# US 4,532,066 A · Stable mildly acidic aqueous polishing cleanser and preparation thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,532,066 A
- Document ID: US4532066A
- Status: Granted
- Kind: A
- Application number: 06/585,947
- Filed: 1984-03-05
- Granted: 1985-07-30
- Earliest claimed: 1984-03-05
- Assignees: Sterling Drug Inc.
- Inventors: Leon E. Paszek; Ernest Bernarducci
- Web page: https://patentgrep.com/patent/US4532066A

## CPC

- C11D 3/2082: {Polycarboxylic acids-salts thereof}
- C09D 9/02: with abrasives
- C11D 3/124: {Silicon containing, e.g. silica, silex, quartz or glass beads}
- C11D 3/1266: {in liquid compositions}
- C23F 3/00: Brightening metals by chemical means
- C11D: DETERGENT COMPOSITIONS; USE OF SINGLE SUBSTANCES AS DETERGENTS; SOAP OR SOAP-MAKING; RESIN SOAPS; RECOVERY OF GLYCEROL
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25

## Abstract

A stable mildly acidic aqueous polishing cleanser for removing stains from hard surfaces comprising by weight from about 8 to 20% of a polishing agent having an average particle size of about 2 to 10 microns and a particle size distribution from about 1 to 40 microns, from about 1 to 5% of a nonionic surfactant, from about 1 to 2.25% of a thickening agent comprising smectite clay and xanthan gum in a ratio of about 2:1 respectively, from about 1.25 to 6.25% of an oxalate salt selected from ammonium bioxalate or a mixture of ammonium bioxalate and ammonium oxalate, and from about 68 to 89% of water, said cleanser having a pH of about 3.0 to 4.5. Preparation of the cleanser and its properties are given.

## Claims

### Claim 1

A stable mildly acidic aqueous polishing cleanser for removing stains from hard surfaces comprising by weight from about 8 to 20% of a polishing agent having an average particle size of about 2 to 10 microns and a particle size distribution from about 1 to 40 microns, from about 1 to 5% of a nonionic surfactant, from about 1 to 2.25% of a thickening agent comprising smectite clay and xanthan gum in a ratio of about 2:1 respectively, from about 1.25 to 6.25% of an oxalate salt selected from ammonium bioxalate or a mixture of ammonium bioxalate and ammonium oxalate, and from about 68 to 89% of water, said cleanser having a pH of about 3.0 to 4.5.

### Claim 2 (depends on 1)

A polishing cleanser according to claim 1 comprising by weight about 14 to 16% of a polishing agent having an average particle size of about 2 microns and a particle size distribution of about 1 to 15 microns, about 2 to 3% of a nonionic surfactant, about 1.0 to 1.1% of smectite clay, about 0.5 to 0.60 of xanthan gum and about 3.75 to 5% of an oxalate salt, and having a pH of about 3.5 to 4.0.

### Claim 3

The process for preparing a stable mildly acidic aqueous polishing cleanser for removing stains from hard surfaces comprising by weight from about 8 to 20% of a polishing agent having an average particle size of about 2 to 4 microns, from about 1 to 5% of a nonionic surfactant, from about 1 to 2.25% of a thickening agent consisting of smectite clay and xanthan gum in a weight ratio of about 2:1 respectively, from about 1.25 to 6.25% of an oxalate salt selected from ammonium bioxalate or a mixture of ammonium bioxalate and ammonium oxalate, and from about 68 to 89% of water, said process which comprises adding successively with stirring or mixing to the water heated to about 110.degree.-150.degree. F. the polishing agent, the smectite clay, the xanthan gum and the nonionic surfactant, cooling the mixture to at least below 80.degree. F., then adding successively with stirring or mixing about 1 to 5% by weight of oxalic acid as its dihydrate and about 1.2 to 1.6 mole equivalent of ammonium hydroxide per mole of oxalic acid, and, if necessary, adjusting the pH to about 3.0 to 4.5.

### Claim 4 (depends on 3)

The process according to claim 3 utilizing about 14 to 16% of a polishing agent having an average particle size about 2 microns and a particle size distribution of about 1 to 15 microns, about 2 to 3% of a nonionic surfactant, about 1.0 to 1.1% of smectite clay, about 0.5 to 0.60% of xanthan gum, about 3 to 4% of oxalic acid and about 2.34% to 3.12% of concentrated aqueous ammonium hydroxide solution, and having a pH of about 3.5 to 4.0.

### Claim 5

The process for preparing a stable mildly acidic aqueous polishing cleanser for removing stains from hard surfaces comprising by weight from about 8 to 20% of a polishing agent having an average particle size of about 2 to 10 microns and having a particle size distribution from about 1 to 40 microns, from about 1 to 5% of a nonionic surfactant, from about 1 to 2.25% of a selected thickening agent, about 1.25 to 6.25% of an oxalate salt selected from ammonium bioxalate or a mixture of ammonium bioxalate and ammonium oxalate, and, from about 68 to 89% of water, said process which comprises adding successively with stirring or mixing to the water, smectite clay, xanthan gum, the nonionic surfactant, about 1 to 5% by weight of oxalic acid as its dihydrate about 1.2 to 1.6 mole equivalent of ammonium hydroxide per mole of oxalic acid, if necessary adjusting the pH to about 3.0 to 4.5, and, the polishing agent.

### Claim 6 (depends on 5)

The process according to claim 5 utilizing about 14 to 16% of a polishing agent having an average particle size about 2 microns and a particle size distribution of about 1 to 15 microns, about 1.0 to 1.1 g of smectite clay, about 0.50 to 0.60% of xanthan gum, about 2 to 3% of nonionic surfactant, about 3 to 4% of oxalic acid and about 2.34% to 3.12% of concentrated aqueous ammonium hydroxide solution, and having a pH of about 3.5 to 4.0.