Back to results
US 4,542,112 AGranted
Method for producing spinel fine powders
AssigneeNGK Insulators, Ltd.
InventorsMinoru Matsui, Tomonori Takahashi
Life of this patent
Estimating the term…
Abstract
Spinel fine powders having high purity suitable for raw materials for producing a dense and uniform spinel sintered body, are produced by hydrolyzing an alcohol solution of specifically defined magnesium alkoxides and aluminum alkoxides in a specific mixing ratio.
Claims14
A method for producing spinel fine powders comprising the steps of:
- (a) dissolving 1 mole of magnesium alkoxide of the formula
- Mg(OR).sub.2
- wherein R is an alkyl group having 1-3 carbon atoms, and, from 2.1 to 3 moles of aluminum alkoxide of the formula
- Al(OR').sub.3
- wherein R' is an alkyl group having 1-3 carbon atoms, in an alcohol of the formula
- R"OH
- wherein R" is an alkyl group having 1-3 carbon atoms to form a solution;
- (b) hydrolyzing said solution;
- and
- (c) heating precipitates formed by said hydrolysis at temperatures from 700.degree. C. to 1200.degree. C. to form fine powders consisting of single-phase spinel-structured solid solutions of oxides of aluminum and magnesium of the formula
- MgOxAl.sub.2 O.sub.3
- wherein x is from 1.05 to 1.5.