# US 4,554,313 A · Process for preparing bitumen-polymer compositions, application of these compositions of the obtention of coverings and mother solution of polymer usable for the obtention of the said compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,554,313 A
- Document ID: US4554313A
- Status: Granted
- Kind: A
- Application number: 06/502,827
- Filed: 1983-06-09
- Granted: 1985-11-19
- Earliest claimed: 1982-06-10
- Assignees: Societe Anonyme dite: Elf France
- Inventors: Germain Hagenbach; Paul Maldonado; Jacques Maurice
- Web page: https://patentgrep.com/patent/US4554313A

## CPC

- C10C 3/026: {with organic compounds}
- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- C10C: WORKING-UP PITCH, ASPHALT, BITUMEN, TAR; PYROLIGNEOUS ACID (compositions of bituminous materials C08L95/00; carbon filaments by decomposition of organic filaments D01F9/14)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Bitumen-polymer compositions are prepared, by mixing, at between 130.degree. C. and 230.degree. C., a bitumen with a styrene and conjugated diene copolymer and a sulphur source, the copolymer and the sulphur source being added to the bitumen either directly, or in the form of a mother solution in a hydrocarbon oil, then by maintaining the whole under stirring at between 130.degree. C. and 230.degree. C. for at least fifteen minutes. By way of sulphur source is used 0.005 to 15% by weight, with respect to bitumen, one or several polymeric or not, cyclic or linear polysulphides, and especially ditertiododecyl or dinonyl pentasulphide. The bitumen-polymer compositions obtained can be used for the obtention of superficial road coverings and present a constant quality of its properties.

## Claims

### Claim 1

A process for the preparation of a bitumen-polymer composition which comprises:
(a) forming a mixture of a bitumen, from about 0.5 to 15% by weight of the bitumen of a styrene-conjugated diene copolymer and from about 0.005 to 15% by weight of the bitumen of a polysulfide of the formula:
R.sub.1 --(S).sub.m (R--(S).sub.m).sub.x R.sub.2
wherein R.sub.1 and R.sub.2 are each independently a C.sub.1 to C.sub.20 saturated monovalent hydrocarbon radical or a C.sub.1 to C.sub.20 unsaturated monovalent hydrocarbon radical, or R.sub.1 and R.sub.2 can be linked to form a C.sub.1 to C.sub.20 saturated divalent hydrocarbon radical or a C.sub.1 to C.sub.20 unsaturated divalent hydrocarbon radical; R is a C.sub.1 to C.sub.20 saturated divalent hydrocarbon radical or a C.sub.1 to C.sub.20 unsaturated divalent hydrocarbon radical; (S).sub.m is a divalent group of m sulfur atoms wherein m can be different for each group and represents a whole number of from 1 to about 6 with at least m in one group being at least 2; and x is a whole number ranging from 0 to 10; and
(b) heating the mixture at a temperature of from about 130.degree. C. to about 230.degree. C. for at least 15 minutes to form the bitumen-polymer composition.

### Claim 2 (depends on 1)

A process according to claim 1, wherein the polysulfide is a compound of the formula:
R.sub.1 --(S)n--R.sub.2
wherein (S).sub.n is a divalent group of n sulfur atoms with n being an integer of from 2 to 6.

### Claim 3 (depends on 1, 2)

A process according to claim 1 or 2, wherein the R.sub.1 and R.sub.2 radicals of the polysulfide are identical and selected from the group consisting of C.sub.1 and C.sub.20 alkyl radicals, C.sub.6 to C.sub.20 cycloalkyl radicals and C.sub.6 to C.sub.20 aryl radicals or R.sub.1 and R.sub.2 are linked together to form a divalent radical selected from the group consisting of C.sub.1 to C.sub.20 alkylene radicals, C.sub.6 to C.sub.20 cycloalkylene radicals and C.sub.6 to C.sub.20 arylene radicals, and the R divalent radical is selected from the group consisting of C.sub.1 to C.sub.20 alkylene radicals, C.sub.6 to C.sub.20 cycloalkylene radicals and C.sub.6 to C.sub.20 arylene radicals.

### Claim 4 (depends on 1)

A process according to claim 1, wherein the polysulfide is a compound of the formula:
R.sub.3 --(S).sub.p --R.sub.3
wherein (S).sub.p is a divalent group of p sulfur atoms with p being an integer of from 2 to 5 and the R.sub.3 are each a C.sub.6 to C.sub.16 alkyl radical.

### Claim 5 (depends on 1, 4)

A process according to claim 1 or 4, wherein the polysulfide is used in a quantity ranging from about 0.1% to about 5% by weight of the bitumen.

### Claim 6 (depends on 1, 4)

A process according to claim 1 or 4, wherein the bitumen has a penetration between 5 and 500.

### Claim 7 (depends on 1, 4)

A process according to claim 1 or 4, wherein the copolymer is a random copolymer or a block copolymer of styrene with a conjugated diene, said diene being selected from the group consisting of butadiene, isoprene, chloroprene, carboxylated butadiene and carboxylated isoprene.

### Claim 8 (depends on 1, 4)

A process according to claim 1 or 4, wherein the copolymer has a weight content in styrene ranging from 15 to 40%.

### Claim 9 (depends on 1, 4)

A process according to claim 1 or 4, wherein the copolymer has an average viscosimetric molecular weight between 30,000 and 300,000.

### Claim 10 (depends on 1, 4)

A process according to claim 1 or 4, wherein the quantity of copolymer added to the bitumen is between about 0.7% and about 10% by weight of the bitumen.

### Claim 11 (depends on 1, 4)

A process according to claim 1 or 4, wherein the copolymer and polysulfide are incorporated into the bitumen in the form of a mother solution of these two products in a solvent consisting of a hydrocarbon oil having a distillation range between 100.degree. C. and 450.degree. C. at atmospheric pressure.

### Claim 12 (depends on 11)

A process according to claim 11, wherein the hydrocarbon oil is selected from the group consisting of petroleum cuts having an aromatic character, petroleum cuts having a naphtheno-paraffinic character, petroleum cuts having a naphtheno-aromatic character, coal oils and, oils of vegetable origin.

### Claim 13 (depends on 11)

A process according to claim 11, wherein the mother solution is prepared by contacting the ingredients entering into its composition, under stirring, at temperatures between 20.degree. C. and 170.degree. C.

### Claim 14 (depends on 11)

A process according to claim 11, wherein the respective quantities of copolymer and polysulfide in the mother solution range from 5% to 40% and from 0.1% to 15% by weight of the hydrocarbon oil.

### Claim 15 (depends on 11)

A process according to claim 11, wherein the mother solution contains from 10% to 35% copolymer and 0.5% to 5% polysulfide expressed by weight, of the hydrocarbon oil.

### Claim 16 (depends on 1, 4)

A process according to claim 1 or 4, wherein bitumen has a penetration between 20 and 400.

### Claim 17 (depends on 1, 4)

A process according to claim 1 or 4, wherein the bitumen is selected form the group consisting of direct distillation bitumens, blown bitumens, and semi-blown bitumens.

### Claim 18 (depends on 1, 4)

A process according to claim 1 or 4, wherein the copolymer has an average viscosimetric molecular weight between 70,000 and 200,000.

### Claim 19 (depends on 11)

A process according to claim 11, wherein the hydrocarbon oil has a distillation range between 150.degree. C. and 370.degree. at atmospheric pressure.

### Claim 20 (depends on 11)

A process according to claim 11, wherein the mother solution is prepared by contacting the ingredients entering into its composition, under stirring, at temperatures between 40.degree. C. and 120.degree. C.

### Claim 21 (depends on 1)

A bitumen-polymer composition prepared by the process according to claim 1.

### Claim 22

A process for the preparation of a bitumen-polymer composition which comprises:
(a) contacting, at a temperature between 130.degree. C. and 230.degree. and under stirring, from 80% to 95% by weight of a bitumen with 20% to 5% by weight of a mother solution, which consists of a solution of a styrene/conjugated diene copolymer and a polysulfide in a solvent consisting of a hydrocarbon oil having a distillation range between 100.degree. C. and 450.degree. C. at atmospheric pressure and contains, by weight of the solvent, from 10% to 35% copolymer and 0.5% to 5% polysulfide, said polysulfide having the formula:
R.sub.1 --(S).sub.m --R--(S).sub.m)R.sub.2
wherein R.sub.1 and R.sub.2 are each independently a C.sub.1 to C.sub.20 saturated monovalent hydrocarbon radical or a C.sub.1 to C.sub.20 unsaturated monovalent hydrocarbon radical or R.sub.1 and R.sub.2 can be linked to form a C.sub.1 to C.sub.20 saturated divalent hydrocarbon radical or a C.sub.1 to C.sub.20 unsaturated divalent hydrocarbon radical, R is a C.sub.1 to C.sub.20 saturated divalent hydrocarbon radical or a C.sub.1 to C.sub.20 unsaturated divalent hydrocarbon radical, (S).sub.m is a divalent group of m sulfur atoms wherein m can be different for each group and represents a whole number of from 1 to about 6 with at least m in one group being at least 2 and x is a whole number ranging from 0 to 10; and
(b) maintaining the thus obtained mixture, under stirring, at a temperature of from about 130.degree. C. to about 230.degree. C. for period of at least 15 minutes to form the bitumen-polymer composition.

### Claim 23 (depends on 22)

A process according to claim 22, wherein said period of time is between 15 and 90 minutes.

### Claim 24 (depends on 22)

A process according to claim 22, wherein during said period of time the mixture is maintained at a temperature corresponding to that prevailing during the step of contacting the bitumen with the mother solution.

### Claim 25 (depends on 22)

A process according to claim 22, wherein the polysulfide is a compound of the formula:
R.sub.1 --(S).sub.n --R.sub.2
wherein (S).sub.n is a divalent group of n sulfur atoms with n being an integer of from 2 to 6.

### Claim 26 (depends on 22)

A process according to claim 22, wherein the R.sub.1 and R.sub.2 radicals of the polysulfide are identical and selected from the group consisting of C.sub.1 to C.sub.20 alkyl radicals, C.sub.6 to C.sub.20 cycloalkyl radicals and C.sub.6 to C.sub.20 aryl radicals or R.sub.1 and R.sub.2 are linked together to form a divalent radical selected from the group consisting of C.sub.1 to C.sub.20 alkylene radicals, C.sub.6 to C.sub.20 cycloalkylene radicals and C.sub.6 to C.sub.20 arylene radicals and the R divalent radical is selected from group consisting of C.sub.1 to C.sub.20 alkylene radicals, C.sub.6 to C.sub.20 cycloalkylene radicals and C.sub.6 to C.sub.20 arylene radicals.

### Claim 27 (depends on 22)

A process according to claim 22, wherein the polysulfide is a compound of the formula:
R.sub.3 --(S).sub.p --R.sub.3
wherein (S).sub.p is a divalent group of p sulfur atoms with p being an integer of from 2 to 5 and R.sub.3 are each a C.sub.6 to C.sub.16 alkyl radical.

### Claim 28 (depends on 22)

A process according to claim 22, wherein the bitumen has a penetration between 5 and 500.

### Claim 29 (depends on 22)

A process according to claim 22, wherein the copolymer is a random copolymer or a block copolymer of styrene with conjugated diene, said diene being selected from the group consisting of butadiene, isoprene, chloroprene, carboxylated butadiene and carboxylated isoprene.

### Claim 30 (depends on 22)

A process according to claim 22, wherein the copolymer has a weight content in styrene ranging from 15 to 40%.

### Claim 31 (depends on 22)

A process according to claim 22, wherein the copolymer has an average viscosimetric molecular weight between 30,000 and 300,000.

### Claim 32 (depends on 22)

A process according to claim 22, wherein the hydrocarbon oil is selected from the group consisting of petroleum cuts having an aromatic character, petroleum cuts having a naphtheno-paraffinic character, petroleum cuts having a naphtheno-aromatic character, coal oils and, oils of vegetable origin.

### Claim 33 (depends on 22)

A process according to claim 22, wherein the mother solution is prepared by contacting the ingredients entering into its composition, under stirring, at temperatures between 20.degree. C. and 170.degree. C.

### Claim 34 (depends on 22)

A process according to claim 22, wherein the bitumen has a penetration between 20 and 400.

### Claim 35 (depends on 22)

A process according to claim 22, wherein the bitumen is selected from the group consisting of direct distillation bitumens, blown bitumens and semi-blown bitumens.

### Claim 36 (depends on 22)

A process according to claim 22, wherein the copolymer has an average viscosimetric molecular weight between 70,000 and 200,000.

### Claim 37 (depends on 22)

A process according to claim 22, wherein the hydrocarbon oil has a distillation range between 150.degree. C. and 370.degree. C. at atmospheric pressure.

### Claim 38 (depends on 22)

A process according to claim 22, wherein the ingredients forming the mother solution are contacted, under stirring, at temperatures between 40.degree. C. and 120.degree. C. to produce the mother solution.

### Claim 39 (depends on 22)

A bitumen-polymer composition prepared by the process according to claim 22.

### Claim 40 (depends on 11)

A bitumen-polymer composition prepared by a process of claim 11.