Method of preparation of variable permeability fill material for use in subterranean formations
AssigneeHalliburton Company
InventorsJoseph R. Murphey, Kenneth D. Totty, Susan V. Fulton
Life of this patent
Estimating the term…
Abstract
A method and composition for filling voids in a subterranean formation to provide a fill having a substantially uniform permeability. A viscosified aqueous fluid is prepared to which is added a first particulate having a particle size no greater than about 10 mesh, another particulate having a particle size of less than about 1/7th the median diameter of the first particulate and a resin composition capable of coating at least a portion of the particulate. The fluid is introduced into a subterranean formation to fill at least a portion of the voids that may be present in the formation, compacted and allowed to set to provide the permeable fill material.
Claims20
A method of filling voids in a subterranean formation comprising the steps of:
- admixing an aqueous fluid with a viscosifying agent comprising a polysaccharide in an amount sufficient to viscosify said aqueous fluid;
- admixing a first particulate with said viscosified aqueous fluid, said particulate having a particle size of no greater than about 10 mesh;
- admixing a resin composition with said viscosified aqueous fluid in an amount of from about 4 to about 20% by weight of the particulate;
- admixing a second particulate with said viscosified aqueous fluid, said second particulate having a median diameter of less than about 1/7th the median diameter of said first particulate, said second particulate comprising from about 1 to about 30% by volume of the particulate present;
- coating said first particulate with said resin in said viscosified fluid prior to admixture of said second particulate whereby upon addition of said second particulate at least a portion of said second particulate is caused to cluster about and adhere to the individual particles of the first particulate;
- introducing said viscosified aqueous fluid containing said resin coated particulate into a subterranean formation containing voids whereby at least a portion of said voids are filled by said viscosified aqueous fluid containing said particulate;
- and
- compacting said particulate in said voids by application of pressure to said viscosified aqueous fluid to provide a fill material having a substantially uniform permeability upon hardening of the resin composition.
A method of filling voids in a subterranean formation comprising the steps of:
- admixing an aqueous fluid with a viscosifying agent comprising a polysaccharide in an amount sufficient to viscosify said aqueous fluid;
- admixing a first particulate with said viscosified aqueous fluid, said first particulate having a particle size of no greater than about 10 mesh;
- admixing another particulate with said viscosified aqueous fluid, said another particulate having a particle size having a median diameter of less than about 1/7th the median diameter of said first particulate, said another particulate comprising from about 1 to about 30% by volume of the particulate present;
- admixing a resin composition and a hardener with said viscosified aqueous fluid in an amount sufficient to effect at least partial coating of the total particulate admixed with said viscosified fluid whereby at least a portion of the first particulate is coated by said resin composition and at least a portion of said another particulate is caused to adhere upon the surface of said first particulate;
- introducing said viscosified aqueous fluid containing said resin coated particulate into a subterranean formation containing voids whereby at least a portion of said voids are filled by said viscosified aqueous fluid to provide a fill material upon hardening of said resin composition having a substantially uniform permeability.
A method of filling voids in a subterranean formation comprising the steps of:
- admixing an aqueous fluid with a viscosifying agent comprising a polysaccharide in an amount sufficient to vscosify said aqueous fluid;
- admixing in the following sequence:
- (a) a first particulate with said viscosified aqueous fluid, said particulates having a particle size of no greater than about 10 mesh;
- (b) a reson composition with said viscosified aqueous fluid in an amount of from about 4 to about 20% by weight of the particulate;
- and
- (c) a second particulate with said viscosified aqueous fluid, said second particulate having a median diameter of less than about 1/7th the median diameter of said first particulate, said second particulate comprising from about 1 to about 30% by volume of the particulate present;
- coating said first particulate with said resin in said viscosified fluid prior to admixture of said second particulate whereby upon addition of said second particulate at least a portion of said second particulate is caused to cluster about and adhere to the individual particles of the first particulate;
- introducing said viscosified aqueous fluid containing said resin coated particulate into a subterranean formation containing voids whereby at least a portion of said voids are filled by said viscosified aqueous fluid containing said particulate;
- and
- compacting said particulate in said voids by application of pressure to said viscosified aqueous fluid to provide a fill material having a substantially uniform permeability upon hardening of the resin composition.
A method of filling voids in a subterranean formation comprising the steps of:
- admixing an aqueous fluid with a viscosifying agent comprising a polysaccharide in an amount sufficient to viscosify said aqueous fluid;
- admixing in the following sequence:
- (a) a resin composition with said viscosified aqueous fluid in an amount of from about 4 to about 20% by weight of the particulate;
- (b) a first particulate with said viscosified aqueous fluid, said particulate having a particle size of no greater than about 10 mesh;
- (c) a second particulate with said viscosified aqueous fluid, said second particulate having a median diameter of less than about 1/7th the median diameter of said first particulate, said second particulate comprising from about 1 to about 30% by volume of the particulate present,
- coating said first particulate with said resin in said viscosified fluid prior to admixture of said second particulate whereby upon asddition of said second particulate at least a portion of said second particulate is caused to cluster about and adhere to the individual particles of the first particulate;
- introducing said viscosified aqueous fluid containing said resin coated particulate into a subterranean formation containing voids whereby at least a portion of said voids are filled by said viscosified aqueous fluid containing said particulate;
- and
- compacting said particulate in said voids by application of pressure to said viscosified aqueous fluid to provide a fill material having a substantially uniform permeability upon hardening of the resin composition.
A method of filling voids in a subterranean formation comprising the steps of:
- admixing an aqueous fluid with a viscosifying agent comprising a polysaccharide in an amount sufficient to viscosify said aqueous fluid;
- admixing in the following sequence;
- (a) a first particulate with said viscosified aqueous fluid, said first particulate having a particle size of no greater than about 10 mesh;
- (b) a resin composition and a hardener with said visosified aqueous fluid in an amount sufficient to effect at least partial coating of the total particulate admixed with said viscosified fluid;
- and
- (c) another particulate with said viscosified aqueous fluid, said another particulate having a particle size having a median diameter of less than about 1/7th the median diameter of said first particulate said another particulate comprising from about 1 to about 30% by volume of the particulate present,
- whereby at least a portion of the first particulate is coated by said resin composition and at least a portion of said another particulate is caused to adhere upon the surface of said first particulate;
- introducing said viscosified aqueous fluid containing said resin coated particulate into a subterranean formation containing voids whereby at least a portion of said voids are filled by said viscosified aqueous fluid to provide a fill material upon hardening of said resin composition having a substantially uniform permeability.
A method of filling voids in a subterranean formation comprising the steps of:
- admixing an aqueous fluid with a visosifying agent comprising a polysaccharide in an amount sufficient to viscosify said aqueous fluid;
- admixing in the following sequence:
- (a) a resin composition and a harder with said viscosified aqueous fluid in an amount sufficient to effect at least partial coating of the total particulate to be admixed with said viscosified fluid;
- (b) a first particulate with said viscosified aqueous fluid, said first particulate having a particle size of not greater than about 10 mesh;
- and
- (c) another particulate with said vscosified aqueous fluid, said another particulate having a particle size having a median diameter of less than about 1/7th the median diameter of said first particulate said another particulate comprising from about 1 to about 30% by volume of the particulate present,
- whereby at least a portion of the first particulate is coated by said resin composition and at least a portion of said another particulate is caused to adhere upon the surface of said first particulate;
- introducing said viscosified aqueous fluid containing said resin coated particulate into a subterranean formation containing voids whereby at least a portion of said voids are filled by said viscosified aqueous fluid to provide a fill material upon hardening dening of said resin composition having a substantially uniform permeability.