Method of touching up surface-blemished matt-finished surface grained colored molded plastic parts
AssigneeChem-Pak, Inc.
InventorGeorge P. Duane, Jr.
Life of this patent
Estimating the term…
Loading patent…
AssigneeChem-Pak, Inc.
InventorGeorge P. Duane, Jr.
Estimating the term…
Surface finish blemishes in "color coded" surface grained parts injection molded from colored plastic can be removed by spraying the blemished surface area of the part with a sprayable mixture comprised of (a) a substantially non-yellowing, solvent-soluble generally transparent, binder resin in the amount of about 2-10%, (b) a finely divided flatting pigment which is generally transparent when suspended in said resin, the amount of said pigment being about 0.4-1%, and (c) about 90-95% of a volatile solvent medium effective to dissolve said resin without destroying the surface grain of the part when sprayed thereon, thereby to cover the blemished area with at least one coating of a transparent, matt-surfaced solid film of flatting pigment dispersed in said resin which coating blends substantially completely uniformly with the original matt finish of said part. Where the part is molded of a plastic which is solvent-resistant such as polyethylene or polypropylene, a chlorinated polyolefin resin is added in the amount of about 0.2-2% and sufficient to promote adhesion to said surface, such polyolefin resin being compatible with said binder resin and soluble in said solvent medium at least prior to evaporation of the latter.
A method of removing surface finish blemishes in matt-finished injected molded color-coded, grained plastic parts, which comprises spraying the surface area of said part containing such blemishes with a sprayable mixture comprised of (a) a resin component consisting essentially of a substantially nonyellowing, solvent-soluble substantially transparent, binder resin which comprises an acrylic resin, (b) a finely divided flatting pigment which is substantially transparent when in said resin component, the amount of said pigment being about 0.4-1%, and (c) about 85-95% of a volatile solvent medium effective to dissolve said resin component at least before the evaporation thereof and upon spraying on said surface area of said part to wet the same without significantly softening that surface area and thereby degrading the grained finish thereof, thereby to cover the blemished area with at least one coating of a transparent, matt-surfaced solid film of flatting pigment dispersed in said resin component and blending substantially uniformly with the original matt surface finish of said part, all percentages being by weight of the total mixture.
A method of removing surface finish blemishes in matt-finished injected molded color-coded, grained plastic parts molded from solvent-resistant polyolefin plastic, which comprises spraying the surface area of said part containing such blemishes with a sprayable mixture of (a) a finely divided flatting pigment in the amount of about 0.4-1.0%, (b) a resin component for adhering said pigment to said surface consisting essentially of a substantially nonyellowing, solvent-soluble substantially transparent, binder resin, said pigment being substantially transparent when in said resin component, and (c) about 85-95% of a volatile solvent medium effective to dissolve said resin component at least before the evaporation thereof and upon spraying on said surface area of said part to wet the same without significantly softening that surface area and thereby degrading the grained finish thereof, thereby to cover the blemished area with at least one coating of a transparent, matt-surfaced solid film of flatting pigment dispersed in said resin component and blending substantially uniformly with the original matt surface finish of said part, all percentages being by weight of the total mixture.