The object of the invention is to provide a process for the recovery of iron and nickel from low iron content laterite ores. Said process comprises subjecting the ore to a carburizing step in the presence of a reducing agent and carbon supplying agent to convert the iron to iron carbide, followed by smelting the residue or product of the carburizing step to produce a ferronickel product. An alternative embodiment is the recovery of the iron and nickel from the product of the carburizing step by magnetic separation.
Claims6
A process for recovering a metal which has a melting point in excess of about 750.degree. C, and is capable of alloying with iron, in the form of an iron alloy from a material containing iron and said metal, said process comprising:
- (a) contacting said material with iron carbide, at least some of said iron carbide being formed by converting at least some of said iron in the material containing iron to iron carbide in a fluidized bed in the presence of a carbon-supplying material and a reducing agent, and
- (b) smelting the product of step (a) to produce the alloy of said metal with iron
A process for producing an alloy of iron and another metal, said other metal having a melting point in excess of about 750.degree. C. and being capable of alloying with iron, from an ore containing iron and said other metal, comprising:
- (a) contacting said ore with iron carbide, at least sone of said iron carbidge being formed by converting at least some of said iron in said ore to iron carbide in a fluidized bed in the presence of a carbon-supplying material and a reducing agent, and
- (b) smelting the product of step (a) to produce the alloy of said metal with iron.