# US 4,452,882 A · Silver halide photographic materials and process of developing them

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,452,882 A
- Document ID: US4452882A
- Status: Granted
- Kind: A
- Application number: 06/489,907
- Filed: 1983-04-29
- Granted: 1984-06-05
- Earliest claimed: 1982-04-30
- Assignees: Fuji Photo Film Co., Ltd.
- Inventors: Yoshitaka Akimura; Eiichi Okutsu; Shigenori Moriuchi; Naomi Saeki; Taiji Hashimura; Hiroyuki Mifune
- Web page: https://patentgrep.com/patent/US4452882A

## CPC

- G03C 1/043: Polyalkylene oxides; Polyalkylene sulfides; Polyalkylene selenides; Polyalkylene tellurides
- Y10S 430/15: Lithographic emulsion
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A silver halide photographic light-sensitive material and a developing process used in connection with that material are disclosed. The material is comprised of a support having thereon a silver halide emulsion layer containing a silver halide emulsion in which at least 80 mole % of the whole silver halide is composed of silver chloride, the mean grain size thereof is less than 0.4 .mu.m, and which contains more than 1.times.10.sup.-6 mole of a water-soluble rhodium salt per mole of silver at an optional period before finishing the first ripening in the production step for the silver halide emulsion. The material also contains 1.times.10.sup.-5 to 1.times.10.sup.-2 mole of polyalkylene oxide having a molecular weight of at least 600 or a derivative thereof per mole of silver. The process involves imagewise exposing the material and processing it in a developer containing 0.05 to 0.5 mole/liter of a dihydroxybenzene series developing agent, 0 to 0.05 g/liter of an auxiliary developing agent, at least 0.25 mole/liter of a free sulfite ion, at least 20 mg/liter of 5- or 6-nitroindazole, and an alkali of an amount sufficient for keeping the pH of the developer higher than 10.5. The material and processing are capable of providing good letter image quality in a short developing time.

## Claims

### Claim 1

A silver halide photographic light-sensitive material comprising a support having thereon a silver halide emulsion layer containing a silver halide emulsion in which at least 80 mole% of the whole silver halide is composed of silver chloride, the mean grain size thereof is less than 0.4 .mu.m, and which contains more than 1.times.10.sup.-6 mole of a water-soluble rhodium salt per mole of silver at an optional period before finishing the first ripening in the production step for the silver halide emulsion, said silver halide photographic light-sensitive material further containing 1.times.10.sup.-5 to 1.times.10.sup.-2 mole of polyalkylene oxide having a molecular weight of at least 600 or a derivative thereof per mole of silver.

### Claim 2 (depends on 1)

A silver halide photographic light-sensitive material as claimed in claim 1, wherein the polyalkylene oxide is present within the silver halide emulsion layer.

### Claim 3 (depends on 1)

A silver halide photographic light-sensitive material as claimed in claim 1, further comprising a hydropholic colloid layer which contains the polyalkylene oxide.

### Claim 4 (depends on 1)

A silver halide photographic light-sensitive material as claimed in claim 1, further comprising an additional compound selected from the group consisting of a benzotriazole compound and a mercapto compound.

### Claim 5

A developing process, comprising the steps of:
providing a silver halide photographic light-sensitive material comprised of a support having thereon a silver halide emulsion layer containing a silver halide emulsion in which at least 80 mole% of the whole silver halide is composed of silver chloride, the mean grain size thereof is less than 0.4 .mu.m, and which contains more than 1.times.10.sup.-6 mole of a water-soluble rhodium salt per mole of silver at an optional period before finishing the first ripening step in the production step of the silver halide emulsion, said silver halide photographic light-sensitive material further containing 1.times.10.sup.-5 to 1.times.10.sup.-2 mole of polyalkylene oxide having a molecular weight of at least 600 or a derivative thereof per mole of silver;
imagewise exposing the photographic material: and
processing the exposed material with a developer containing 0.05 to 0.5 mole/liter of a dihydroxybenzene series developing agent, 0 to 0.05 g/liter of an auxiliary developing agent, at least 0.25 mole/liter of a free sulfite ion, at least 20 mg/liter of 5- or 6-nitroindazole, and an alkali of an amounts sufficient for keeping the pH of the developer above 10.5.

### Claim 6 (depends on 5)

A developing process as claimed in claim 5, wherein the dihydroxybenzene series developing agent is present in an amount within the range of 0.1 to 0.4 mole/liter.

### Claim 7 (depends on 5)

A developing process as claimed in claim 5, wherein the pH of the developer is adjusted to a level ranging from higher than 10.5 up to 12.5.

### Claim 8 (depends on 7)

A developing process as claimed in claim 7, wherein the pH of the developer is adjusted to a level ranging from higher than 11.5 up to 12.5.

### Claim 9 (depends on 5)

A developing process as claimed in claim 5, wherein the developer contains solely a dihydroxybenzene containing no auxiliary developing agent.

### Claim 10 (depends on 9)

A developing process as claimed in claim 9, wherein the dihydroxybenzene is hydroquinone.