High molecular weight unsaturated polyesters of cyclohexanedimethanols
AssigneeEastman Kodak Company
InventorsWinston J. Jackson, Jr., Herbert F. Kuhfuss, Joseph J. Watkins
Life of this patent
Estimating the term…
Abstract
Disclosed are linear, high molecular weight unsaturated polyesters prepared by reacting essentially equimolar amounts of an acid selected from maleic acid, maleic anhydride or fumaric acid and cyclohexanedimethanol at temperatures of less than about 200.degree. C. until an I.V. of about 0.5 is reacted.
Claims9
A linear unsaturated polyester comprising 100 mole % of an acid component and 100 mole % of a glycol component, said acid component comprising at least 50 mole % of repeat units from maleic or fumaric acid, and said glycol component consisting essentially of repeat units from 1,3-cyclohexanedimethanol, 1,4-cyclohexanedimethanol or mixtures thereof, said polyester having an I.V. of at least 0.5.
A linear unsaturated polyester wherein said acid component comprises at least 50 mole % of repeat units from maleic acid or maleic anhydride.
A linear unsaturated polyester wherein said acid component comprises at least 50 mole % of repeat units from fumaric acid.
A linear unsaturated polyester wherein said glycol component consists essentially of 1,3-cyclohexanedimethanol.
A linear unsaturated polyester wherein said glycol component consists essentially of 1,4-cyclohexanedimethanol.
A process for preparing linear, high molecular weight polyesters which comprises reacting about 100 mole % of an acid component comprising at least 50 mole % maleic acid, maleic anhydride or fumaric acid with about 100 mole % of a glycol component consisting essentially of 1,3-cyclohexanedimethanol or 1,4-cyclohexanedimethanol at a temperature of between about 160.degree. C. and about 200.degree. C. until an I.V. of at least 0.5 is reached.
Dependencies are inferred from the claim text.