# US 4,492,628 A · Method of treating clay to improve its whiteness

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,492,628 A
- Document ID: US4492628A
- Status: Granted
- Kind: A
- Application number: 06/411,588
- Filed: 1982-08-25
- Granted: 1985-01-08
- Earliest claimed: 1982-08-25
- Assignees: Freeport Kaolin Company
- Inventors: Raymond H. Young; Horton H. Morris; Robert L. Brooks
- Web page: https://patentgrep.com/patent/US4492628A

## CPC

- B28C 1/08: Separating suspensions, e.g. for obtaining clay, for removing stones; {Cleaning clay slurries}
- B03D 1/016: Macromolecular compounds
- B03D 1/02: Froth-flotation processes
- B03D 3/06: Flocculation
- B03D 2201/005: Dispersants
- Y02P 40/60: Production of ceramic materials or ceramic elements, e.g. substitution of clay or shale by alternative raw materials, e.g. ashes
- B28C: PREPARING CLAY; PRODUCING MIXTURES CONTAINING CLAY OR CEMENTITIOUS MATERIAL, e.g. PLASTER (preparing material for foundry moulds B22C5/00)
- B03D: FLOTATION; DIFFERENTIAL SEDIMENTATION (sedimentation in general B01D21/00; in combination with other separation of solids B03B; sink-float separation B03B5/28; detergents, soaps C11D)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of treating a clay to remove therefrom titanium mineral impurities comprising the steps of mixing an aqueous slurry of said clay having a high solids content with an activator and a collector for the titanium mineral impurities; conditioning the aqueous clay slurry at said high solids content for a time sufficient to dissipate therein at least 25 horsepower hours of energy per ton of solids; adding to the conditioned aqueous clay slurry a polyacrylate salt deflocculant; subjecting the conditioned aqueous clay slurry undiluted containing the polyacrylate salt deflocculant to a froth flotation process and removing the titanium impurities with the froth; and recovering clay having a reduced titanium minerals impurities content.

## Claims

### Claim 1

A method of treating clay to remove therefrom titanium mineral impurities, said method comprising the steps of:
(a) mixing said clay in the form of an aqueous slurry having a solids content of clay and said impurities of at least 20% by weight with a collector for the titanium mineral impurities, and an activator for the titanium mineral impurities comprising a water-soluble salt of a metal chosen from the alkaline earth metals and the heavy metals;
(b) conditioning the aqueous clay slurry at a solids content of at least 20% by weight for a time sufficient to dissipate therein at least 25 horsepower hours of energy per ton of solids at a pH below 7;
(c) mixing a polyacrylate salt deflocculant with the resulting conditioned aqueous clay slurry after conditioning;
(d) subjecting the resulting mixture of conditioned aqueous slurry having a solids content of at least 20 wt. % and the polyacrylate salt deflocculant to an air flotation process by passing air bubbles upwardly through the conditioned aqueous slurry and removing titanium mineral impurities with the froth; and
(e) recovering clay having a reduced titanium minerals impurities content.

### Claim 2 (depends on 1)

Method as claimed in claim 1 wherein the first stage of said flotation step (d) is carried out at an acid pH and an alkaline pH is used in succeeding stages of said flotation step.

### Claim 3 (depends on 1)

Method as claimed in claim 1 wherein, prior to mixing said clay slurry with said collector and activator, said clay slurry is bleached with an oxidative bleach at a pH of about 6 to about 7.

### Claim 4 (depends on 3)

Method as claimed in claim 3 wherein said oxidative bleach is potassium monopersulfate.

### Claim 5 (depends on 3)

Method as claimed in claim 3 wherein the polyacrylate salt deflocculant used in step (c) is the sodium salt.

### Claim 6 (depends on 3)

Method as claimed in claim 3 wherein the polyacrylate salt deflocculant used in step (c) is the lithium salt.

### Claim 7 (depends on 3)

Method as claimed in claim 3 wherein the polyacrylate salt deflocculant used in step (c) is the ammonium salt.

### Claim 8 (depends on 1)

Method as claimed in claim 1 wherein said conditioning step (b) is carried out in a conditioning vessel and the resulting conditioned clay slurry is transferred to a froth flotation device wherein steps (c) and (d) are carried out.

### Claim 9 (depends on 8)

Method as claimed in claim 8 wherein slurry treated by the froth flotation is removed from the froth flotation device and air is bubbled into the removed slurry which then is recycled to the froth flotation of step (d).

### Claim 10 (depends on 1)

Method as claimed in claim 1, wherein said polyacrylate salt deflocculant used in step (c) is the lithium salt.

### Claim 11 (depends on 10)

Method as claimed in claim 10 wherein, prior to bleaching said clay slurry is dispersed with a dispersant.

### Claim 12 (depends on 11)

Method as claimed in claim 11 wherein said dispersant is sodium silicate.

### Claim 13 (depends on 10)

Method as claimed in claim 10 wherein said collector is oleic acid and said activator includes calcium oxide and/or calcium chloride.

### Claim 14 (depends on 10)

Method as claimed in claim 10 wherein said collector is oleic acid and said activator is a ferrous compound.

### Claim 15 (depends on 10)

Method as claimed in claim 10 wherein said clay contains iron mineral impurities and said activator is a ferrous salt formed in situ by adding a reducing agent in place of some or all of said activator in step (a).

### Claim 16 (depends on 15)

Method as claimed in claim 15 wherein said reducing agent is sodium dithionite.

### Claim 17 (depends on 10)

Method as claimed in claim 10 wherein, after said froth flotation (d), said slurry is flocculated and bleached with a reductive bleach.

### Claim 18 (depends on 17)

Method as claimed in claim 17 wherein said slurry is flocculated with sulfuric acid and said reductive bleach is sodium dithionite.

### Claim 19 (depends on 17)

Method as claimed in claim 17 wherein, before flocculation and reductive bleaching, said slurry is allowed to settle and is dewatered by decanting.