# US 4,416,170 A · Method of producing a steel caul

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,416,170 A
- Document ID: US4416170A
- Status: Granted
- Kind: A
- Application number: 06/479,106
- Filed: 1983-03-28
- Granted: 1983-11-22
- Earliest claimed: 1980-10-29
- Assignees: Champion International Corporation
- Inventors: Donald B. Gibson; Gerald F. Laughinghouse
- Web page: https://patentgrep.com/patent/US4416170A

## CPC

- B27N 3/16: Transporting the material from mat moulding stations to presses (B27N3/22 takes precedence); Apparatus specially adapted for transporting the material or component parts therefor, e.g. cauls (transport devices in general B65G)
- B23P 15/24: dies (B21C3/18, B21C25/10, B21D37/20 take precedence)
- Y10T 156/1039: Surface deformation only of sandwich or lamina [e.g., embossed panels]
- Y10T 428/12993: Surface feature [e.g., rough, mirror]
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)
- B23P: METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS (arrangements for copying or controlling B23Q)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A steel caul for forming wood panels is sandblasted to roughen the contact face thereof. The process of roughening the face results in a multiplicity of minute indentations in the surface of the face which function to capture and retain therein carbonized materials which are produced when the caul is employed to press panel products, thereby extending the period which the caul can be used without the need for cleaning carbon deposits from the same.

## Claims

### Claim 1

A process for forming a steel caul to use in forming panel surfaces on panels made of reconstituted wood by pressing said cauls against said reconstituted wood at temperatures of up to about 475.degree. F., said process comprising the steps of:
a. selecting one face of said caul to form said panel surfaces,
b. forming a decorative pattern on said selected face, said decorative pattern being adapted to be pressed against the reconstituted wood panels to form the panel surfaces on said panels, and
c. thereafter, roughening the decorative pattern formed on the selected face of said steel caul by sand blasting said face with number 12-35 sand thereby forming a multiplicity of indentations in said decorative pattern on said selected face said indentations being large enough to capture and retain the carbon materials produced by the use of said caul in forming said panel surfaces, but not being so large as to have a visibly noticeable detrimental effect on the said decorative pattern in said selected face.

### Claim 2 (depends on 1)

A process as in claim 1 further comprising the step of smoothing said one face prior to roughening.

### Claim 3 (depends on 1)

A process as in claim 1 further comprising the step of embossing said face with a decorative design prior to roughening.

### Claim 4 (depends on 1)

A method as in claim 1 further including the step of forming said indentations in a random orientation.