Back to results
US 4,442,072 AGranted
Selective recovery of base metals and precious metals from ores
AssigneeThe United States of America as represented by the Secretary of the Interior
InventorsElizabeth G. Baglin, John M. Gomes
Life of this patent
Estimating the term…
Abstract
Metal values are recovered from ore concentrates by forming a sulfide matte, grindng the matte, leaching with sulfuric acid at elevated temperature to selectively extract nickel and iron, and roasting and leaching the residue with dilute sulfuric acid to selectively extract copper. The residue contains a high concentration of platinum, palladium and gold.
Claims3
A process for recovery of nickel, iron, copper, platinum, palladium and gold values from ore concentrates consisting essentially of:
- (a) smelting the concentrate with a flux to form a matte and slag,
- (b) grinding the matte to a particle size suitable for leaching,
- (c) leaching, in a first-stage, the ground matte with sulfuric acid of a concentration of about 10 to 40 wt-pct at a temperature of about 40.degree. to 100.degree. C. and atmospheric pressure to selectively extract nickel and iron values, and
- (d) roasting and leaching, in a second-stage, the residue from the first-stage leach, the roasting being at a temperature of about 300.degree. to 500.degree. C., and the leaching being with dilute sulfuric acid at ambient temperature and pressure, to selectively extract copper values and provide a residue containing a high concentration of platinum, palladium and gold.
1 more element