn, Cu and mixture thereof, said process comprising heating one or more precursors, at a temperature of at least about 150.degree. C., in the presence of sulfur and under oxygen-free conditions for a time sufficient to form said catalyst, wherein said precursor salts contain a thiometallate anion of Mo, W or mixture thereof and two or more cations comprising divalent iron and at least one additional divalent promoter metal selected from the group consisting of Ni, Co, Mn, Zn, Cu and mixture thereof, wherein said promoter metals in said cations are chelated by at least one neutral, nitrogen-containing polydentate ligand.
A process for preparing a catalyst comprising a mixture of (i) an amorphous sulfide of iron and at least one metal selected from the group consisting of Mo, W and mixture thereof and, (ii) metal sulfide of at least one promoter metal selected from the group consisting of Ni, Co, Mn, Zn, Cu and mixture thereof, said process comprising heating at least two precursor salts, at a temperature of at least about 200.degree. C., in the presence of sulfur and under oxygen-free conditions for a time to form said catalyst, wherein said precursor salts are of the formula (ML) (Mo.sub.y W.sub.1-y S.sub.4) wherein M comprises divalent Fe and at least one divalent promoter metal selected from the group consisting of Ni, Co, Mn, Zn, Cu and mixture thereof with Fe, wherein y is any value ranging from 0 to 1 and wherein L is one or more neutral, nitrogen-containing ligands, at least one of which is a chelating polydentate ligand.