# US 4,414,304 A · Forehardened high aspect ratio silver halide photographic elements and processes for their use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,414,304 A
- Document ID: US4414304A
- Status: Granted
- Kind: A
- Application number: 06/430,574
- Filed: 1982-09-30
- Granted: 1983-11-08
- Earliest claimed: 1981-11-12
- Assignees: Eastman Kodak Company
- Inventors: Robert E. Dickerson
- Web page: https://patentgrep.com/patent/US4414304A

## CPC

- G03C 5/16: X-ray, infrared, or ultraviolet ray processes
- G03C 1/0051: {Tabular grain emulsions}
- G03C 1/30: Hardeners
- Y10S 430/167: X-ray
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

Forehardened photographic elements, particularly radiographic elements, intended to produce silver images are disclosed including among hydrophilic colloid layers at least one emulsion layer containing thin tabular silver halide grains. When developed in less than 1 minute to produce a viewable silver image, these photographic elements exhibit increased covering power.

## Claims

### Claim 1

In a radiographic element comprised of
a support and, located on the support,
one or more hydrophilic colloid layers including at least one emulsion layer containing radiation-sensitive silver halide grains,
the improvement wherein
at least 50 percent of the total projected area of said silver halide grains in at least said one emulsion layer is provided by thin tabular grains having an average aspect ratio of greater than 8:1 and a thickness of 0.2 micron or less and
said hydrophilic colloid layers are forehardened in an amount sufficient to reduce swelling of said layers to less than 200 percent, percent swelling being determined by (a) incubating said photographic element at 38.degree. C. for 3 days at 50 percent relative humidity, (b) measuring layer thickness, (c) immersing said photographic element in distilled water at 21.degree. C. for 3 minutes, and (d) determining the precent change in layer thickness as compared to the layer thickness measured in step (b).

### Claim 2 (depends on 1)

An improved radiographic element according to claim 1 wherein said silver halide grains have an average diameter of at least 0.6 micron.

### Claim 3 (depends on 2)

An improved radiographic element according to claim 2 wherein said silver halide grains have an average diameter of at least 1.0 micron.

### Claim 4 (depends on 1)

An improved radiographic element according to claim 1 wherein said silver halide is a silver bromide or silver bromoiodide.

### Claim 5 (depends on 1)

An improved radiographic element according to claim 1 wherein said hydrophilic colloid layers contain gelatin or a hardenable gelatin derivative.

### Claim 6 (depends on 1)

An improved radiographic element according to claim 1 wherein said hydrophilic colloid layers are forehardened with an aldehyde type hardener.

### Claim 7 (depends on 1)

An improved radiographic element according to claim 1 wherein said hydrophilic colloid layers are forehardened with an active olefin type hardener containing two or more active olefin bonding sites.

### Claim 8 (depends on 1)

An improved radiographic element according to claim 1 wherein said hydrophilic colloid layers are forehardened with a halogen-substituted aldehyde acid type hardener.

### Claim 9 (depends on 1)

An improved radiographic element according to claim 1 wherein said hydrophilic colloid layers are forehardened in an amount sufficient to reduce swelling of said layers to less than 100 percent.

### Claim 10 (depends on 1)

An improved radiographic element according to claim 1 wherein said photographic element exhibits a covering power of at least 80 when developed in less than 1 minute.

### Claim 11 (depends on 1)

An improved radiographic element according to claim 1 wherein said tabular silver halide grains account for at least 70 percent of the total projected area of said silver halide grains.

### Claim 12

In a radiographic element comprised of a substantially specularly transmissive support having first and second major surfaces and, located on each of said major surfaces,
one or more hydrophilic colloid layers including at least one emulsion layer containing radiation-sensitive silver bromide grains containing up to 6 mole percent iodide,
the improvement wherein
at least 50 percent of the total projected area of said silver bromide grains in at least one emulsion layer is provided by thin tabular silver bromide grains optionally containing iodide having a thickness of less than 0.2 micron and an average aspect ratio in the range of at least 12:1 and
said hydrophilic colloid layers being forehardened in an amount sufficient to reduce swelling of said layers to less than 200 percent, percent swelling being determined by (a) incubating said photographic element at 38.degree. C. for 3 days at 50 percent relative humidity, (b) measuring layer thickness, (c) immersing said photographic element in distilled water at 21.degree. C. for 3 minutes, and (d) determining the percent change in layer thickness as compared to the layer thickness measured in step (b).

### Claim 13 (depends on 12)

An improved radiographic element according to claim 12 wherein said silver halide grains have an average diameter of at least 0.6 micron.

### Claim 14 (depends on 13)

An improved radiographic element according to claim 13 wherein said tabular silver halide grains have an average diameter of at least 1.0 micron.

### Claim 15 (depends on 12)

An improved radiographic element according to claim 12 wherein said hydrophilic colloid layers consist essentially of a gelatin or a hardenable gelatin derivative vehicle.

### Claim 16 (depends on 15)

An improved radiographic element according to claim 15 wherein said hydrophilic colloid layers are forehardened with a hardener chosen from the group consisting of an aldehyde type hardener, a hardener having two or more vinylsulfonyl or vinylsulfonyl precursor groups, and a mucochloric acid hardener.

### Claim 17 (depends on 12)

An improved radiographic element according to claim 12 wherein said thin tabular grains have an average aspect ratio of at least 25:1 and a thickness of 0.10 micron or less.

### Claim 18 (depends on 12)

An improved radiographic element according to claim 12 wherein said hydrophilic colloid layers forehardened in an amount sufficient to reduce swell of said layers to less than 100 percent.

### Claim 19 (depends on 18)

An improved radiographic element according to claim 18 wherein said radiographic element exhibits a covering power of at least 100.

### Claim 20 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

A process of producing a high covering power silver image comprising
imagewise exposing a radiographic element according to any one of claims 1 through 11 and
developing a viewable silver image in less than 1 minute.

### Claim 21 (depends on 20)

A process according to claim 20 wherein a hydroquinone developing agent is employed.

### Claim 22 (depends on 12, 13, 14, 15, 16, 17, 18, 19)

A process of producing a high covering power silver image comprising
imagewise exposing a radiographic element according to any one of claims 12 through 19 and
developing a viewable silver image in less than 1 minute.

### Claim 23 (depends on 22)

A process according to claim 22 wherein a hydroquinone developing agent is employed.

### Claim 24 (depends on 22)

A process according to claim 22 wherein processing is undertaken at a temperature in the range of from 25.degree. to 50.degree. C.