# US 4,395,509 A · Poly(arylene sulfide) composition suitable for molding

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,395,509 A
- Document ID: US4395509A
- Status: Granted
- Kind: A
- Application number: 06/354,129
- Filed: 1982-03-02
- Granted: 1983-07-26
- Earliest claimed: 1982-03-02
- Assignees: Phillips Petroleum Company
- Inventors: Jennings P. Blackwell; Dale O. Tieszen; Jack G. Scruggs
- Web page: https://patentgrep.com/patent/US4395509A

## CPC

- C08K 13/04: Ingredients characterised by their shape and organic or inorganic ingredients
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A composition suitable for molding applications containing from about 30 to about 50 weight percent poly(arylene sulfide), about 10 to about 30 weight percent glass fibers, about 30 to about 60 weight percent of a component chosen from glass beads, fused silica and mixtures thereof, from about 0 to about 3 weight percent colorant, and from about 0.5 to about 2 weight percent of a processing aid chosen from among N,N'-alkylenebis(alkanamides), glycerides and phosphated glycerides of saturated fatty acids containing from 10 to 30 carbon atoms, mono- and dialkanolamides derived from saturated fatty acids and esters derived from a saturated long-chained fatty acid and long-chained saturated aliphatic alcohol. A method for improving processability of a composition containing from about 30 to about 50 weight percent poly(arylene sulfide), from about 10 to about 30 weight percent glass fibers, from about 30 to about 60 weight percent of a component chosen from glass beads, fused silica and combinations thereof and from 0 to about 3 weight percent colorant in which there is admixed with this composition a processing aid in the amount of about 0.5 to about 2 weight percent with the processing aid chosen from N,N'-alkylenebis(alklanamides), glycerides and phosphated glycerides of saturated fatty acids containing from 10 to 30 carbon atoms, mono- and dialkanolamides derived from saturated fatty acids and esters derived from a saturated long-chained fatty acid and long-chained saturated aliphatic alcohol.

## Claims

### Claim 1

A composition suitable for molding comprising:
(a) from about 30 to about 50 weight percent poly(arylene sulfide),
(b) from about 10 to about 30 weight percent glass fibers,
(c) from about 30 to about 60 weight percent of a component chosen from glass beads, fused silica and mixtures thereof, and
(d) from about 0.5 to about 2 weight percent of a processing aid chosen from N,N'-alkylenebis(alkanamides), glycerides and phosphated glycerides of saturated fatty acids, containing from 10 to 30 carbon atoms, mono- and dialkanolamides derived from saturated fatty acids and esters derived from a saturated long-chain fatty acid and long-chain saturated aliphatic alcohol.

### Claim 2 (depends on 1)

A composition of claim 1 also containing a finite amount of up to about 3 weight percent colorant.

### Claim 3 (depends on 1)

A composition of claim 1 in which the processing aid is N,N'-alkylenebis(alkanamide) described by the formula ##STR2## where a and c are integers in the range of 10 to 25, preferably 15 to 20, and b is an integer in the range of 2 to 10, preferably 2 to 6.

### Claim 4 (depends on 1)

A composition of claim 1 in which the processing aid is a glyceride of saturated fatty acid.

### Claim 5 (depends on 1)

A composition of claim 1 in which the processing aid is a phosphated glyceride of saturated fatty acid.

### Claim 6 (depends on 1)

A composition of claim 1 in which the processing aid is chosen from mono- and dialkanolamides derived from saturated fatty acids and esters derived from a saturated long-chained fatty acid and long-chained saturated aliphatic alcohol.

### Claim 7

A method for improving processability of a composition comprising from about 30 to about 50 weight percent poly(arylene sulfide), about 10 to about 30 weight percent glass fibers, and from about 30 to about 60 weight percent of a component chosen from glass beads, fused silica and mixtures thereof said method comprising the addition to said composition of from about 0.5 to about 2 weight percent of a processing aid chosen from N,N'-alkylenebis(alkanamides), glycerides and phosphated glycerides of saturated fatty acids containing from 10 to 30 carbon atoms, mono- and dialkanolamides derived from saturated fatty acids and esters derived from a saturated long-chain fatty acid and long-chain saturated aliphatic alcohol.

### Claim 8 (depends on 7)

A method of claim 7 in which the processing aid is N,N'-alkylenebis(alkanamide) described by the formula ##STR3## where a and c are integers in the range of 10 to 25, preferably 15 to 20, and b is an integer in the range of 2 to 10, preferably 2 to 6.

### Claim 9 (depends on 7)

A method of claim 7 in which the processing aid is a glyceride of saturated fatty acid.

### Claim 10 (depends on 7)

A method of claim 7 in which the processing aid is a phosphated glyceride of saturated fatty acid.

### Claim 11 (depends on 7)

A method of claim 7 in which the processing aid is chosen from mono- and dialkanolamides derived from saturated fatty acids and esters derived from a saturated long-chain fatty acid and long-chain saturated fatty alcohol.