# US 4,444,871 A · Method for forming a direct positive color image

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,444,871 A
- Document ID: US4444871A
- Status: Granted
- Kind: A
- Application number: 06/429,157
- Filed: 1982-09-30
- Granted: 1984-04-24
- Earliest claimed: 1981-10-08
- Assignees: Konishiroku Photo Industry Co., Ltd.
- Inventors: Kazuyoshi Miyaoka; Shigeharu Koboshi
- Web page: https://patentgrep.com/patent/US4444871A

## CPC

- G03C 5/50: Reversal development; Contact processes (G03C5/315, G03C8/00 take precedence)
- Y10S 430/141: Direct positive material
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

Method for forming a direct positive-color image in which an imagewise exposure is applied to a direct positive silver halide color photosensitive material comprising a support and at least one light-sensitive silver halide emulsion layer which contain internal latent image type silver halide grains whose surfaces are not fogged, said method including applying a fogging exposure and color development wherein said fogging exposure is applied in a wet condition with a solution containing at least one fluorescent whitening agent.

## Claims

### Claim 1

A method for forming a direct positive color image in which an imagewise exposure is applied to a direct positive silver halide color photosensitive material comprising a support and at least one light-sensitive silver halide emulsion layer selected from the group consisting of a blue-sensitive, a green-sensitive and a red-sensitive silver halide emulsion layers containing respectively internal latent image type silver halide grains whose surfaces are not fogged and a fogging exposure is then applied and further a color development is made, wherein said fogging exposure is applied in a wet condition with a solution containing a fluorescent whitening agent.

### Claim 2 (depends on 1)

A method according to claim 1, wherein said fluorescent whitening agent is one selected from the group consisting of stilbene compounds, coumalin compounds, biphenyl-compounds, azole compounds, naphthalimide compounds and pyrazoline compounds.

### Claim 3 (depends on 2)

A method according to claim 2, wherein said stilbene compounds are represented by the Formula: ##STR11## Wherein Y.sub.1 and Y.sub.2 represent respectively ##STR12## group in which R.sub.1, R.sub.2 and R.sub.3 represent respectively a hydroxyl group, a halogen atom, a morpholino group, an alkoxy group, an aryloxy group, an alkyl group, an aryl group, an amino group, an alkylamino group, an arylamino group.

### Claim 4 (depends on 1)

A method according to claim 1, wherein said fogging exposure is applied by exposing the entire surface of said photosensitive material.

### Claim 5 (depends on 1)

A method according to claim 1, wherein said light-sensitive silver halide emulsion layer would give the density of 0.6 when the density of silver of said emulsion layer is 35 mg Ag/dm.sup.2 and said emulsion layer provided on said support is developed without any exposure to light, with the surface developing liquid A mentioned below at 20.degree. C. for ten minutes:
______________________________________ Surface Developing Liquid A: ______________________________________ Metol (p-methylamino- 2.5 g phenol sulfate) l-ascorbic acid 10 g NaBO.sub.2.4H.sub.2 O 35 g KBr 1 g Add water to make 1 ltr. ______________________________________

### Claim 6 (depends on 1)

A method according to claim 1, wherein said light-sensitive silver halide emulsion layer would give a maximum density which is at least 5 times, when exposed for a given time up to 1 second and then developed at 20.degree. C. for 4 minutes with an internal developing liquid B mentioned below, as dense as that obtained when exposed to light under the same condition and is then developed with a surface developing liquid A:
______________________________________ Surface Developing Liquid A: Metol (p-methylamino- 2.5 g phenol sulfate) l-ascorbic acid 10 g NaBO.sub.2.4H.sub.2 O 35 g KBr 1 g Add water to make 1 ltr. Internal Developing Liquid B: Metol 2 g Sodium sulfite, anhydrous 90 g Hydroquinone 8 g Sodium carbonate, monohydrate 52.5 g KBr 5 g KI 0.5 g Add water to make 1 ltr. ______________________________________