## CPC

- H10W 70/048: {Mechanical treatments, e.g. punching, cutting, deforming or cold welding}
- H10W 70/688: {Flexible insulating substrates}
- H05K 3/4007: {Surface contacts, e.g. bumps (H05K3/4092 takes precedence; deposition of finish layers on pads H05K3/24; forming solder bumps H05K3/3465)}
- H05K 3/4092: {Integral conductive tabs, i.e. conductive parts partly detached from the substrate}
- Y10T 29/49121: Beam lead frame or beam lead device
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Mechanically punching bumps in a thin copper or aluminum foil and etching the foil to form beams with a bump at the end of each beam. Alternatively increasing the layers by casting or gluing polyimide film to the foil and etching the polyimide film in designated areas to expose the copper or aluminum.

## Claims

### Claim 1

In a method for making a bumped-beam tape for tape bonding semiconductor chips to lead frames, ceramic chip carriers or hybrid substrates, the method employing a pilot punch to engage multiple registration holes on each edge of a substrate containing at least in part a thin copper or aluminum foil, the improvement comprising (a) forming the bumps on the copper or aluminum foil by positioning the foil with the pilot punch in a forming die having a predetermined array of male punch members and causing the punch members to strike the foil with sufficient force to produce deformations in the foil, (b) selectively etching beams in the foil either before or after forming the bumps, and (c) bonding the bumps to a semiconductor chip.

### Claim 2

In a method for making a bumped-beam tape for tape bonding semiconductor chips to lead frames, ceramic chip carriers or hybrid substrates, the method employing a pilot punch to engage multiple registration holes on each edge of a substrate containing at least in part a thin copper or aluminum foil, the improvement comprising (a) positioning the foil with the pilot punch in a forming die having a predetermined array of male punch members, causing the punch members to strike the foil producing corresponding deformations in the foil, (b) thereafter selectively etching beams in the foil with one of the deformations at the end of each beam and (c) bonding the deformation to a semiconductor chip.

### Claim 3

In a method for making a bumped-beam tape for tape bonding semiconductor chips to lead frames, ceramic chip carriers or hybrid substrates, the method employing a pilot punch to engage multiple registration holes on each edge of a substrate containing at least in part a thin copper or aluminum foil, the improvement comprising (a) selectively etching multiple beams in the foil, (b) thereafter positioning the etched foil with the pilot punch in a forming die having a predetermined array of male punch members and causing the punch members to strike the foil producing corresponding deformations in the foil at the ends of each beam and (c) bonding the deformations to a semiconductor chip.

### Claim 4 (depends on 2, 3)

The method according to claims 2 or 3 wherein the foil is adhesively bonded to a polyester or polyimide film to form the substrate and the film is etched to provide registration holes and a personality hole.

### Claim 5 (depends on 2, 3)

The method according to claims 2 or 3 wherein the foil is adhesively bonded to a polyester, polyimide or epoxy-glass film to form the substrate and the film is prepunched to provide registration holes and a personality hole.

### Claim 6 (depends on 2, 3)

The method according to claims 2 or 3 wherein a liquid polyimide is cast onto the copper or aluminum foil to form the substrate and the polyimide is etched to provide registration holes and a personality hole.

### Claim 7 (depends on 2, 3)

The method according to claims 2 or 3 wherein copper is plated onto a polyimide, polyester or epoxy-glass film having prepunched registration holes to form the substrate.

### Claim 8 (depends on 2, 3)

The method according to claims 2 or 3 wherein copper is plated onto a polyimide or polyester film to form the substrate and the film is etched to form registration holes and a personality hole.

### Claim 9 (depends on 2, 3)

The method according to claims 2 or 3 wherein the deformations are plated with a nobel metal.

### Claim 10 (depends on 2, 3)

The method according to claims 2 or 3 wherein the foil is plated with a nobel metal.

### Claim 11 (depends on 2, 3)

The method according to claims 2 or 3 wherein the deformations are plated with gold.

### Claim 12 (depends on 2, 3)

The method according to claims 2 or 3 wherein the foil is plated with gold.

### Claim 13 (depends on 2, 3)

The method according to claims 2 or 3 wherein the foil is copper.

### Claim 14 (depends on 2, 3)

The method according to claims 2 or 3 wherein the foil is aluminum.