# US 4,434,226 A · High aspect ratio silver bromoiodide emulsions and processes for their preparation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,434,226 A
- Document ID: US4434226A
- Status: Granted
- Kind: A
- Application number: 06/429,420
- Filed: 1982-09-30
- Granted: 1984-02-28
- Earliest claimed: 1981-12-12
- Assignees: Eastman Kodak Company
- Inventors: Herbert S. Wilgus; John A. Haefner
- Web page: https://patentgrep.com/patent/US4434226A

## CPC

- G03C 1/0051: {Tabular grain emulsions}
- G03C 1/09: Noble metals or mercury; Salts or compounds thereof; Sulfur, selenium or tellurium, or compounds thereof, e.g. for chemical sensitising (G03C1/34, G03C1/35 take precedence)
- G03C 7/3022: {Materials with specific emulsion characteristics, e.g. thickness of the layers, silver content, shape of AgX grains}
- G03C 2001/0055: {Aspect ratio of tabular grains in general; High aspect ratio; Intermediate aspect ratio; Low aspect ratio}
- G03C 2001/0156: {pAg value; pBr value; pCl value; pI value}
- G03C 2001/03511: {Bromide content}
- G03C 2001/03558: {Iodide content}
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)

## Abstract

A tabular grain silver halide emulsion is disclosed comprised of a dispersing medium and silver bromoiodide grains. Tabular silver bromoiodide grains having a thickness less than 0.3 micron and a diameter of at least 0.6 micron have an average aspect ratio of greater than 8:1 and account for at least 50 percent of the total projected area of the silver bromoiodide grains. The high aspect ratio silver bromoiodide grains are prepared by concurrently running silver, bromide, and iodide salts into a reaction vessel while controlling pBr. Prior to the concurrent addition of silver and iodide salts the reaction vessel is substantially free of iodide.

## Claims

### Claim 1

A high aspect ratio tabular grain silver halide emulsion comprised of a dispersing medium and silver bromoiodide grains, wherein tabular silver bromoiodide grains having a thickness of less than 0.3 micron and a diameter of at least 0.6 micron have an average aspect ratio of greater than 8:1 and account for at least 50 percent of the total projected area of said silver bromoiodide grains.

### Claim 2 (depends on 1)

A silver halide emulsion according to claim 1 wherein the average aspect ratio is at least 12:1.

### Claim 3 (depends on 1)

A silver halide emulsion according to claim 1 wherein the average aspect ratio is at least 20:1.

### Claim 4 (depends on 1)

A silver halide emulsion according to claim 1 wherein the dispersing medium is a peptizer.

### Claim 5 (depends on 1)

A silver halide emulsion according to claim 1 wherein the peptizer is gelatin or a gelatin derivative.

### Claim 6 (depends on 2)

A silver halide emulsion according to claim 2 wherein the tabular silver halide grains account for at least 70 percent of the totaal projected area of said silver halide grains.

### Claim 7 (depends on 6)

A silver halide emulsion according to claim 6 wherein the tabular silver halide grains account for at least 90 percent of the total projected area of said silver halide grains.

### Claim 8 (depends on 1)

A silver halide emulsion according to claim 1 wherein iodide is present in said silver bromoiodide grains in a concentration of from 0.05 to 40 mole percent.

### Claim 9 (depends on 8)

A silver halide emulsion according to claim 8 wherein iodide is present in said silver bromoiodide grains in a concentration of from 0.1 to 20 mole percent.

### Claim 10

A high aspect ratio tabular grain silver halide emulsion comprised of gelatin or a gelatin derivative peptizer and silver bromoiodide grains comprised of from 0.1 to 20 mole percent iodide, wherein tabular silver bromoiodide grains having a thickness of less than 0.3 micron and a diameter of at least 0.6 micron have an average aspect ratio of at least 12:1 and account for at least 70 percent of the the total projected area of said silver bromoiodide grains.

### Claim 11

A high aspect ratio tabular grain silver halide emulsion comprised of gelatin or a gelatin derivative peptizer and silver bromoiodide grains comprised of up to 15 mole percent iodide, wherein said silver bromoiodide grains having a thickness of less than 0.3 micron and a diameter of at least 0.6 micron have an average aspect ratio in the range of from 20:1 to 50:1 and account for at least 90 percent of the total projected area of said silver bromoiodide grains.

### Claim 12 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

In a photographic element comprised of a support and at least one radiation-sensitive emulsion layer, the improvement wherein said emulsion layer is comprised of an emulsion according to claim 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, or 11.

### Claim 13 (depends on 12)

A process of producing a visible photographic image comprising processing in an aqueous alkaline solution in the presence of a developing agent an imagewise exposed photographic element according to claim 12.

### Claim 14

In a process of preparing a radiation-sensitive silver bromoiodide emulsion comprised of a dispersing medium and silver bromoiodide grains by introducing silver, bromide, and iodide salts into a reaction vessel containing at least a portion of the dispersing medium,
the improvement comprising
adjusting the pBr of the dispersing medium within the reaction vessel prior to introduction of the iodide salt to a level of from 1.1 to 1.6,
maintaining the reaction vessel substantially free of iodide prior to introduction of the silver and bromide salts, and
maintaining the pBr within the reaction vessel at a level of at least 0.6 during introduction of the iodide salt,
thereby producing within the dispersing medium contained within the reaction vessel silver bromoiodide grains, said silver bromoiodide grains having a thickness of less than 0.3 micron and a diameter of at least 0.6 micron exhibiting an average aspect ratio of greater than 8:1 and account for at least 50 percent of the total projected area of said silver bromoiodide grains.

### Claim 15 (depends on 14)

In an improved process according to claim 14, introducing a peptizer into the reaction vessel so that it is present during introduction of the silver, bromide, and iodide salts.

### Claim 16 (depends on 14)

In an improved process according to claim 14, maintaining the contents of the reaction vessel in the range of from 30.degree. to 90.degree. C. while concurrently introducing the silver, bromide, and iodide salts.

### Claim 17 (depends on 16)

In an improved process according to claim 16, maintaining the contents of the reaction vessel in the range of from 40.degree. to 80.degree. C. during the concurrent introduction of silver, bromide, and iodide salts.

### Claim 18 (depends on 14)

In an improved process according to claim 14, adjusting the pBr of the dispersing medium within the reaction vessel prior to introduction of the silver and iodide salts to a level of from 1.1 to 1.5

### Claim 19 (depends on 14)

In an improved process according to claim 14, maintaining the pBr within the reaction vessel in the range of from 0.8 to 1.6 during concurrent introduction of silver and iodide salts.

### Claim 20 (depends on 14)

In an improved process according to claim 14, maintaining the pBr within the reaction vessel in the range of 0.6 to 2.2 while introducing the iodide salt.

### Claim 21 (depends on 14)

In an improved process according to claim 14, introducing the silver salt and at least one of the bromide and iodide salts in the form of silver halide grains having an average diameter of less than 0.1 micron.

### Claim 22 (depends on 14)

In an improved process according to claim 14, maintaining the concentration of iodide within the reaction vessel below 0.5 mole percent of the total halide concentration in the reaction vessel prior to concurrent introduction of the silver and halide salts.