# US 4,395,563 A · Hydrolysis of alkoxysilanes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,395,563 A
- Document ID: US4395563A
- Status: Granted
- Kind: A
- Application number: 06/316,241
- Filed: 1981-10-29
- Granted: 1983-07-26
- Earliest claimed: 1981-10-29
- Assignees: General Electric Company
- Inventors: Susan E. Hayes
- Web page: https://patentgrep.com/patent/US4395563A

## CPC

- C07F 7/0874: {Reactions involving a bond of the Si-O-Si linkage}
- C07F 7/0836: {Compounds with one or more Si-OH or Si-O-metal linkage}
- C08G 77/045: {containing less than 25 silicon atoms}
- C07F: ACYCLIC, CARBOCYCLIC OR HETEROCYCLIC COMPOUNDS CONTAINING ELEMENTS OTHER THAN CARBON, HYDROGEN, HALOGEN, OXYGEN, NITROGEN, SULFUR, SELENIUM OR TELLURIUM (metal-containing porphyrins C07D487/22)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Alkoxysilanes are hydrolyzed with water in the presence of various hydrolysis catalysts. The hydrolysis catalysts include the solid oxides of the Group IIa metals and solid acid catalysts. The solid acid catalysts are used in conjunction with neutralizing agents and optionally with condensation catalysts. Generally, the process for hydrolyzing alkoxysilanes comprises: mixing an alkoxysilane, a stoichiometric excess of water and an effective catalytic amount of hydrolysis catalyst selected from the group consisting of a solid oxide of a Group IIa metal, a solid acid catalyst and mixtures thereof; neutralizing the hydrolysis mixture with a sufficient amount of neutralizing agent, for example, magnesium oxide; and separating the hydrolysis product from the mixture. When a Group IIa metal oxide hydrolysis catalyst is used, the liquid portion of the hydrolysate is neutral, and no additional neutralizing agent is required in the mixture. By the process of the present invention, the average chain length of silanol-stopped polysiloxanes can be controlled. A stabilized, crystalline tetramethyldisiloxane diol and a crystalline dimethyldisilanol have also been prepared by modified catalytic hydrolysis processes using solid acid catalysts to catalyze the hydrolysis of dimethyldimethoxysilane with water.

## Claims

### Claim 1

A process for hydrolyzing alkoxysilanes comprising:
(a) mixing an alkoxysilane having the general formula:
(R'O).sub.a Si R.sub.4-a
wherein R is selected from the group consisting of alkyl, cycloalkyl, aryl, arylalkyl, haloalkyl, alkaryl, alkenyl, hydrogen and mixtures thereof; R' is alkyl; and a is an integer from 1 to 4; a stoichiometric excess of water and an effective catalytic amount of solid hydrolysis catalyst selected from the group consisting of a solid oxide of a Group IIa metal and solid acid catalyst to form a hydrolysis mixture of hydrolyzed product, reaction byproducts, hydrolysis catalyst and unreacted water;
(b) separating volatile by-products and unreacted reagents from the hydrolyzed product in the presence of the solid hydrolysis catalyst to form a devolatilized hydrolysis mixture, said separation being one which reduces the alkoxy content of the alkoxysilane;
(c) neutralizing the devolatilized hydrolysis mixture with a sufficient amount of neutralizing agent when the catalyst is a solid acid catalyst and optionally adding a suitable amount of condensation catalyst to increase the molecular weight of the hydrolysis product; and
(d) separating the hydrolysis catalyst from the product.

### Claim 2 (depends on 1)

The process of claim 1 wherein the solid acid catalyst is an acid activated clay and wherein the neutralizing agent is selected from the group consisting of magnesium oxide, calcium oxide and mixtures thereof.

### Claim 3 (depends on 1)

The process of claim 1 wherein the neutralizing/condensation agent is the oxide of the Group IIa metal, and the hydrolysis mixture is hydrolyzed and condensed simultaneously with mixing the dialkoxysilane, water and solid oxide of a Group IIa metal to form a neutral hydrolysis mixture.

### Claim 4 (depends on 1, 3)

The process of claims 1 or 3 further comprising adding a filter aid to the hydrolysis mixture or neutral hydrolysis mixture and filtering the hydrolysis mixture or neutral hydrolysis mixture to remove solids therefrom.

### Claim 5 (depends on 1, 3)

The process of claims 1 or 3 further comprising filtering the hydrolysis mixture or the neutralized hydrolysis mixture to remove solids therefrom.

### Claim 6 (depends on 1)

The process of claim 1 wherein the hydrolyzed product is separated from the hydrolysis mixture by stripping volatile reaction by-products and unreacted water from the hydrolysis mixture and thereafter filtering the solids from the stripped hydrolysis mixture.

### Claim 7 (depends on 1)

The process of claim 1 comprising distilling the hydrolysis mixture to devolatilize the hydrolysis mixture in the presence of unneutralized solid acid catalyst whereby alkoxy groups from the alkoxysilanes are removed by condensation.

### Claim 8 (depends on 1)

The process of claim 1 further comprising maintaining the mixture of dialkoxysilane, water and hydrolysis catalyst at a temperature of about -10.degree. C. to about 60.degree. C.

### Claim 9 (depends on 1)

The process of claim 1 wherein the alkoxysilanes are dialkoxysilanes having the general formula:
(R).sub.2 Si(OR').sub.2

### Claim 10

A process for the catalytic hydrolysis of dialkoxysilanes comprising:
(a) mixing a dialkoxysilane with a stoichiometric excess of water in the presence of an effective catalytic amount of a solid Group IIa metal oxide catalyst to form a silanol-stopped polysiloxane product; and
(b) separating volatile reaction by-products, unreacted water and solids from the silanol-stopped polysiloxane product.

### Claim 11 (depends on 10)

The process of claim 10 further comprising adding a filter aid to the silanol-stopped polysiloxane product and filtering the silanol-stopped polysiloxane product to separate the solids therefrom.

### Claim 12 (depends on 10)

The process of claim 10 wherein the dialkoxysilane has the general formula:
(R).sub.2 Si(OR').sub.2
wherein R is selected from the group consisting of alkyl, haloalkyl, cycloalkyl, aryl, alkenyl, aralkyl, alkaryl, hydrogen and mixtures thereof, and R' is alkyl.

### Claim 13 (depends on 12)

The process of claim 12 wherein the dialkoxysilane is dimethyldimethoxysilane.

### Claim 14 (depends on 10)

The process of claim 10 wherein at least 3 moles of water per mole of dialkoxysilane are vigorously mixed with the dialkoxysilane.

### Claim 15 (depends on 10)

The process of claim 10 wherein the dialkoxysilane, water and metal oxide catalyst are vigorously mixed at a temperature of about 0.degree. C. to about 60.degree. C.

### Claim 16 (depends on 10)

The process of claim 10 wherein the dialkoxysilane, water and metal oxide catalyst are vigorously mixed for about 10 minutes to about 24 hours.

### Claim 17 (depends on 10)

The process of claim 10 wherein the metal oxide catalyst is selected from the group consisting of magnesium oxide, calcium oxide and barium oxide.

### Claim 18 (depends on 10, 17)

The process of claims 10 or 17 wherein the metal oxide catalyst comprises about 0.01 to about 10 parts by weight of Group IIa metal oxide catalyst per 100 parts by weight of dialkoxysilane.

### Claim 19 (depends on 10, 17)

The process of claims 10 or 17 wherein the metal oxide catalyst comprises about 0.08 to about 1.5 parts by weight of Group IIa metal oxide catalyst per 100 parts by weight of dialkoxysilane.

### Claim 20 (depends on 10)

The process of claim 10 wherein the volatile reaction by-products and unreacted water are separated from the silanol-stopped polysiloxane product by distillation.

### Claim 21 (depends on 10)

The process of claim 10 wherein the volatile reaction by-products and unreacted water are separated from the polysiloxane product by distillation, and thereafter solids are separated from the silanol-stopped polysiloxane product by filtration.

### Claim 22 (depends on 10, 11, 21)

The process of claims 10, 11 or 21 further comprising subjecting the silanol-stopped polysiloxane product to reduced pressure at an elevated temperature.

### Claim 23 (depends on 10, 11, 21)

The process of claims 10, 11 or 21 further comprising subjecting the silanol-stopped polysiloxane product to reduced pressure to complete the removal of volatile components.

### Claim 24

A method for controlling the chain length of silanol-stopped polysiloxanes prepared by the catalytic hydrolysis of dialkoxysilanes comprising:
(a) mixing an effective catalytic amount of a Group IIa metal oxide catalyst selected from the class consisting of magnesium oxide, calcium oxide and barium oxide with a dialkoxysilane and a stoichiometric excess of water to form a silanol-stopped diorganopolysiloxane; and,
(b) separating volatile reaction by-products unreacted water and solids from the silanolstopped polysiloxane product, whereby the polymer chain length varies according to the specific metal oxide catalyst, the silanol-stopped polysiloxane having a shorter average chain length when magnesium oxide is used as catalyst, an intermediate average chain length when calcium oxide is used as catalyst and a longer average chain length when barium oxide is used as catalyst.

### Claim 25 (depends on 24)

The method of claim 24 wherein the solids are separated from the silanol-stopped polysiloxane product by filtration.

### Claim 26 (depends on 24)

The method of claim 24 further comprising adding a filter aid to the silanol-stopped polysiloxane product and filtering the silanol-stopped polysiloxane product to separate the solids therefrom.

### Claim 27 (depends on 24)

The method of claim 24 wherein the volatile reaction by-products and unreacted water are separated from the silanol-stopped polysiloxane product by distillation.

### Claim 28 (depends on 24)

The method of claim 24 wherein the volatile reaction by-products and unreacted water are separated from the polysiloxane product by distillation, and thereafter solids are separated from the silanol-stopped polysiloxane product by filtration.

### Claim 29 (depends on 24, 27, 28)

The method of claims 24, 27 or 28 further comprising subjecting the product to reduced pressure at an elevated temperature to complete the removal of volatile components.

### Claim 30 (depends on 24)

The method of claim 24 wherein the average chain length of the silanol-stopped polysiloxane product is about 2 to about 3 siloxane (--SiO--) units when magnesium oxide is used as catalyst.

### Claim 31 (depends on 24)

The method of claim 24 wherein the average chain length of the silanol-stopped polysiloxane is about 4 to about 6 siloxane (--SiO--) units when calcium oxide is used as catalyst.

### Claim 32 (depends on 24)

The method of claim 24 wherein the dialkoxysilane has the general formula:
(R).sub.2 Si(OR').sub.2
wherein R is selected from the group consisting of alkyl, cycloalkyl, aryl, alkenyl, aralkyl, alkaryl, hydrogen and mixtures thereof, and R' is alkyl.

### Claim 33 (depends on 24, 32)

The method of claims 24 and 32 wherein the dialkoxysilane is dimethyldimethoxysilane.

### Claim 34 (depends on 24)

The method of claim 24 wherein at least 3 moles of water per mole of dialkoxysilane are vigorously mixed with the dialkoxysilane.

### Claim 35 (depends on 24)

The method of claim 24 wherein the dialkoxysilane, water and metal oxide catalyst are vigorously mixed for about 10 minutes to about 24 hours.

### Claim 36 (depends on 24)

The method of claim 24 wherein the dialkoxysilane, water and metal oxide catalyst are vigorously mixed at a temperature of about 0.degree. C. to about 60.degree. C.

### Claim 37 (depends on 24)

The method of claim 24 wherein the catalyst comprises about 0.01 to about 10 parts by weight of the catalyst per 100 parts by weight of the dialkoxysilane.

### Claim 38

A method for controlling the chain length of silanol-stopped dialkylpolysiloxanes prepared by the catalytic hydrolysis of dialkyldialkoxysilanes comprising:
(a) mixing a Group IIa metal oxide catalyst selected from the class consisting of magnesium oxide, calcium oxide and barium oxide with a dialkyldialkoxysilane and from about 3 to about 6 moles of water per mole of dialkyldialkoxysilane of about 0.degree. C. to about 60.degree. C., the catalyst being used in an amount from about 0.01 to about 1.5 parts by weight of metal oxide catalyst per 100 parts by weight of dialkyldialkoxysilane;
(b) distilling the reaction mixture after vigorously mixing for about 10 minutes to about 24 hours to separate volatile components and water from the silanol-stopped dialkylpolysiloxane product; and
(c) adding a solid filtering medium to the silanol-stopped dialkylpolysiloxane product and filtering said product, whereby the polymer chain length varies according to the specific metal oxide catalyst, the silanol-stopped dialkylpolysiloxane having an average chain length of about 2 to about 3 siloxane (--SiO--) units when magnesium oxide is used as a catalyst, an average chain length of about 4 to about 6 siloxane (--SiO--) units when calcium oxide is used as catalyst, and a longer average chain length when barium oxide is used as catalyst.

### Claim 39

A process for the catalytic hydrolysis of dialkoxysilanes comprising:
(a) mixing an alkoxysilane with a stoichiometric excess of water in the presence of an effective catalytic amount of solid acid catalyst to initiate hydrolysis of the alkoxysilane and thereby form a mixture comprising partially hydrolyzed alkoxysilane, solid acid catalyst, water and reaction by-products;
(b) separating the volatile reaction byproducts and unreacted water from the partially hydrolyzed silane in the presence of the solid acid catalyst to condense alkoxy and silanol groups and thereby form silane diol having a low alkoxy concentration;
(c) neutralizing the silane diol with a suitable solid neutralizing agent thereby obtaining a neutralized, low molecular weight, linear, silanol-stopped polysiloxane and condensation by-products;
(d) optionally adding a solid condensation catalyst to the neutralized polysiloxane to increase the chain length of the polysiloxane; and
(e) separating the volatile by-products and solid catalyst from the low molecular weight, linear, silanol-stopped polysiloxane.

### Claim 40 (depends on 39)

The process of claim 39 further comprising adding a filter aid and filtering the low molecular weight, linear, silanol-stopped polysiloxane to remove the acid solid catalyst.

### Claim 41 (depends on 39)

The process of claim 39 further comprising filtering the low molecular weight, linear, silanol-stopped polysiloxane to separate the acid solid catalyst therefrom.

### Claim 42 (depends on 39)

The process of claim 39 wherein the alkoxysilane has the general formula:
(R).sub.2 Si(OR').sub.2
wherein R is selected from the group consisting of alkyl, haloalkyl, cycloalkyl, aryl alkenyl, aralkyl, alkaryl, hydrogen and mixtures thereof, and R' is alkyl.

### Claim 43 (depends on 42)

The process of claim 42 wherein the dialkoxysilane is dimethyldimethoxysilane.

### Claim 44 (depends on 39)

The process of claim 39 wherein at least 3 moles of water per mole of alkoxysilane are vigorously mixed with the alkoxysilane.

### Claim 45 (depends on 39)

The process of claim 39 further comprising cooling the water and the acid solid catalyst to a temperature below ambient temperature and adding the alkoxysilane to the cooled aqueous medium.

### Claim 46 (depends on 45)

The process of claim 45 further comprising vigorously mixing the alkoxysilane, acid solid catalyst and water while maintaining the temperature below ambient.

### Claim 47 (depends on 45, 46)

The process of claims 45 or 46 wherein the temperature is about -10.degree. C. to about 60.degree. C.

### Claim 48 (depends on 39, 45, 46)

The process of claims 39, 45 or 46 wherein the mixture of alkoxysilane, water and solid acid catalyst are vigorously mixed for a sufficient length of time to form a single phase.

### Claim 49 (depends on 39)

The process of claim 39 wherein the solid acid catalyst is an acid-activated clay.

### Claim 50 (depends on 39, 49)

The process of claims 39 or 49 wherein the solid acid catalyst is used in an amount of about 0.01 to about 20 parts by weight of catalyst per 100 parts by weight of alkoxysilane.

### Claim 51 (depends on 39, 49)

The process of claims 39 or 49 wherein the solid acid catalyst is used in an amount of about 0.5 to about 2.0 parts by weight of catalyst per 100 parts by weight of alkoxysilane.

### Claim 52 (depends on 39)

The process of claim 39 wherein the volatile reaction by-products and unreacted water are separated from the partially hydrolyzed silane in the presence of the acid solid catalyst by distillation at a pressure of about 55 mm Hg to about 760 mm Hg.

### Claim 53 (depends on 39, 40, 41, 52)

The process of claims 39, 40, 41 or 52 further comprising subjecting the silanol-stopped, low molecular weight, linear polysiloxane to reduced pressure at a temperature between about 10.degree. C. to about 60.degree. C. to complete the removal of volatile components.

### Claim 54 (depends on 39)

The process of claim 39 wherein the solid neutralizing agent is solid magnesium oxide, and the average chain length of the silanol-stopped, low molecular weight, linear polysiloxane is about 3 to about 4 siloxane (--SiO--) units.

### Claim 55 (depends on 39, 54)

The process of claims 39 or 54 wherein the amount of neutralizing agent is about 0.05 part by weight to about 6.0 parts by weight solid neutralizing agent per 1.0 part by weight of acid solid catalyst.

### Claim 56 (depends on 39)

The process of claim 39 wherein the solid condensation catalyst is solid calcium oxide, and the average chain length of the silanol-stopped low molecular weight, linear polysiloxane is about 5 to about 6 siloxane (--SiO--) units.

### Claim 57 (depends on 39, 56)

The process of claims 39 or 56 wherein the amount of solid condensation catalyst is 0.05 part by weight to about 6.0 parts by weight condensation catalyst per 1.0 part by weight of acid solid catalyst.

### Claim 58

A process for the catalytic hydrolysis of dialkyldialkoxysilanes comprising:
(a) adding a dialkyldialkoxysilane to a mixture of about 3 to about 6 moles of water per mole of dialkyldialkoxysilane and about 0.5 to about 2.0 parts by weight of acid activated clay catalyst per 100 parts by weight of dialkyldialkoxysilane at a temperature of about -10.degree. C. to about 25.degree. C.;
(b) mixing vigorously the mixture of step (a) at a temperature between about -10.degree. C. to about 50.degree. C. for the minimum time required to form a single phase to about 45 minutes to initiate hydrolysis of the dialkyldialkoxysilane and thereby form a mixture comprising partially hydrolyzed dialkylsilanes, acid solid catalyst, water and reaction by-products;
(c) distilling the mixture at a temperature between about 15.degree. C. and about 50.degree. C. and at reduced pressure no less than about 15 mm Hg. pressure in the presence of the unneutralized solid acid catalyst to separate the volatile reaction by-products and water from the partially hydrolyzed dialkylsilane and to condense alkoxy and silanol groups, thereby forming low molecular weight, linear dialkylsilane diol product having a low alkoxy concentration;
(d) adding about 0.05 to about 6.0 parts by weight solid magnesium oxide neutralizing agent and condensation catalyst per 1.0 part by weight of acid solid catalyst, and stirring for a sufficient time to evenly disperse the solid magnesium oxide, thereby obtaining a mixture containing neutralized, low molecular weight, linear, silanol-stopped dialkyl polysiloxane having an average chain length of about 3 to about 4 siloxane (--SiO--) units;
(e) optionally adding up to about 6.0 parts by weight solid calcium oxide condensation catalyst per 1.0 part by weight of acid solid catalyst and stirring for a sufficient time to evenly disperse the solid calcium oxide in the mixture, thereby obtaining a mixture containing condensed, low molecular weight, linear, silanol-stopped dialkylpolysiloxane having an average chain length of about 5 to about 6 siloxane (--SiO--) units;
(f) distilling the mixture containing low molecular weight, linear, silanol-stopped dialkylpolysiloxane until all volatile materials are removed; and
(g) filtering the mixture remaining after removal of volatile materials to remove solid catalysts to obtain low molecular weight, linear, silanol-stopped dialkylpolysiloxane product.

### Claim 59 (depends on 58)

The process of claim 58 wherein the dialkyldialkoxysilane is dimethyldimethoxysilane, and the product is dimethylpolysiloxanediol.

### Claim 60 (depends on 58)

The process of claim 58 further comprising adding a filter aid to the mixture remaining after removal of the volatile materials to aid in the removal of the solid catalysts and to adjust the pH of the mixture.

### Claim 61

A method for controlling the chain length of low molecular weight, linear, silanol-stopped polysiloxanes prepared by the catalytic hydrolysis of dialkoxysilanes comprising:
(a) mixing a dialkoxysilane with a stoichiometric excess of water in the presence of an effective catalytic amount of solid acid catalyst to initiate hydrolysis of the dialkoxysilane and thereby form a mixture comprising partially hydrolyzed alkoxysilane, acid solid catalyst, water and reaction by-products;
(b) separating the volatile reaction by-products and water from the partially hydrolyzed silane in the presence of the solid acid catalyst to condense alkoxy and silanol groups and thereby form silane diol having a low alkoxy concentration;
(c) adding an effective amount of solid magnesium oxide catalyst to neutralize the acid solid catalyst and to condense the silane diol to form a mixture containing neutralized, low molecular weight, linear, silanol-stopped polysiloxane;
(d) optionally adding an effective catalytic amount of solid calcium oxide catalyst to the mixture containing neutralized, low molecular weight, linear, silanol-stopped polysiloxane to condense the silanol-stopped polysiloxane and thereby increase the chain length of the polysiloxane; and
(e) separating the volatile by-products and solid catalysts from the low molecular weight, linear, silanol-stopped polysiloxane, whereby the polymer chain length varies according to the specific catalyst or catalyst combination, the silanolstopped polysiloxane having an average chain length of about 2.5 to about 4 siloxane units when magnesium oxide is used as catalyst, and the silanol-stopped polysiloxane having an average chain length of about 5 to about 6 siloxane units when calcium oxide is used as catalyst after magnesium oxide is used as catalyst.

### Claim 62 (depends on 61)

The method of claim 61 further comprising adding a filter aid and filtering the low molecular weight, linear polysiloxane to remove the solid catalyst.

### Claim 63 (depends on 61)

The method of claim 61 wherein at least 3 moles of water per mole of dialkoxysilane are vigorously mixed with the dialkoxysilane.

### Claim 64 (depends on 61)

The method of claim 61 wherein the mixture of dialkoxysilane, water and acid solid catalyst are vigorously mixed at about -10.degree. C. to about 60.degree. C. for a period of time sufficient to obtain a homogeneous mixture to about 45 minutes.

### Claim 65 (depends on 61)

The method of claim 61 wherein the acid solid catalyst is an acid-activated clay used in an amount of about 0.5 to about 2.0 parts by weight of catalyst per 100 parts by weight of dialkoxysilane.

### Claim 66 (depends on 61)

The method of claim 61 wherein the solid magnesium oxide is used in an amount between about 0.05 parts by weight to about 6.0 parts by weight per 1.0 part by weight of acid solid catalyst.

### Claim 67 (depends on 61)

The method of claim 61 wherein the solid calcium oxide is used in an amount between about 0.05 part by weight to about 6.0 parts by weight per 1.0 part by weight of acid solid catalyst.

### Claim 68 (depends on 61)

The process of claim 61 wherein volatile by-products and water are separated by vacuum distillation.

### Claim 69

A method of making stabilized, crystalline tetramethyldisiloxanediol comprising:
(a) mixing dimethyldimethoxysilane with a stoichiometric excess of water in the presence of an effective catalytic amount of solid acid catalyst for about 5 minutes to about 25 minutes at a temperature less than about 25.degree. C. to form a partially hydrolyzed dimethyldimethoxysilane;
(b) distilling the reaction mixture in the presence of the solid acid catalyst at a temperature less than about 30.degree. C. and at a pressure less than atmospheric pressure until volatile components are removed to substantially react the remaining alkoxy groups in the dimethylsiloxanediol;
(c) adding an effective catalytic amount of solid magnesium oxide catalyst to condense the hydrolyzed dimethylsiloxanediol and thereby form a reaction mixture containing a mixture of siloxanediols having chain lengths of 1, 2, 3 and 4, condensation by-products and solid catalysts;
(d) filtering the reaction mixture to remove the solid catalysts from the filtrate;
(e) distilling the filtrate at a temperature of about 25.degree. C. to about 65.degree. C. at a pressure less than atmospheric pressure until volatile components are removed therefrom to produce an oil; and,
(f) cooling the oil to crystalize stable tetramethyldisiloxanediol.

### Claim 70 (depends on 69)

The method of claim 69 further comprising adding a filter aid to the reaction mixture prior to filtering the reaction mixture to remove the solid catalysts from the filtrate.

### Claim 71 (depends on 69)

The method of claim 69 wherein at least 3.0 moles of water per mole of dimethyldimethoxysilane are vigorously mixed with the dimethyldimethoxysilane.

### Claim 72 (depends on 69)

The method of claim 69 wherein the mixture of dimethyldimethoxysilane, water and acid solid catalyst are vigorously mixed at about -10.degree. C. to about 25.degree. C.

### Claim 73 (depends on 69)

The method of claim 69 wherein the acid solid catalyst is an acid-activated clay used in an amount of about 0.5 to about 2.0 parts by weight per 100 parts by weight of dimethyldimethoxysilane.

### Claim 74 (depends on 69)

The method of claim 69 wherein the solid magnesium oxide is used in an amount between about 0.05 part by weight and about 6.0 parts by weight per 1.0 part by weight of acid solid catalyst.

### Claim 75 (depends on 69)

The method of claim 69 wherein the reaction mixture and the filtrate are distilled at a pressure of about 5 mm Hg to about 120 mm Hg.

### Claim 76

A method of making crystalline dimethylsilanediol comprising:
(a) mixing neutral dimethyldimethoxysilane with a stoichiometric excess of water in the presence of an effective catalytic amount of solid acid catalyst free of soluble acid for about 5 minutes to about 25 minutes at a temperature less than about 5.degree. C.;
(b) filtering the reaction mixture cold to form a cold filtrate;
(c) distilling the cold filtrate at a pressure less than atmospheric pressure until crystals of dimethyldisilanol form in the filtrate; and
(d) isolating the dimethyldisilanol crystals from the filtrate.

### Claim 77 (depends on 76)

The method of claim 76 wherein at least 3.0 moles of water per mole of dimethyldimethoxysilane are vigorously mixed with the dimethyldimethoxysilane.

### Claim 78 (depends on 76)

The method of claim 76 wherein the mixture of dimethyldimethoxysilane, water and acid solid catalyst are vigorously mixed at about -15.degree. C. to about +10.degree. C.

### Claim 79 (depends on 76)

The method of claim 76 wherein the acid solid catalyst is a neutralized acid-activated clay used in an amount of about 0.5 to about 2.0 parts by weight per 100 parts by weight of dimethyldimethoxysilane.

### Claim 80 (depends on 76)

The method of claim 76 wherein the filtration and the distillation are carried out at less than about 10.degree. C.

### Claim 81 (depends on 76)

The method of claim 76 wherein the pressure less than atmospheric pressure is about 5 mm Hg to about 150 mm Hg.