Polyacrylonitrile (PAN) fiber of high strength (tensile strength.gtoreq.20 g/d) produced from a polymer composed mainly of acrylonitrile (AN) and having a weight average molecular weight not less than 400,000, and a method of producing said fiber characterized by a multistage stretching step and a drying step under particular conditions.
Claims1
A polyacrylonitrile fiber having a tensile strength not less than 20 g/d, and produced from a polymer composed mainly of acrylonitrile and having a weight average molecular weight not less than 400,000.